    I just did a job using a new 2-flute solid carbide slot drill in 6061 aluminium on my CNC mill.
    A quick check with a caliper said about 3.85 mm, so I "assumed" it would cut 4 mm.
    Not so, it actually cut like a 3.85mm - duh !

    So, measured carefully the flutes, also 3.85 mm.
    5/32" is 3.97 mm, 9/64" is 3.57 mm, so it does not appear to be imperial.

    Is it normal for cutters like this, probably purchased cheap somewhere, to be somewhat smaller than the expectation ?

    I will start checking actual cutter dimensions for future jobs.

    Keep well,
    John

  2. #2
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,079

    Default

    Just had a look through the Guhring catalogues and their tolerance on flute diameter is generally h10 or e8, which would make a 4mm endmill 3.952 - 4.000mm or 3.962 - 3.980 respectively.

    Some tolerance is to be expected, but 0.15 under is waaay not acceptable.

  3. #3
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    I've found cheap Chinese carbide is sometimes under size by a far amount. I assume they are starting with a nominal size blank and then grinding a bit off.

    Not a big issue for me using CNC so long as I remember to check actual cutter size...

  4. #4
    Join Date
    Mar 2013
    Location
    Mt Pleasant SA
    Posts
    126

    Default

    Back in the olden days HSS slot drills always had a (-) tolerance whereas endmills always had a (+) tolerance but agreed -0.15 on 4mm is a bit gross. Hardly the end of days tho'.

  5. #5
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,475

    Default

    Hi Guys,

    I think I would prefer undersized slot drills to oversize ones, at least you can always take a finishing cut !
    Best Regards:
    Baron J.

  6. #6
    Join Date
    Jun 2016
    Location
    Sydney
    Posts
    283

    Default

    Dear me. Where did that come from???
    But yes, if it is undersize you can handle that. In fact, I often prefer to do it that way, after micing the cutter carefully.

    Cheers
    Roger

Similar Threads

  1. Tap Drill Size Calculator
    By KBs PensNmore in forum CONVERSIONS & CALCULATIONS
    Replies: 0
    Last Post: 21st Apr 2020, 10:33 PM
  2. Tap Drill Size Calculator
    By KBs PensNmore in forum CONVERSIONS & CALCULATIONS
    Replies: 1
    Last Post: 19th Jun 2019, 06:40 PM
  3. What size drill for a 5/16 reamer?
    By ventureoverland in forum METALWORK GENERAL
    Replies: 31
    Last Post: 8th Sep 2014, 10:12 PM
  4. Slot Drill Sharpening - A Case of Making Do ( or not really )
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 12
    Last Post: 29th Oct 2013, 09:37 AM
  5. tee slot size
    By welder in forum METALWORK GENERAL
    Replies: 3
    Last Post: 25th May 2010, 05:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •