Hardly jewellery quality
And we don't have a forum for spectacle repair so I thought it ought to go here.
The wing of my specs broke, alleged to be titanium.20210207_193605.jpg
Turned a bit of brass rod down and managed to drill a hole.
Bit of superglue and she'll do.
20210207_193757.jpg
-
8th Feb 2021, 10:13 AM #2
Titanium specs
My brother Darrell made his own glasses out of Titanium...
... Because he could!
-
8th Feb 2021, 10:50 AM #3Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
I was sold a pricey pair of partially-titanium spectacle frames, only to have it break where it was plastic.
Some have made their own spec frames with MIG welding wire.
-
8th Feb 2021, 06:14 PM #4Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
I bought these from China for about $30, so I'm not very unhappy. Compared to 250+ from optician.
I try to get rimless, no screws.
Similar Threads
-
Setting Up A Jewellery Workshop In A Secondary School
By SpamIsNotHam in forum JEWELLERYReplies: 6Last Post: 12th Mar 2019, 12:58 AM -
Weld Quality
By rod1949 in forum WELDINGReplies: 10Last Post: 15th Apr 2014, 05:01 PM -
Chinese quality versus Swiss quality
By RayG in forum METALWORK GENERALReplies: 28Last Post: 5th Nov 2011, 12:41 PM -
HSS Quality
By xr6t in forum METALWORK GENERALReplies: 20Last Post: 2nd Jan 2010, 11:06 PM