Centering rectangular stock in 4 jaw
I am working on a project where I want to face off some rectangular stock and if possible drill a centre hole (although I could do that on mill later). I intended on facing one side, then flipping over to the other and have two nice parallel surfaces. I have centred round stock in the independent 4 jaw previously using a dial indicator but I am unsure of best approach with the rectangular stock. I wondered if I should pick a corner and basically find a sort of top dead centre to compare and adjust to? I am sure there is a better way so I hope someone can set me right.
Sent from my iPad using Tapatalk
-
17th Nov 2020, 10:13 PM #2Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
I picked up this trick from an Abom video, it requires 2 centres, at least one of which should be dead. This works for clocking up any arbitrary point you want, not just the centre.
Make a punch mark in the centre of the stock, hold a dead centre between the punch mark and another centre which is in the tailstock, then indicate the "floating" dead centre. Picture...1000 words...etc:
PXL_20201117_111121068.jpg
-
18th Nov 2020, 03:47 AM #3
Hi Ian, Guys,
That is basically the technique that I use ! Draw a pencil line from corner to corner and prick punch the centre. I have a 10 inch length of 5 mm silver steel rod with a point on one end which I clamp in the tailstock drill chuck, then using a dial indicator with an elephants foot resting on the rod. Adjust for no indicator movement as the chuck is rotated.Best Regards:
Baron J.
-
18th Nov 2020, 07:14 AM #4Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
-
18th Nov 2020, 08:01 AM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
It should be no different to centring square stock, except do the opposite sides before moving around 90 degrees. I find that I usually have to wind the carriage back so I don't wipe out the indiator tip when I rotate the corner past the indicator. The centre in a punch mark technique will work, but relies on the punch mark being spot on. Using an indicator on the sides will get you closer to the true centre if it is important
Michael
-
18th Nov 2020, 10:12 AM #6Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
-
18th Nov 2020, 11:05 AM #7Golden Member
- Join Date
- Jun 2007
- Location
- Vic
- Age
- 48
- Posts
- 544
I normally just draw 2 diagnose lines then eyeball it with the dead centre on the tailstock if accuracy is not required
-
18th Nov 2020, 01:17 PM #8Senior Member
- Join Date
- Jul 2011
- Location
- Berowra Waters
- Posts
- 149
I reckon I would be more concerned about how likely it will snap the tip of the tool off when you get out to the outside and there’s fresh air before the edge of the workpiece hits the tool. It wouldn’t matter if it was not exactly centred if you’re just facing it off would if?
-
18th Nov 2020, 03:37 PM #9Golden Member
- Join Date
- Jun 2007
- Location
- Vic
- Age
- 48
- Posts
- 544
I find it is better to use HSS for interrupted cut, the insert tends to chip/break.
-
18th Nov 2020, 05:25 PM #10Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
18th Nov 2020, 07:56 PM #11
Spring Centre !
Hi Guys,
This is my spring centre, I usually use it for keeping taps straight when threading holes.
01-09-2018-001.jpg
Its home brew and very simple to make. Though not a good tool for centre finding !Best Regards:
Baron J.
-
18th Nov 2020, 07:57 PM #12
-
19th Nov 2020, 06:59 AM #13Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 205
-
19th Nov 2020, 03:51 PM #14Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
-
19th Nov 2020, 04:32 PM #15Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
For a job like that, seeing as you mentioned using a mill, I’d use a face mill or fly cutter, then bore the centre hole. Only have to clean and oil one machine then...
Similar Threads
-
Bending rectangular tubing
By rbtp in forum METALWORK GENERALReplies: 14Last Post: 30th Mar 2020, 12:51 PM -
Centering Hex stock in a 4 jaw?
By topari in forum METALWORK GENERALReplies: 3Last Post: 27th Jul 2018, 06:55 PM -
Centering stock in 3 jaw chuck
By oohsam in forum METALWORK GENERALReplies: 26Last Post: 16th Jun 2014, 11:17 AM -
How to cut a rectangular hole in a gutter
By ratchet in forum METALWORK GENERALReplies: 12Last Post: 6th Sep 2011, 08:20 PM -
Centering square stock in a 4 jaw chuck
By Dingo Dog in forum METALWORK GENERALReplies: 2Last Post: 11th Apr 2008, 09:13 AM