i have a manual burnout oven that is difficult to maintain 350-400 degree temperature for melting out the wax. But it runs like a champ for the rest of the burnout cycle. My question is can I do a melt out of the wax in a craft oven (or a toaster oven at 350 degrees) for the appropriate time and then move it back to my burnout oven to complete the cycle?