Thanks: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 4 of 4
-
17th Apr 2021, 09:49 PM #1Golden Member
- Join Date
- May 2020
- Location
- Willowbank QLD
- Posts
- 535
Black friction reduction anti corrosion at home
Hello all
I am working on a 48 Indian and they have exposed kick start gears. It got me thinking. Is there a practical way to stop the gear corroding, give it a nice black colour and help with reduced friction.
Something like metal blacking comes to mind if the right finishing oil was used. I am keen to do this at home. Even if I decide not to go this way on this gear I would be interested in options. I am always keen to learn. Please share your anti friction recipes and experiences.
Thanks Steve
-
17th Apr 2021, 09:57 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Even the very best commercial metal blackening/bluing will not resist metal on metal contact and it will eventually rub away. About the best you can do is keep a thin layer of oil on it.
Heres my DIY metal bluing thread that might give you some ideas.
https://metalworkforums.com/f65/t197115-metal-bluing?
-
18th Apr 2021, 12:14 AM #3
Hi Steve,
from memory, the '48 Chief had a silver coloured kick start lever and gear. I would get it nickel plated to prevent rust or corrosion. It won't help much with friction reduction, but drylube will. The kind used on off-road bike chains. That will also prevent corrosion as long as it is there - so regular squirts are in order....
oh, just noticed your question of doing it at home: Janekit in Sydney sell "electroless nickel" plating kits. I use them quite a bit and they work very well.Cheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
-
18th Apr 2021, 01:27 AM #4Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
Chromium nitride would probably work a treat (excellent corrosion and wear resistance, as well as reducing friction), but it's not the kind of thing you can DIY
Similar Threads
-
Noise Reduction
By Satwinder Singh in forum METALWORK GENERALReplies: 25Last Post: 17th May 2020, 10:27 PM -
GMC 2200W friction cut off saw SWITCH help?
By Grahame Collins in forum METALWORK GENERALReplies: 8Last Post: 6th Sep 2017, 11:35 AM -
Speed reduction vs. Stalling a motor vs. Horsepower
By steamingbill in forum METALWORK GENERALReplies: 8Last Post: 26th Feb 2017, 03:27 PM -
More on lube and anti corrosion /reclaimation
By Grahame Collins in forum METALWORK GENERALReplies: 3Last Post: 16th Apr 2012, 12:07 AM -
VSD Hp reduction
By Stustoys in forum METALWORK GENERALReplies: 31Last Post: 12th Jan 2011, 02:04 PM