Sometimes setups are so awkward
The T slots in my new 6" rotary table won't allow common T slot nuts to fit all the way in.
20210125_100925.jpg
The T nuts will be used for holding down my new 63mm machine vise to the rotary table and I used it here to make the nuts.
It took a rather awkward setup to make a couple of T nuts suitable for the plate.
Center the rotary table, center the part and align the vise with the mill's X axis. Fun !
20210124_145632.jpg
20210124_145640.jpg
The results :
20210125_095812.jpg
-
25th Jan 2021, 10:50 AM #2Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Thats a great idea, making and radiusing some T nuts for the RT.
Talking about akward, some of my most dodgiest setups have been on my RT!
I got an 8" and there always seems to be not enough room!
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
25th Jan 2021, 12:12 PM #3Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 205
Looks good.
I am after a small vice like that - what did you buy and are you happy with it? Have you checked it out for precision at all?
Ian
-
25th Jan 2021, 12:12 PM #4Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
I made them from a piece of 25mm square standing on its end in the vise. After milling I cut the T nut off and faced it.
The table on my mill isn't big enough. If I put the BS-0 dividing head as far on the left as possible, and its tailstock far to the right, there's only about 100mm between centres.
-
25th Jan 2021, 01:13 PM #5Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
This is the one I bought. Quick delivery too , 5 days..
I haven't measured everything on it yet but it's really nicely made. I'd say it would be pretty close to accurate. It's heavy enough and all surfaces are ground.
The weakest link is the tightening screw. It's 8mm and I won't know how tight I can make it until the day I strip it or its nut.
https://www.ebay.com.au/itm/QKG-50mm...frcectupt=true
-
25th Jan 2021, 01:36 PM #6Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 205
Thanks very much.
I was looking at the same kind of size from Dawn. Trying to support an Aussie business and pay for good quality but the Dawn is close to $500 and I’m just not so sure I’ll notice much difference....