Needs Pictures: 0
Results 1 to 15 of 16
Thread: Bearing Question
-
22nd Feb 2021, 07:24 PM #1
Bearing Question
G'day...hoping someone may be able to help me out with some local knowledge on a bearing issue ......let me explain:
Recently acquired an old Servian Pedestal Drill press from a deceased estate and doing a minor resto starting on the quill. First up thought I would change the bearings. They aren't seized up or anything and could probably be repacked and left alone, but there's the start of an annoying grate much like a politician at a sausage sizzle so while it's apart, reckon it's time to change them as I will also be changing the donk to a variable speed and putting new pulley on the quill.
The bearings on it are stamped "Made in England - FBC - L610" but I cannot find any information on them nor does that lettering show up in any of the material I have.
Beauty of old English engineering is everything is legible and I measured them out as OD:2.25"; ID: 1" and Width : ~0.615.
Thinking I would like to replace them with some type of sealed or shielded bearing but afraid my knowledge is limited on what's the best way to go with them.....especially when I can't find a direct equivalent.
I don't have a fly or other press so may have to send them out to be removed and new ones fitted but was hoping to get newbies first and send them along with the quill to be fitted at the same time rather than not know what they have been replaced with....
Appreciate any suggestion you may have..................Lee
-
22nd Feb 2021, 07:42 PM #2Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
Found some (basically) direct equivalents for you 2.25 x 1 x 0.625 (5/8)
Open: https://www.skf.com/au/products/roll...ductid-RLS%208
Shielded: https://www.skf.com/au/products/roll...tid-RLS%208-2Z
Sealed: https://www.skf.com/au/products/roll...d-RLS%208-2RS1
There's no real reason to go sealed in a drill press IMO as there's little chance of much dust getting in
-
22nd Feb 2021, 07:51 PM #3Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
-
22nd Feb 2021, 08:06 PM #4Senior Member
- Join Date
- Mar 2013
- Location
- Mt Pleasant SA
- Posts
- 126
Hi, looks like your bearings are equivalent to the old Hoffman LS10 whose width is 0.625" ( I doubt your width measurement). Try Googling (ball bearing 1" x 2.25" x 0.625" ). There is at least one UK company specialising in old equivalents, but don't leap on the first you see, I was recently on a similar hunt & found a UK source for an old style bearing, 145 POUNDS ea, as used on old BSA m/c ! Ended up getting one OFF the SHELF at local BRG shop .. $16. Afterthought, I doubt you'll get anything other than open type, but you never know. SLOW typist, started before the other posts!
-
22nd Feb 2021, 08:27 PM #5
Thank you for the input..it's greatly appreciated.....yes, I did recheck the width several times and I do get 0.61 but they are coupled next to the large washer and butted tight so it's difficult to get an exact measurement while they are in situ.
I would have thought it'd be 5/8" for sure given the DNA of the machine but I am unable to get an accurate measurement while they are mounted - was hoping the Part number L610 would give me the exact dimensions - hence the query.
Will take some piccies and post them tomorrow.
As an aside the press belonged to an old electrician so was told ---- with the utmost respect to any sparkies out there, the plug and wiring was a nightmare, bare wires, frayed connections and a broken bakelite switch so must have been one of those TUIT jobs we all have but he probably ran out of time...
-
22nd Feb 2021, 09:10 PM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
-
22nd Feb 2021, 09:53 PM #7Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
Could also be Fischer Bearing Company. https://www.gracesguide.co.uk/Fischer_Bearings_Co
Gold, the colour of choice for the discerning person.
-
22nd Feb 2021, 09:53 PM #8Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
-
22nd Feb 2021, 09:57 PM #9Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
The AHR site may be of help for technical questions about the original bearings.
Nev.
-
23rd Feb 2021, 01:03 AM #10Senior Member
- Join Date
- Aug 2007
- Location
- Saskatoon, Saskatchewan, Canada
- Posts
- 292
Maybe not the brightest question but have you searched around for the manuals or parts diagrams of your drill press? Or for others that have rebuilt one that might have said what bearings they found and where to get replacements? Someone else might have already done the legwork for you.
Pete
-
23rd Feb 2021, 09:52 AM #11Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
If it was me, I would be taking it (sample) to CBC or whoever...and let them tell me if something is available off the shelf or from OS rather than trying to determine if what I see on sites via the internet is really what I need....
if they they say nothing can be found, then I might be be spending the time to see if I can find something.
-
23rd Feb 2021, 11:33 AM #12
Thank you for all the comments and suggestions......they have given me plenty to work with. Unfortunately Pete there are no service manuals or literature for this machine that I could find but in all honesty it is a pretty basic machine, built in Australia around the 40's-50's I believe and built like a tank but elegantly simple....the pedestal which is over a meter tall is made from solid material probably close to 3" thick though I haven't measured it yet...weighed a ton moving and thankfully the engine hoist did the heavy lifting but initially 4 mates had to lift it from his bench to the ground and they struggled....took lots of hydration therapy for them to cope......I then trolleyed it to my trailer and off to it's new abode where it sits patiently waiting some lippies, spit polish on the pretty bits...and paint on the not so pretty bits....
Thanks Eskimo, will take the disassembled quill and bearing housing along to CBC or equivalent bearing place in nearby town for them to have a gander .....appreciate that suggestion.
Michael G, I'm not sure the L prefix and you are probably correct...hoping the bearing people will be able to confirm what it needs
In the meantime I have taken some piccies of the quill and the housing and you can see there are two different brands of bearings used - one US the other FBC England made..hopefully the piccies make sense but I can take more if you need them.
Found some restos of Servian Drill Presses on the WWW but none had any specs or were different models - they all seemed smaller versions but as it's a pretty basic construction and not overly complicated. Way it's built reckon it will outlast the grand kids when they come to ransack my tool shed after they send me off in the blue bus.
One of the reasons I got this being how solid it was plus it can take MT2 taper so I can at long last use the set of MT2 drills I bought 20+ years ago and not have to use the lathe for them...
Thanks again, I really do appreciate all your help and comments .....stay safe......Lee
-
23rd Feb 2021, 12:12 PM #13Senior Member
- Join Date
- Jul 2007
- Location
- Perth
- Posts
- 332
Hi Lee,
I have just refurbed a Tough drill from roughly the same era and with similar bearings, the local supplier Statewide was able to provide off the shelf items at reasonable cost. Several photos of mods I did which maybe of help during your restoration process, the better one is the split collar with a nylon washer on top to allow the table arm to be swivelled for alignment and the recent Supercheap car jack $27 to tryout table raising, works well, so will make up a similar mechanism more in proportion. The eye bolt lifting ring on top of the column is also useful. Good luck with the restoration and for sure it should last another 50+ years. Alan
-
23rd Feb 2021, 02:31 PM #14Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
Looks like a LS10 bearing and a New Departure 3203. The common equivalent for the ND 3203 is a 5203. New Departure used a 3 where everyone else used a 5.
Gold, the colour of choice for the discerning person.
-
23rd Feb 2021, 06:43 PM #15Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
Similar Threads
-
cam bearing
By morrisman in forum AUTO RESTORATIONReplies: 3Last Post: 18th Oct 2019, 05:53 PM -
NSK bearing DU2 significance
By Ropetangler in forum METALWORK GENERALReplies: 11Last Post: 18th Jun 2015, 09:52 PM -
Bearing
By WesP in forum METALWORK GENERALReplies: 4Last Post: 25th Oct 2014, 12:16 PM -
Air bearing stage...
By RayG in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 13th Oct 2014, 11:49 AM -
A little help finding a bearing?