    Default Scraping a cast iron surface plate

    I recently came into a 1245mm x 750mm cast iron surface plate. Unfortunately moisture had got under the cover and a lot of spots where heavily pitted the plate also had a number of scratches in it. It weighs 280kg so before I unloaded it at my place I took it to get surface ground it should be back within a week.

    I would eventually like to scrape if flat enough to use to scrape straight edges and the like. I am investigating methods that allow scraping plates from smaller reference surfaces. I know this is possible and in fact a common on really large machine tools. I have found this video which shows the use of only a straight edge and an autocollimator to scrape a surface plate https://www.youtube.com/watch?time_c...ature=emb_logo unfortunately its not in English so the explanation of the technique is not clear.

    Can anyone explain the method used here and are does anyone else know of other methods for scraping a larger plate from smaller reference?

    Regards

    Eric

  2. #2
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Robin Renzetti just put up the first video in a series about using an auto collimator.

  3. #3
    Join Date
    Jul 2010
    Location
    Melbourne
    Posts
    9,088

    Default

    Quote Originally Posted by lamestllama View Post
    1245mm x 750mm
    How much smaller are you thinking? and how do you know it is flat?

    Respect for even thinking about trying. I guess it will give you something to past the time if you end up in lock down again.

  4. #4
    Join Date
    Aug 2015
    Location
    Melbourne, Australia
    Posts
    843

    Default

    Renzetti also did another vid re lapping in a large plate using a smaller plate: https://www.youtube.com/watch?v=Qm0QerRvtJQ. May not be useful for cast iron - dunno.

  5. #5
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,479

    Default

    Hi Guys,

    The three plate lapping method works well, but there are some gotchas.
    Best Regards:
    Baron J.

  6. #6
    Join Date
    Jul 2011
    Location
    Adelaide
    Posts
    837

    Default

    Quote Originally Posted by StrayAlien View Post
    Renzetti also did another vid re lapping in a large plate using a smaller plate: https://www.youtube.com/watch?v=Qm0QerRvtJQ. May not be useful for cast iron - dunno.
    I have never heard of cast iron plates being lapped. I would need a material softer than cast iron for the lap so that the abrasive got embedded in it rather than the surface plate. His collimator build was very interesting.

  7. #7
    Join Date
    Jul 2011
    Location
    Adelaide
    Posts
    837

    Default

    Quote Originally Posted by Stustoys View Post
    How much smaller are you thinking? and how do you know it is flat?

    Respect for even thinking about trying. I guess it will give you something to past the time if you end up in lock down again.
    The plan would be to buy or acquire over time whatever was needed.

    Those Japanese guys I linked to where clearly using a straightedge and a collimator to make that large plate flat. Having done some reading I think I understand how they went about it.

    A 4ft or even 3ft straight edge should be quite possible to find in South Australia I would probably have to pay to have someone certify it as for collimator I am thinking US Ebay?

    Of course it all depends on how flat it comes back from the surface grinder.

    I have a Biax scraper so it isn't perhaps as brave as attempting it with a hand scraper.

    If I mess it up I would just take it back to the grinder so the risk is kind of low.

  8. #8
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,479

    Default

    Hi Guys,

    Cast iron is perfect for lapping a cast iron plate. The fact that they are similar metals won't alter the lapping process.

    Once the diamond grains have been pressed into the lap its the lapped surface that will have material removed from it. The lap of course will get clogged by the material removed and will have to be cleaned and re-charged with diamonds.
    Best Regards:
    Baron J.

  9. #9
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Eric, you'll need to live to 130+ to finish all those projects.
    Kryn
    To grow old is mandatory, growing up is optional.

  10. #10
    Join Date
    Jul 2011
    Location
    Adelaide
    Posts
    837

    Default

    Quote Originally Posted by KBs PensNmore View Post
    Eric, you'll need to live to 130+ to finish all those projects.
    Kryn
    Kryn, I expect to live like I will live at least that long.

  11. #11
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by lamestllama View Post
    T

    A 4ft or even 3ft straight edge should be quite possible to find in South Australia .
    how much do you want to pay for one?

  12. #12
    Join Date
    Jul 2011
    Location
    Adelaide
    Posts
    837

    Default

    Quote Originally Posted by eskimo View Post
    how much do you want to pay for one?
    Why do you ask? But it would depend on how provably straight it was.

  13. #13
    Join Date
    Mar 2014
    Location
    South of Adelaide
    Posts
    1,227

    Default

    Must be a pretty dodgy grinding place, should be able to get it ground so you don't have to scrape it.

  14. #14
    Join Date
    Jul 2011
    Location
    Adelaide
    Posts
    837

    Default

    Quote Originally Posted by snapatap View Post
    Must be a pretty dodgy grinding place, should be able to get it ground so you don't have to scrape it.
    I would be surprised if the owner of a surface grinder big enough to grind that plate were dodgy.

    Out of interest what sort of geometrical tolerances do you think a surface grinder should be able to hold over that size? (1245x750)

    If it were flat such that it lay between two parallel planes 0.007mm apart then it would be a ISO grade 0 and between two parallel planes 0.014mm apart it would be a grade 1 (the other consideration being local flatness but I feel this is less of an issue with a surface grinder than with other methods of generation). If grade 1 was achieved I would be happy and the plate could be used as is for scraping the parts I actually want to scrape. Including a straight edge.

    The guy driving the grinder thought he might achieve 0.01mm. However one of the grinding companies I visited with the plate indicated they would expect to achieve 0.025mm (albeit on a Blanchard grinder and it will in fact be ground on a peripheral wheel grinder).

    I am not convinced that grinding will produce the geometrical flatness that you seem to think it should but maybe I will be surprised and delighted. Indeed I wonder why new granite plates are still hand lapped after grinding to achieve flatness?

  15. #15
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,479

    Default

    Hi Guys,

    Actually I would be very delighted to get 0.02 or 0.03. It would not only take a very good machine operator, but an extremely good grinding machine to achieve better !

    I personally would be very interested to find out what is actually obtained !
    Best Regards:
    Baron J.

Page 1 of 2 12 LastLast

Similar Threads

  1. WTB-Cast Small Cast Iron Lapping Plate
    By Betnorm in forum WANTED TO BUY
    Replies: 4
    Last Post: 19th Nov 2019, 01:01 PM
  2. 12 x 24 inch cast iron surface plate
    By iron bark in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 4
    Last Post: 3rd Mar 2018, 01:30 PM
  3. Large Cast Iron Plate - What for?
    By DSEL74 in forum METALWORK GENERAL
    Replies: 14
    Last Post: 28th Jul 2015, 12:21 PM
  4. BBQ cast iron plate for sharpening?
    By Dengue in forum METALWORK GENERAL
    Replies: 4
    Last Post: 24th Aug 2014, 08:33 PM
  5. SOLD: Cast iron table suitable for surface plate etc
    By Greg Q in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 6
    Last Post: 28th Aug 2013, 02:12 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •