I wanted to put a groove in either side of a level I am making. Just to be able to grip it better. Not having a ball end mill on hand, I decided to try a ball end carbide burr.
Put the burr in the collet and just nipped it up to check if I had enough clearance.
Set it all up very carefully and proceeded to start the cut. The burr was cutting wonderfully, then I realised my groove was running downhill. ID10T machine operator forgot to tighten the collet properly. GRRRRRR.
id10t.jpg
Peter
-
25th Jul 2020, 09:15 PM #2Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Been exactly there before. My sympathies. Now all you need to do is start at the same point with the same torque on the collect for the other side.
Sent from my SM-G973F using Tapatalk
-
25th Jul 2020, 11:19 PM #3Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
To make you feel better, I think most of us are/would be guilty of doing something similar in our life.
To recover it, just machine it level to the top and bottom, at least it's not a FUBAR!!
KrynTo grow old is mandatory, growing up is optional.
-
25th Jul 2020, 11:33 PM #4I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,300
Don't think I've ever done that and not realised just before the endmill hit the workpiece...
Forgetting to lock the quill, however.... I've done that. And more than once.
As said, at least it's a decorative/function feature rather than a critical dimension, just make it wider, and say you did it so you can get a better hold!
-
25th Jul 2020, 11:49 PM #5Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Just leave as an Aldi reminder.
-
26th Jul 2020, 09:46 AM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Peter, I think I have a 5/8" or similiar ball mill if you want to borrow one to deepen the groove.
Michael
-
26th Jul 2020, 09:31 PM #7Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
Thanks for that kind offer Michael, however the job is done now. I just widened the groove with a couple of passes. Not as pretty as I had originally anticipated but will do the job.
level 001.jpg
peter
Similar Threads
-
Error message
By AlexS in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 1Last Post: 16th Sep 2013, 09:37 AM -
Posting Error
By Scott in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 8Last Post: 24th Nov 2012, 11:06 AM -
Random error
By chrisb691 in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 23Last Post: 27th Jun 2012, 01:34 PM -
Forum error?
By AlexS in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACKReplies: 5Last Post: 16th Aug 2008, 09:46 PM