I require a very small machine screw as a replacement for one that has fallen out of a Shimano fishing reel. It seems to be a very coarse thread, more so than UNC or metric coarse. The maximum diameter across the tips of the threads is 1.92mm and a 6mm long screw out of the same reel has 14 threads (+/- 56 TPI). As far as I know M2 coarse and UNC of a similar size have 63 TPI. Just wondering if anyone has any idea what thread size I need (1.92mm/56TPI) or could it be custom made for Shimano.
Thanks
Mike
-
7th Oct 2020, 06:04 AM #2
Hi Mike,
Could it be 9BA, that is 1.9 mm 64.9 tpi. I can't find anything around 56 tpi of that diameter,Best Regards:
Baron J.
-
7th Oct 2020, 06:46 AM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
If it is a Shimano fishing reel, it is Japanese so probably their version of metric. You need to be looking at JIS thead tables.
Michael
-
7th Oct 2020, 08:59 AM #4Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Bear in mind that manufacturers can and do make whatever size/thread fixings that best suit the application. They usually follow the thread charts but not always. A Japanese screw with an OD of 1.92mm suggests a 2mm nominal OD.
-
7th Oct 2020, 09:19 AM #5Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
M2 has a pitch of 0.4mm. Assuming it IS a M2 screw, 14 threads would be 5.6mm long. A combination of small errors in length measurement and pitch count would account for the difference (your 6mm screw is unlikely to have exactly 14 threads on it). I'd be trying a M2 first.
Chris
-
7th Oct 2020, 09:19 AM #6Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Can you buy one as a spare part?
-
7th Oct 2020, 09:38 AM #7Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 574
M2.2 coarse is approx 56TPI
-
7th Oct 2020, 09:41 AM #8Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
i'd like to see a close up photo of it laying on a ruler with mm markings on it.
-
7th Oct 2020, 10:22 AM #9Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
7th Oct 2020, 10:28 AM #10Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Probably just file it down to suit, be a good exercise in filing round and debuting small threads.
-
7th Oct 2020, 10:51 AM #11Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
I feel like I’m missing something here, why are metric thread threads being quantified in threads per inch?
-
7th Oct 2020, 11:50 AM #12Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
Some 56 tpi in small diameters on the attached list.
-
7th Oct 2020, 03:06 PM #13Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 574
-
7th Oct 2020, 05:51 PM #14
-
7th Oct 2020, 05:56 PM #15Member
- Join Date
- Nov 2009
- Location
- australia
- Posts
- 57
Think you better go buy a couple of sets of these, buy one set Metric, the other set Imperial !!!!
That way YOU will be able to identify the thread correctly and then YOU will know what your talking about.
Others will then be able to advise correctly, without taking a stab in the dark.
https://www.ebay.com.au/itm/Measurin...AAAOSwyO1awxhg
Similar Threads
-
Extend thread on a socket head bolt
By justask4 in forum METALWORK GENERALReplies: 22Last Post: 31st Oct 2019, 10:49 PM -
Cutting a coarse left hand thread.
By Boringgeoff in forum METALWORK GENERALReplies: 52Last Post: 12th Sep 2019, 10:23 AM -
Imperial and Metric Bolt Thread and Torque Chart
By moorebrm in forum METALWORK GENERALReplies: 5Last Post: 31st May 2016, 01:48 AM -
1" BSP as a nut & bolt thread.
By bob ward in forum METALWORK GENERALReplies: 2Last Post: 22nd Jul 2014, 03:29 PM -
american thread bolt 8-32 where?
By old_picker in forum METALWORK GENERALReplies: 6Last Post: 6th Aug 2011, 06:47 PM