Needs Pictures: 0
Results 1 to 15 of 25
Thread: Why did this stop cutting?????
-
10th Sep 2020, 04:38 PM #1
Why did this stop cutting?????
I have a 180mm diam. piece of G.C.I. mounted in the 4-jaw, and a brand new not cheap 127mm hole saw, (Bi-meatal Coblat) in the tail stock.
Running the lowest RPM I can achieve (130RPM) it started cutting well, no heat and no chatter, ...... got in about 2.5-3mm and it just stopped cutting.
The teeth are perfect, sharp as buggery, but I can apply enough pressure to stall the lathe without any sign of further cutting.
I haven't come across this before, so looking for answers and a solution please.
Hole Saw cut stalling.jpg
-
10th Sep 2020, 04:49 PM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
How many of these plugs at 127 mm dia have you down before?
-
10th Sep 2020, 05:26 PM #3Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Could be because the gullets of the teeth are filled with CI dust. Once they are full the saw won't be able to cut any more. Have you tried "pecking" at the cut? I.e. frequently withdrawing the hole saw and brushing the teeth clean.
Chris
-
10th Sep 2020, 06:03 PM #4
-
10th Sep 2020, 06:05 PM #5
-
10th Sep 2020, 06:09 PM #6Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
Bit late now, but a carbide tipped holesaw would probably be better; significantly fewer teeth and massive gullets would reduce the load and keep the swarf under control.
https://www.totaltools.com.au/145221...lesaw-h1271270
-
10th Sep 2020, 06:28 PM #7Senior Member
- Join Date
- May 2015
- Location
- Richmond
- Posts
- 214
-
10th Sep 2020, 06:45 PM #8I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,297
Don't know what your lathe is, but first guess would be once you add the drag from the sides of the teeth, your machine just doesn't have the oomph to do it? That size holesaw in cast is a fair bit of load... Second guess would be you've hit a hard spot or inclusion in the cast...
I assume you're trying to remove a ring around the outside, to keep for another project? What about grinding a grooving tool (with plenty of relief to account for the curve of the groove) and trying that? At the very least, it should open up the region around the holesaw groove a bit, which would allow you to disprove my first guess...
-
10th Sep 2020, 08:37 PM #9Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
Possibly going to deep for the holesaw?
-
10th Sep 2020, 08:38 PM #10Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Try coolant, if the cast gets over hot it may be jamming your cutter, could also be the material getting hard due to excessive heat.
-
10th Sep 2020, 08:48 PM #11Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
127 x pi is just shy of 400mm circumference ... assuming 4mm tooth pitch, that's 100 teeth ... assuming about 2mm tooth width, that's 200mm of cutting edge to push. You're gonna need a lot of power to do that.
A TCT holesaw of that diameter might only have 5 or 6 teeth, even if they're a bit wider you're still looking at less than 10% of the power.
-
10th Sep 2020, 08:59 PM #12
Swarf was not any part of the issue in this case.
I did see those, but the description is:
"H127 Series TCT Multi Purpose Holesaw range can be uses to cut timber, hardwood, softwood, MDF, plaster board, compressed fibre cement sheet, cement sheet, plastics, ceramic tiles and abrasive materials.
No mention of any metals of any kind at all, which is why I didn't get one.
-
10th Sep 2020, 09:00 PM #13
-
10th Sep 2020, 09:03 PM #14Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
10th Sep 2020, 09:13 PM #15
Still have no idea at all why this happened, but the job is done now.
Out of desperation I drilled about 20 or so 3.5mm holes in the shallow groove that the holesaw cut before it started skating on the surface.
That got it started again, and I cut the rest of the depth dry, and very little heat was produced at all, 40-45 degrees according to the laser doohickey.
It never looked like skating again, just steady cut all the way to 32mm depth.
Similar Threads
-
When does it all stop lol
By wbleeker in forum METALWORK GENERALReplies: 15Last Post: 25th Jul 2014, 09:11 PM -
Plasma cutting capacity or waterjet cutting connections?
By jhovel in forum METALWORK GENERALReplies: 25Last Post: 4th Apr 2014, 11:06 AM -
Thread cutting with a lathe stop