Polishing Aluminum Pots and Pans that have had teflon coating blasted off
After blasting, the metal is slightly rough. What would be
the best way to polish these smooth? Would need to be a flexible
pad because the sides curve up and of course, the side to the
pot is about 6 inches tall.
-
22nd Mar 2021, 05:15 AM #2
-
22nd Mar 2021, 06:58 AM #3New Member
- Join Date
- Mar 2021
- Location
- memphis
- Posts
- 7
-
22nd Mar 2021, 07:47 AM #4Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Hi Virginia,
Aluminium pots that aren't non-stick are anodised. After sandblasting your pots are now raw aluminium which is unsuitable for cooking.
https://www.finecooking.com/article/...stick-coatingsChris
-
22nd Mar 2021, 08:44 AM #5Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Unless the OP knows something about MW then suggest use of a "mop" could be misleading.
What they really need is a bench top grinder fitted with a polishing mop.
However, unless they are just going to be put on display, I actually see little point in polishing them to high gloss finish as they will dull and scratch very easily so perhaps a "brushed" finish would be more practical?
In that case a Scotchbrite type mop on a grinder could be the way to go.
But I also agree with Jack, unless you are just going to boil water or use them for steaming vegetables etc the raw Al will not be that practical and you will be spending a lot of time trying to remove burnt on food from them. If you still have the grinder and mop it will help remove ny burnt stuck food from them.
Something to bear in mind is that for the cost of a grinder and a scothcbrite wheel you could also buy a beaut set of SS or coated Al saucepans.
-
22nd Mar 2021, 10:18 AM #6
After sandblasting it's going to need a lot of rubbing with different grades of sandpaper, then once smooth polish with a mop as described above.
There are some good tutorials online these days.
Sent from my 5007U using TapatalkUsing Tapatalk
-
22nd Mar 2021, 11:37 AM #7New Member
- Join Date
- Mar 2021
- Location
- memphis
- Posts
- 7
Whew....thanks for all the info. Lots more to research.
-
22nd Mar 2021, 05:32 PM #8Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
They are scrap metal.
Nev.
-
22nd Mar 2021, 05:34 PM #9Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
22nd Mar 2021, 07:19 PM #10Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
We have an induction cooktop so (Tin plated) Cu and Al cookware are of no use but SWMBO keeps several hanging up in the kitchen and I occasionally polish them up every now and the when I have the buffing wheels on.
-
23rd Mar 2021, 12:11 AM #11New Member
- Join Date
- Mar 2021
- Location
- memphis
- Posts
- 7
As for usefulness, the info is all over the place. After several google searches, I found googobs of info saying that unanodized aluminum is perfectly safe to use. I'm reading that commercial kitchens and chefs use them all the time for everything and don't find them any harder to clean than other kinds of pots and pans. Several forums are saying that they're safe even according to the Alzheimer's groups. So, I'm going to sand and polish and use unless I get definitive science otherwise or my experience tells me they're not worth it.
Thank you for all the input!
-
23rd Mar 2021, 12:12 AM #12
Hi Guys,
Actually thinking about it, if they have been grit blasted, they might be good candidates for anodising.Best Regards:
Baron J.
-
23rd Mar 2021, 12:21 AM #13New Member
- Join Date
- Mar 2021
- Location
- memphis
- Posts
- 7
-
23rd Mar 2021, 12:27 AM #14Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
I wasn't referring to any safety factors such as alzheimers but the fact that Al cookware doesn't work at all on induction based cook tops as they only heat magnetic (Iron or nickel) based cookware..
To get Al ware to work on an induction cook top they have to have an thick iron web or mesh implanted into the Al os the iron heats the Al.. The other way is to put the Al ware on top of a magnetic material. We have an Al Moka pot that we have managed to get working on our induction cooktop by placing it on top of a cast iron sauce pan. Some people say this is not a good thing to do to the cooktop so we have stopped using it.
The other thing about induction cooktops is the cookware has to be large enough to pick up the alternating magnetic field to heat the cookware. We have another (smaller) stainless steel Moka pot that should work on the induction cooktop but it doesn't because its too small. We tried it in the same cast iron sauce pan as above - it works but its very slow.
-
23rd Mar 2021, 12:32 AM #15New Member
- Join Date
- Mar 2021
- Location
- memphis
- Posts
- 7
Similar Threads
-
How do I attach an aluminum panel to aluminum tubing
By mark234 in forum METALWORK GENERALReplies: 17Last Post: 29th Nov 2018, 11:55 PM -
Newbie here, sanding/polishing for aluminum?
By chughes10 in forum METALWORK GENERALReplies: 16Last Post: 21st Apr 2017, 08:02 AM -
teflon liner in bulk?
By danielhobby in forum WELDINGReplies: 10Last Post: 16th Feb 2014, 08:23 AM -
teflon turning
By azzrock in forum METALWORK GENERALReplies: 13Last Post: 19th Jun 2012, 01:35 AM -
Powder coating DIY?
By neksmerj in forum METALWORK GENERALReplies: 5Last Post: 16th Mar 2009, 11:54 PM