Needs Pictures: 0
Results 1 to 11 of 11
Thread: Old iron, identification?
-
25th Nov 2020, 04:34 PM #1
Old iron, identification?
I was lucky enough to be given some old iron, which is one of two metals, either Double Griffin, or Durax.
It would be very handy to know for sure which it is, so any way to do it without specialist gear?
-
25th Nov 2020, 04:52 PM #2Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,079
If you know it's one of two dissimilar materials (from what I can gather from the internet, Double Griffin is tool steel and Durax is just 1040), a simple hardness test might be enough. Or you could send a sample off for analysis and you'll get a full composition breakdown. No idea how much it'd cost though.
-
25th Nov 2020, 04:59 PM #3Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
-
25th Nov 2020, 05:23 PM #4
-
25th Nov 2020, 05:30 PM #5Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,079
You only need a comparison sample for absolute measurement (how hard is it), for comparative measurement (which one is harder) you'll see straight away. An automatic centre punch might give an indication, but with the difference being so small it might be too hard to tell just by looking.
-
25th Nov 2020, 05:53 PM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Probably easier to do a grinder spark test if one is tool steel and the other low carbon steel.
Michael
-
25th Nov 2020, 06:36 PM #7Golden Member
- Join Date
- Sep 2008
- Location
- Riddells Creek, Vic.
- Posts
- 838
To answer your question,yes,there are ways of doing it with specialist gear. One way would be to get one of these:
xrf gun.jpg
XRF Scan (1).jpg
Would it be economical, I doubt it.
-
25th Nov 2020, 06:57 PM #8
I don't know about the durax but here is the specs for double griffin from an old Eagle and Globe steel handbook.
If it helps.
Eagle & Globe.
Double Griffin- shock resisting steel. AS1239/ AISI spec: S100A.
C .35
Si .2
Mn .3
Cr 1.75
Ni 3.5
Forging range 850-1100 C
Annealing temp 750 C
approx. annealed hardness (Brinell) 220
hardening temp. 850-950 C
quenching medium: air-salt-oil
tempering temp. range: 0-550 C
working hardness, Rockwell 'C' 40-51
Applications: Ni-Cr shock-resisting steel. Punches, shear blades, chisels, snaps, wedges.
Grahame
-
25th Nov 2020, 08:32 PM #9
I didn't realise the original post was ambiguous.
I only have ONE type of steel, which is ONE of the metals Durax OR Double griffin,
which is why I would need a known sample of either to do a simple hardness test.
-
26th Nov 2020, 12:44 AM #10
ptrott
From your OP I realised that you had one piece of metal and you did not know what it was.
I gave specs for the double griffin as we had chisels from it in the seventies and had a general idea of its hardness,but couldn't remember the specific number.
Ok double griffin is 40 to 51 Rockwell C and that converts to 375 to 495 Brinell
Durax 1045 converts to Rockwell 20 C but listed as 223 Brinel. Here is the link to check
https://www.engineersedge.com/hardness_conversion.htm
A cheap way to gauge the hardness is with a set of hardness testing files. - knifemakers use them - look them up on Ebay.
Much cheaper but way less accurate but should get you there would be to centerpop some known mild steel and then your lump of steel.
If the pop gives approximately the same mark -its Durax 1045. If it flattens the end of the pop it is double griffin.
Please take some pics if you can so we can all learn something.
Around $190 dollars for a set of six if you buy Japanese made or $40 odd if you buy chinese.
Grahame
-
26th Nov 2020, 05:53 PM #11
Similar Threads
-
When does cast iron not machine like cas t iron?
By simonl in forum METALWORK GENERALReplies: 20Last Post: 31st Jul 2018, 08:57 PM -
Cast iron fireplace - Question for restoring using Penetrol & Liberon Iron Paste
By mookschank in forum METALWORK GENERALReplies: 8Last Post: 19th Jun 2013, 06:32 PM -
Lathe identification
By Malibu in forum THE HERCUS AREAReplies: 13Last Post: 11th Mar 2011, 11:15 AM -
Identification problem
By Ralphie in forum THE HERCUS AREAReplies: 5Last Post: 3rd Jan 2009, 10:19 PM -
lathe identification
By tanii51 in forum METALWORK GENERALReplies: 18Last Post: 24th Aug 2008, 10:13 PM