Needs Pictures: 0
Results 1 to 9 of 9
-
21st Dec 2020, 10:47 PM #1Golden Member
- Join Date
- Jul 2011
- Location
- Adelaide
- Posts
- 837
Supplier advice for rubber bush/mount.
Imagine if you will a rubber grommet with ID ⅜" designed to go through a hole that is 11/16" in diameter in a piece of ⅜" plate.
This is what the 3 motor plate isolation bushes in my Steelfast 370M looked like before oil rotted them away.
Has anybody got any ideas on where I might find such a thing? I have already tried Fitch/UES in Adelaide.
-
21st Dec 2020, 11:09 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Hi Eric, I doubt that you'll get a proper grommet in the size you're after, but I found something that may be adaptable for you.
Here's the link;
https://www.ebay.com.au/itm/10pcs-La....c100752.m1982
Does it have to be rubber?? There use to be a place on Manton St Hindmarsh that made gear using urethane, similar to suspension bushes, it was called Agriculture Rubber and Plastics, they're now out Greenfields
https://www.startlocal.com.au/indust...d_2069445.html
HTH
KrynTo grow old is mandatory, growing up is optional.
-
21st Dec 2020, 11:31 PM #3China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
You could try this company, I purchased some small urethane bushes for the motor on my my buzzer from them a few years ago ( hope they are still around )
https://www.technicalurethanes.com.au/
Royce Cross may have them
-
21st Dec 2020, 11:33 PM #4Senior Member
- Join Date
- Nov 2011
- Location
- Port Sephens NSW Southside
- Posts
- 123
Cable Glands
Eric
Would a cable gland do the job. Jaycar carry some as well as RS Components.
https://au.rs-online.com/web/p/cable-glands/6694664
This one fits a 20mm hole with 15mm of thread for mounting & cable size of 6-12mm.
Bag of for $13.54
JohnQ
-
22nd Dec 2020, 12:02 AM #5I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,300
If you've got a lathe, you can knock some up out of polyurethane rod....
https://superpro.com.au/blog/116-superpro-poly-rods
Superpro have a few stiffnesses, plus there are some helpful maching tips on the page, but there are many other suppliers.
I've turned some polyurethane before, with a fairly high rake tool (although not as high as Superpro are suggesting), and it turns fairly well once you get the hang of the feed required. Haven't drilled it though, the stuff I've got was actually tube with a 1/2 hole in the middle which was all I needed. Don't know that it's available in anything smaller than that ID, but it might be.
-
22nd Dec 2020, 02:49 AM #6Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
Mackay Industrial Rubber (anyone that stocks Mackay Automotive products should be able to order them)
https://9198c40c-83e9-4d43-bf42-8056bee9b747.filesusr.com/ugd/17eaaa_0f660765b3a74b3aa2a499143e646e5f.pdf
Vibration Solutions
https://vibrationsolutions.com.au/product/scb-mount/
Evil bay (not quite your exact dimensions, but very close)
https://www.ebay.com.au/itm/4pcs-Two...wAAOSwtfNfcE1Y
-
23rd Dec 2020, 11:58 AM #7Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
anything on this page
Pages from ues_cat_f_2.jpg
As Adam suggests, I reckon there would have to be something in the Mackay range that would suit
https://www.mackayrubber.com.au
-
23rd Dec 2020, 12:01 PM #8Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
I've been making simple multi piece moulds and casting a few different grommets for an old car project. Small quantities of PU rubber liquids come from Rowe Trading in Adelaide.
A crude sketch saves a thousand words.
grommet mould sketch23122020.jpg
IMG_3462.jpg IMG_3708.jpg
-
23rd Dec 2020, 08:36 PM #9Senior Member
- Join Date
- Nov 2011
- Location
- Port Sephens NSW Southside
- Posts
- 123
Cable gland
Sorry, miss read original post, thought it was for a cable to pass through.
JohnQ
Similar Threads
-
Bush Fires !
By BaronJ in forum GENERAL DISCUSSION / OFF TOPICReplies: 59Last Post: 23rd Jan 2020, 05:30 PM -
Rubber Rope
By BobL in forum GENERAL DISCUSSION / OFF TOPICReplies: 4Last Post: 22nd Aug 2019, 11:17 AM -
Tipping Trailer Pivot Pin & Bush Supplier Req'd
By Bad Fruit in forum TRAILERS & OTHER FABRICATED STUFFReplies: 3Last Post: 9th May 2012, 12:37 AM -
Another bloke needing advice - drawbar mount?
By Tim37 in forum TRAILERS & OTHER FABRICATED STUFFReplies: 12Last Post: 25th Oct 2010, 06:44 PM