    Default Vintage brass fire extinguishers- How to remove dents?

    Good Day,

    Anyone have any experience removing dents from old brass fire extinguishers? I have an old 2 gal foam fire extinguisher that has a few dents in it, worst about 5 mm deep and 75 mm long. Googled "removing dents from fire extinguishers" and found nothing except removing dents from a tuba. Plenty of polishing info on line but I am actually going to repaint it the correct blue colour once restored. Going onto a vintage truck. Thought about heating it up and cooling the dented area quickly to anneal it a bit then push it out with a shaped bit of wood. Don't want to stuff it up however and anyone's experience would be most appreciated. Likewise the base is a bit battered and thought about annealing it, removing the wire ring, then bead rolling it if I can find someone locally with a bead roller.

    Cheers,
    Attached Images Attached Images

  2. #2
    Join Date
    Jun 2007
    Location
    Ipswich QLD
    Age
    68
    Posts
    1,997

    Default

    Cant see the dent ? If it is on the main body and seals tight you can do a few things. Fill it with air and see ifvit pops out as you heat it.
    Get a bucket of water rag and heat the area and about around it, soak the rag and quench the area this will shrink and pop the dent out.
    As you say bit of timber or metal used internally heat and force the dent out.

    Good luck

  3. #3
    Join Date
    Jun 2007
    Location
    Ipswich QLD
    Age
    68
    Posts
    1,997

    Default

    As for painting they look far better polished

  4. #4
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    168

    Default

    Try deflating a soccer ball and placing inside where dent is. Slowly inflate and gently tap with a soft hammer or leather mallet. Ive used this to push out dents on car panels.
    and yes they do look better polished up.

  5. #5
    Join Date
    Sep 2013
    Location
    Melbourne
    Posts
    30

    Default

    Quote Originally Posted by wheelinround View Post
    As for painting they look far better polished
    Maybe so, but on a military truck that was not such a good idea! Dead giveaway from the air.
    That's where mine is going and not beside the fireplace.

  6. #6
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    a little bit of bog.

  7. #7
    Join Date
    Jun 2007
    Location
    Ipswich QLD
    Age
    68
    Posts
    1,997

    Default

    Quote Originally Posted by Jacqualos View Post
    Maybe so, but on a military truck that was not such a good idea! Dead giveaway from the air.
    That's where mine is going and not beside the fireplace.
    How you fit a fire truck beside a fireplace is mind boggling. My wife wont let me bring tools in unless a job needs doingVintage brass fire extinguishers- How to remove dents? Darn but wirh impending invasion Blue will be best.

    The soccer ball is ideal for car panels as they are not thick were as the copper side wall needs to be due tp pressure. It just might work tho.

  8. #8
    Join Date
    Jun 2007
    Location
    Ipswich QLD
    Age
    68
    Posts
    1,997

    Default

    Quote Originally Posted by azzrock View Post
    a little bit of bog.
    Wash your mouth out Vintage brass fire extinguishers- How to remove dents?Vintage brass fire extinguishers- How to remove dents? lead wipe would be the go too of the day

  9. #9
    Join Date
    Sep 2005
    Location
    Bendigo
    Age
    60
    Posts
    419

    Default

    Google "bullseye pick", it is the tool used in auto bodywork to get to dents in hard to reach places.

  10. #10
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    If you're just painting I would also go bog.

  11. #11
    Join Date
    Sep 2013
    Location
    Melbourne
    Posts
    30

    Default

    Quote Originally Posted by BobL View Post
    If you're just painting I would also go bog.
    I could, but I really dislike bog. Maybe get most of the dent out then live with it. It adds some character!

  12. #12
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    If your painting it, just bog it up as others have suggested, you will never get them perfect anyway, unless you really know what your doing and have a lifetime experience.

    There are some good body fillers on the market, that will stay on and outlast us.
    Using Tapatalk

  13. #13
    Join Date
    Sep 2019
    Location
    Newcastle, AU
    Posts
    238

    Default

    Take a look at the way people remove dents from motorcycle fuel tanks for some ideas.

    I have gotten dents out of steel fuel tanks before with a hot glue gun and some screws - put some glue down in a blob, work the screw into it, let it all cool then gently pull on the screw with vice grips. Works best if you work from the edge of the dent in.

    I often put a bunch of blobs and screws down at once and work them slowly and evenly around the inside of the dent.

    Never tried it on brass but I would give it a go before using bog, myself...

  14. #14
    Join Date
    Sep 2013
    Location
    Melbourne
    Posts
    30

    Default

    Quote Originally Posted by J.C. View Post
    Take a look at the way people remove dents from motorcycle fuel tanks for some ideas.

    I have gotten dents out of steel fuel tanks before with a hot glue gun and some screws - put some glue down in a blob, work the screw into it, let it all cool then gently pull on the screw with vice grips. Works best if you work from the edge of the dent in.

    I often put a bunch of blobs and screws down at once and work them slowly and evenly around the inside of the dent.

    Never tried it on brass but I would give it a go before using bog, myself...
    Thanks J.C. for your suggestions. Think I will give that a try first. I have a glue gun and have read about paintless dent removal so I should be able to get a good pull from the outside. I can live with a few defects even if it isn't show perfect with bog. Just put the dent to the back of the holder on the truck.

  15. #15
    Join Date
    Feb 2013
    Location
    Laidley, SE Qld
    Posts
    1,039

    Default

    The short answer is fill the fire extinguisher with water and put it in the freezer.

    The longer answer is as above but be cautious about how much water you put in, you don't want to create a volume of ice larger than that of the extinguisher or create too high an air pressure within the extinguisher.

    Water expands by around 9% when it freezes, filling the extinguisher to 90% means the trapped 10% of air will reduce in volume to 1%, Boyles Law comes into play.

Page 1 of 2 12 LastLast

Similar Threads

  1. Lathe from a fire
    By SurfinNev in forum METALWORK GENERAL
    Replies: 6
    Last Post: 4th Jul 2018, 06:18 PM
  2. VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
    By thumbsucker in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 7
    Last Post: 18th Mar 2013, 03:36 PM
  3. help fire damage
    By wodstok in forum WELDING
    Replies: 6
    Last Post: 24th Sep 2010, 10:04 PM
  4. Remove machining marks in brass?
    By neksmerj in forum METALWORK GENERAL
    Replies: 7
    Last Post: 18th Oct 2007, 11:44 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •