    Default O Granowski Power Hacksaw

    Hello All

    Today I picked up, with the help of a crane, my latest acquisition. It is an O Granowski Power Hacksaw that was originally made in Melbourne. The old bloke I got it off told me he tendered for it when the Ipswich Rail Workshops closed down and got it for scrap price. He didn't charge scrap price but both of us seem happy with the deal.

    It turns on and runs which is a great start. Unfortunately it does not have a blade fitted and the rear mount for the blade may not have been assembled correctly. I can see it is meant to tension but I am not sure how the blade attaches.

    So the gold plated solution would be if someone has a scanned copy of the original manual. I would be very happy with a description or photo of the blade mounting.

    I would also be interested to find out how old this hacksaw is. It looks like if I give it a cleanup and service I should get at least 50 years out of it. The same probably can't be said for me.

    Thanks

    Steve

  2. #2
    Join Date
    Nov 2019
    Location
    Brisbane
    Age
    69
    Posts
    452

    Default Power hacksaw

    Hello Steve.
    Power hacksaws are usually measured from the center of the blade holes. You can judge it's capacity by the clearance from the bottom of the overarm to the teeth on the blade. I have a 12" and a 16" saw and use them both often. They are economical to run but a bit slow on solid stock. Take care at getting the vice fixed jaw at right angles to the blade. it makes a big difference.
    A few pics would be nice.
    BC

  3. #3
    Join Date
    May 2020
    Location
    Willowbank QLD
    Posts
    535

    Default

    I have now worked out the blade mounting. The threaded piece that tensions the blade was broken so I made a new one. I have completed a test cut and for 1 inch bar it took 30 seconds.

    I will include a photo, as the new guy here the moderators may not allow it.

    Steve
    Attached Images Attached Images

  4. #4
    Join Date
    Nov 2019
    Location
    Brisbane
    Age
    69
    Posts
    452

    Default Hacksaw

    Hello Reidy41.
    I see your at Willowbank. We went past you on the way to Warwick Saturday. My shed is at Geebung. Clean that saw up and it should last 50 years. Check the electrics, mine was dangerous when I got it. All the old rubber insulation had perished.
    Regards
    BC

  5. #5
    Join Date
    May 2020
    Location
    Willowbank QLD
    Posts
    535

    Default

    BC

    I know Warwick very well. I went to high school there and Mum and Dad now live in town. I grew up 40 k's west at a District called Thanes Creek. My sister is out the other side of town toward Killarney.

    The electric motor is not original and looks in good condition. Someone has removed the cutoff switch which I may replace.

    Steve

  6. #6
    Join Date
    Nov 2010
    Location
    Frankston south
    Posts
    102

    Default

    I Have the same machine, I'm happy with it so far..I see yours has an oil pump, what is that feeding?

  7. #7
    Join Date
    May 2020
    Location
    Willowbank QLD
    Posts
    535

    Default

    As it stands there is a plastic tube that runs from the tank and did not go anywhere. I cleaned out the tank and put some soluble oil in it. It pumped that up at about 1/2 a liter a minute. It drains back to the tank.

    Just near the down stop there is a vertical metal rod that does not appear to have any purpose in life. I am summarising that the oil feed should clamp to that and the height adjusted dependent on the diameter of the stock being cut.

    The plastic tube is about as flexible as a 90 year old man on a cold winters morning so I will replace it in the near future and devise a clamp.

    Steve

  8. #8
    Join Date
    Aug 2010
    Location
    Melbourne
    Posts
    25

    Default Granowski Power Hacksaw

    Hi Steve and Waxen,

    I also have a Granowski power hacksaw #501. I bought it off ebay 10 years ago and have just started the restoration of this saw. Did you disassemble the main spindle? On mine, there is a 176 tooth spur gear and it's mated to a 16 tooth pinion. My question is that I want to take off the large gear and am wondering if it has a press fit, i.e., needing heat to expand the hub and pull it off the main shaft? I did a search and found your thread here. All else is fine with this saw. Just a pull down, rust removal, paint, lube and it should be good to last another 100 years. TIA.

    George

  9. #9
    Join Date
    May 2020
    Location
    Willowbank QLD
    Posts
    535

    Default

    George, I have not disassembled mine. If you need a close up photo of a part just let me know.

    Steve

  10. #10
    Join Date
    Aug 2010
    Location
    Melbourne
    Posts
    25

    Default

    Thanks Steve,

    Other than this obstacle I am fine. I pulled down the dampener today. What a mess!

    Funny thing, I was given 20 x 17" new blades and I bought the saw to use them, not the other way round. It's been fun so far, tomorrow I will use heat and see how I go. The pain is that the large gear has 5 spokes and my gear puller is a standard 3 jaw. I will improvise.

    Cheers,
    George

Similar Threads

  1. Joe's power hacksaw
    By Michael G in forum METALWORK GENERAL
    Replies: 2
    Last Post: 23rd Jun 2019, 08:56 PM
  2. power hacksaw ID
    By dodge at4 in forum ANTIQUE AND VINTAGE MACHINERY
    Replies: 2
    Last Post: 9th Jun 2016, 02:13 PM
  3. SOLD: power hacksaw
    By mistercartoon in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 2
    Last Post: 19th Mar 2011, 05:51 PM
  4. Power Hacksaw
    By Bryan in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 15
    Last Post: 13th Oct 2010, 07:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •