Thanks: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 15 of 19
-
21st Nov 2020, 10:11 PM #1New Member
- Join Date
- Nov 2020
- Location
- Daisy Hill
- Age
- 78
- Posts
- 4
Astronomical observatory roof roller steel u channel
A few years ago I recovered an astronomical observatory. It consisted of a 3 meter square wooden structure on on which a 3 three meter rotating steel dome stood. I have recently started rebuilding it and have laid the concrete slab, telescope pier foundation, and walls to ceiling height but to cut a long story short have decided to forego reassembling the dome and instead opt for a simpler and lighter roll off roof.
For the rolling mechanism I have some industrial stainless steel pallet rollers which I plan to use upside down rolling in a U shaped steel channel. The U channel steel would need to be 50 mm wide and 40 mm high and 2mm thick to accommodate the rollers.
I have been unable to find anyone who can supply U section of this dimension but I can get 50 x 50 x 2 square section. I would however have to cut off one side of the square tube to give me a height of 40mm.
My thoughts are to do this with an angle grinder with a metal cutting disc but because I would need to make two lengthwise cuts into 12 meters of square tube (24 meters of cut) it seems a daunting task and am wondering whether there is an easier option.
Open for any suggestions.
Geoff
-
21st Nov 2020, 11:37 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Hi Geoff and WELCOME to a TOP FORUM.
If you have a decent sized compressor available, you could hire a Plasma Cutter. Set it up with a guide so that you're able to cut a constant 40mm wide section. That's about the easiest way i can think off. If you get your pressure and speed right, there should be very little cleanup required.
HTH
KrynTo grow old is mandatory, growing up is optional.
-
22nd Nov 2020, 12:06 AM #3I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,294
I wouldn't be too keen to take that approach myself.... RHS can take some very interesting shapes sometimes when you cut one side of it out, you might end up with a badly warped track, which I assume is undesirable. Depends on the luck of the draw as to how much stress is in the bits of RHS you buy.
All depends on the tools you have of course. I'd sooner weld my own profiles out of 40mm and 50mm (or wider, depending on attachment design) flat bar, but that does bring some challenges in avoiding warpage too, and of course requires a welder. Not too sure about getting flat bar in less than 3mm thickness either, if that is a fixed constraint.
Ideal solution for the profile exactly as specified would be to find a decent size fabrication shop with a guillotine and pressbrake to make up that profile out of 2mm plate - preferably with an owner very fond of beer.
Without knowing the space and design constraints you have, bit hard to offer much else...
-
22nd Nov 2020, 01:08 AM #4China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
As said above cutting would be the stuff of nightmares, far simpler to fabricate from flat bar.
-
22nd Nov 2020, 03:24 AM #5
Hi Geoff, Guys,
I would have thought at 2 mm thick it would be screwed to a timber support. Though there are UPV plastic sections that might do the job.
One thing that would bother me is the wind ripping it off. But without knowing the design details difficult to advise.Best Regards:
Baron J.
-
22nd Nov 2020, 09:25 AM #6Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,552
No, that’s the easiest option. You can cut it with a grinder reasonably easily, and consistently if you make a guide or rest to support the grinder. Not overly difficult at all, just needs to be a block of timber or something that holds the grinder guard at the correct height and not allow it to rock or tilt. Use a 1.6mm disc and remember to cut the face with the seam off.
-
22nd Nov 2020, 09:47 AM #7Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
How about some commercial C channel, with either bigger rollers or two small rollers, one for each flange? I agree with all those comments about cutting RHS - it will not work well.
These guys have hot rolled 100x50
https://www.orrconsteel.com.au/produ...-steel/channel
Or there is cold rolled
http://www.bluescopesteel.com.au/fil...rtiesjan10.pdf
Michael
-
22nd Nov 2020, 09:58 AM #8Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,552
Interesting, I’ve sectioned RHS and SHS on quite a few occasions and never found it difficult or challenging. Everything presents differently to the individual I guess.
-
22nd Nov 2020, 03:18 PM #9China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Yeh! for short lengths maybe, we are are talking "12 mtr cut"
-
22nd Nov 2020, 03:48 PM #10Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,552
I think it was 24m, I’m imagining being a 3m structure, the lengths are 6m each to allow the roof to slide back so the top can be fully opened.
Random suggestion.. what about a roller door for the roof?
-
22nd Nov 2020, 04:14 PM #11Senior Member
- Join Date
- May 2013
- Location
- Rockhampton, QLD
- Age
- 68
- Posts
- 455
Welcome to the forum Geoff.
Ross
-
22nd Nov 2020, 05:00 PM #12China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Roller door would need fixed supports this would create obstructions at some point, this is why the preferred method is a dome can be moved to to any position giving unrestricted view, the are some designs with a square type roof although these are normally mounted on a circular bearing of some configuration, it seems like Geoff has chosen to just slide the entire roof from the top of the building, not ideal for many reasons, but I am sure he has researched this and come up with his own compromise.
-
22nd Nov 2020, 06:50 PM #13New Member
- Join Date
- Nov 2020
- Location
- Daisy Hill
- Age
- 78
- Posts
- 4
Thanks for the welcome all. Very much appreciated by an old codger trying his hand at metalworking and welding for the first time.
The original dome was made out of a steel rhs geodesic frame covered by sheet steel rotating on a huge 3 meter steel ring. We managed to get the steel ring home but had to cut the dome into three sections. I decided against reassembling it as it was just so heavy and would have been difficult to use without also investing substantially in precision power assistance. I also briefly considered a garage panel door but I had concerns with waterproofing, overhead obstruction, and condensation whereas a simple insulated roll off Could avoid all those issues.
So committed now to the project, I purchased a short piece ( 0.6m ) of 50 x 50 rhs to practice on.
it took me about 20 minutes and one cutting disc to turn it into a 50 x40 channel.
I was happy the way the roller fitted into the newly made channel and how easily it ran.
Calculating things out that equates to roughly 6 hours of cutting time and about 20 cutting discs for my small grinder. I think can do that if I set the job up up well and not try to do things too hastily.
Just some pics of the work.
.7071809C-1B1D-44A7-A18E-9FF60AF584ED.jpg65BED89F-3CBC-4964-BD67-B7E6538E8F0F.jpg
-
22nd Nov 2020, 07:23 PM #14
-
24th Nov 2020, 06:09 PM #15Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Similar Threads
-
My YouTube Channel!
By Patrick-C in forum Members VideosReplies: 3Last Post: 25th Mar 2020, 04:03 PM -
My YouTube Channel!
By Patrick-C in forum ANNOUNCEMENTSReplies: 0Last Post: 2nd Mar 2020, 03:49 PM -
which steel for small jeweller roller?
By Alex_Campili in forum JEWELLERYReplies: 2Last Post: 12th Nov 2017, 12:44 AM -
Steel Roller Question
By BobL in forum METALWORK GENERALReplies: 21Last Post: 7th Feb 2013, 01:00 AM -
Best way to cut colourbond channel
By Sterob in forum METALWORK GENERALReplies: 15Last Post: 7th Feb 2009, 04:24 PM