Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 15 of 27
Thread: Sutton "Viper" line
-
25th Dec 2020, 12:07 AM #1Member
- Join Date
- Mar 2012
- Location
- adelaide
- Posts
- 91
Sutton "Viper" line
does any one know were Suttons make their "Viper" line of drill bits are made ?
-
25th Dec 2020, 09:09 AM #2Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
According to this mob they're made here (I believe the factory is in Melbourne) https://www.revolutionindustrial.com...rill-set-m2-hs
According to the Sutton website the HSS stock is European sourced
-
25th Dec 2020, 09:45 AM #3Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Oz, NZ and China. Wouldn’t be surprised if they are slowly shifting all manufacturing to China. I’ll ask the rep next time I see him.
Chris
-
25th Dec 2020, 10:05 AM #4Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
I don't think they will move entirely to China, at least not in the short term. They bought Carbitool a few years ago (and haven't just absorbed it and shut it down), so that indicates to me that they're going to keep some production local; probably the premium stuff here and the budget stuff offshore.
Their PVD coating operation is definitely in Melbourne; we just paid a small fortune to have some parts CrN coated. Plain nitriding would probably do, but aerospace customer wants CrN, so aerospace customer gets CrN
-
25th Dec 2020, 11:59 AM #5Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
When I visited a year or so ago all the HSS tooling that is sutton branded (not PN or frost) was made here with the heat treating done at the old patience and Nicholson works.
all the frost stuff is out of China.
The viper drills are split point. Very good indeed.
Sent from my SM-G973F using Tapatalk
-
25th Dec 2020, 01:47 PM #6Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
I definitely saw "Made in China" on the packaging of some of the smaller Viper bits in Bunnings last week. Interestingly, some older stock of the same sized bits were made in NZ. So maybe a recent change? The cobalt bits were all marked Made in Oz.
Chris
-
25th Dec 2020, 03:15 PM #7Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
It would be a brave or foolhardy Australian company nowadays that outsourced to China.
-
25th Dec 2020, 06:46 PM #8Senior Member
- Join Date
- Sep 2009
- Location
- Newcastle
- Posts
- 342
-
25th Dec 2020, 07:08 PM #9Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
We are trying to 'on-shore' some production at the moment. The biggest stumbling block seems to be some of our production staff, who see the level of automation we need to develop as 'too complicated', and want an off the shelf, turn-key solution.
Michael
-
26th Dec 2020, 11:09 AM #10
Just had a look at my Sutton Viper set ,can’t see any where it says where it is made, just 100% Australian owned.They are a few years old.
Sent from my iPhone using Tapatalk
Ratty 05/2004 -05/07/2010 COOPER 01/08/1998-31/01/2012
-
26th Dec 2020, 11:14 AM #11Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Looking at the Australian made campaign. It seems in plain HSS drills they only make the stub and long drills and the inbox stuff here. The others must be outsourced.
That sucks and certainly did not used to be the case.
Sent from my SM-G973F using Tapatalk
-
27th Dec 2020, 12:39 PM #12Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
Had a look in total tools today, some of the viper drills were made in NZ and some were unlabeled. the carbon steel taps were made in japan. i wonder if they are getting squeezed by the big green shed to cut costs on the retail lines they sell.
-
28th Dec 2020, 04:20 PM #13Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Nearly every Viper bit I looked at in Bunnings today was made in NZ. A few were marked “100% Australian Owned” which of course means “made in China”.
Chris
-
28th Dec 2020, 05:21 PM #14Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
I thought country of origin was mandatory on packaging...
-
28th Dec 2020, 08:39 PM #15Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
So did I.
Chris
Similar Threads
-
" ? - Burton " line shaft drop hammer
By TAnnarelli in forum METALWORK GENERALReplies: 13Last Post: 10th Jul 2016, 09:39 PM -
Ignyte Precision Granite Surface Plate 24" x 18" x 4"
By kwijibo99 in forum METALWORK - Machinery, Equipment, MARKETReplies: 10Last Post: 5th Jul 2016, 10:41 PM -
P&N / Sutton Tap Wrench Size for 1/2" BSP Tap?
By ventureoverland in forum METALWORK GENERALReplies: 10Last Post: 14th Aug 2015, 07:24 AM -
Opposing toothed "Clutch-Plate" Nuts? (a bit like "Castle" Nuts...)
By Batpig in forum METALWORK GENERALReplies: 6Last Post: 5th May 2009, 08:18 PM -
Difference "Galvanised" and "Primed" Steel
By Fr_303 in forum METALWORK GENERALReplies: 4Last Post: 22nd Jan 2008, 05:59 PM