Results 1 to 11 of 11
  1. #1
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default Welding bench (machining content)

    After the long project of the crane I'm glad to be back into the short time builds, this is one of them.

    This one was only a week or so, a new welding bench. I've never owned a dedicated welding bench.
    I like to weld and grind outside but my driveway has a slight slop so I needed a movable table adjustable.

    The 12mm top came from the side of the road collection, the basic 75x75x6mm stand was my old surface plate stand modified and the other steel I had second hand here. I also had the wheels from an old metal scrap bin which are made in England and full bearings with grease nipples etc.

    The jockey wheel was made out of an old car scissor jack thread rod/nut and some 40x40 and 50x50mm square tube.

    The draws and feet basses came from Bollie (Peter) a member here thank you.
    I also added a level from an old TV wall bracket to easily see if I've wound down the adjustable feet enough etc.

    Total cost was some hours, spray cans, and the gears which where $6 from AliExpress and the bearings for a a few dollars.
    So I spent some saved money on adding some 90 degree angle clamps and a set of 6 vice grip type welding clamps on top of what you see lol, all up around $100.
    Peter sent me a link after building it to H&F welding bench for $3250, wow.

    The gear ratio is 2.66 to 1, makes easy winding and the wheels make easy moving it.
    Empty it weighed 160kg, full it weighs just on 250kg.

    Dave J
    Using Tapatalk

  2. #2
    Join Date
    Oct 2008
    Location
    N.W.Tasmania
    Posts
    1,407

    Default

    Great work there Dave, especially when you consider what your budget was.

  3. #3
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Great work.

  4. #4
    Join Date
    May 2013
    Location
    Rockhampton, QLD
    Age
    68
    Posts
    455

    Default

    Nice outcome.

    Ross

  5. #5
    Join Date
    Sep 2006
    Location
    Mallacoota,VIC,Australia
    Age
    53
    Posts
    1,010

    Default

    Looks great Dave
    All The Best steran50 Stewart

    The shortest way to do many things is to do only one thing at once.

  6. #6
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Thanks guys, this was just a quick throw together project of what I had laying around that I'd collected up.

    The only wait was on the Makita angle sander gears (as advertised) that sized up right on AliExpress and the bearings, both where done after the table was finished and painted. Gears are so cheap on AliExpress as I found building the crane it's not worth making them.

    I wasn't waiting on them to finish after the crane taking so long waiting for parts in covid, I've got a massive backlog of projects with all the parts here already I'm moving onto.

    I'll post them up as I go.

    Dave J




    Sent from my 5007U using Tapatalk
    Using Tapatalk

  7. #7
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Some more pictures, 6mm earth clamp spots and cover over the greased bevel gears.

    Another recycled item is a old wall TV bracket level I had and mounted it close to the winding handle to adjust the feet to level the table easily, I even left there brand on there, lol.

    I'm sorry for the screen shots but seems to be the only easy way to reduce picture size easily.

    Also I'vee been told many years ago how to get rid of the annoying sent from X phone, I looked but can't find it, any members help would be appreciated to get rid of it as I know everyone hates it.

    Dave J
    Using Tapatalk

  8. #8
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Tapatalk?

    On the Tapatalk home screen, at top right hit the person icon, then settings, then signature. Turn off.

  9. #9
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by pippin88 View Post
    Tapatalk?

    On the Tapatalk home screen, at top right hit the person icon, then settings, then signature. Turn off.
    Done thank you, now I just need to find out how to do it with the forum on the internet.

    Stupid Tapatalk only allow so many pictures per month as I found out last week unless I pay.

    Looking forward to participating again but don't want to pay for pictures.
    Who would have thought photo bucket would have started charging, or hold your photos for randsom by not displaying them on forums, lol


    Sent from my 5007U using Tapatalk
    Using Tapatalk

  10. #10
    Join Date
    Sep 2006
    Location
    Australind , WA
    Age
    58
    Posts
    1,281

    Default

    I upload to Google photos and post the links, as I can't post pictures either.
    Almost as easy.

    Steve

    Sent from my SM-G970F using Tapatalk

  11. #11
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by Sterob View Post
    I upload to Google photos and post the links, as I can't post pictures either.
    Almost as easy.

    Steve

    Sent from my SM-G970F using Tapatalk
    Thanks,I have all my pictures in google

    Sent from my 5007U using Tapatalk
    Using Tapatalk

Similar Threads

  1. rusty welding bench top
    By WelderMick in forum METALWORK GENERAL
    Replies: 15
    Last Post: 12th Nov 2011, 06:45 PM
  2. Anyone need help with Machining or welding in SEQ
    By new_guy90 in forum METALWORK GENERAL
    Replies: 3
    Last Post: 6th Nov 2011, 09:59 PM
  3. hows this sound for a welding/work bench?
    By gros21 in forum METALWORK GENERAL
    Replies: 11
    Last Post: 20th Jun 2011, 01:11 PM
  4. Tig welding bench
    By chips63 in forum WELDING
    Replies: 20
    Last Post: 6th Oct 2009, 04:07 PM
  5. welding bench
    By Gags_17 in forum WELDING
    Replies: 35
    Last Post: 8th Jul 2009, 01:10 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •