I would think twice before using that method. It will work if and I do stress IF you are very confident that you can pull the pulley off before the weld cools and contracts. If you cannot achieve this, then you will be left with a pulley that is actually tighter than before. Welds always contract more than they expand.
A better method that utilises the same principle is to heat the boss with either Oxy Acetylene or Oxy Propane (perhaps straight propane may suffice if the burner is large enough), the trick is large tips/burners and get the heat in quickly. You want the boss as hot as possible and the shaft as cold as possible.
The weld bead method does however make removal of bearing cups from internal bores like child's play.
-
1st Nov 2020, 07:20 PM #17Intermediate Member
- Join Date
- May 2011
- Location
- Melbourne
- Posts
- 33
Another idea
I hesitate to suggest this approach for freeing something as large as this, but for releasing stuck smaller components I have had good results with Loctite's Freeze and Release spray: https://www.repco.com.au/en/oils-flu...10g/p/A9328441
Similar Threads
-
removing elec motor fan
By bollie7 in forum METALWORK GENERALReplies: 22Last Post: 15th Oct 2019, 07:49 PM -
Waldown 4 Step Motor Pulley
By Anorak Bob in forum METALWORK - Machinery, Equipment, MARKETReplies: 3Last Post: 19th Nov 2018, 03:57 PM -
Ways to remove stubborn set screw in motor pulley?
By Gunnaduit in forum METALWORK GENERALReplies: 90Last Post: 27th Jul 2018, 05:50 PM -
Removing Mill Motor
By electrosteam in forum METALWORK GENERALReplies: 7Last Post: 10th Jul 2010, 09:54 AM -
Motor twin pulley dimensions ???
By bitza500 in forum THE HERCUS AREAReplies: 2Last Post: 29th Nov 2008, 04:43 PM