Hi all,
I'm giving a 1930s qualcast push mower some resto love.
The wheels have these bearings in them. One is save able, the other is rusty powder.
IMG_20200520_173554.jpg
I'm not even sure how they are called. I took them to a bearing place and they just said they were old and can't supply.
Any clues as to getting replacements?
Many thanks,
Greg
-
20th May 2020, 06:52 PM #2
-
20th May 2020, 06:57 PM #3Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Thanks BaronJ, it is a single row of bearings in there .. but I think the magic words are "ball race cage"!
-
20th May 2020, 07:11 PM #4Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
It would be a caged thrust brg i reckon, a brg supplier should have or be able to get.....
-
20th May 2020, 07:17 PM #5Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
I did neglect to say that the whole thing fits into a recess with one side sitting flat (the side facing down in the pic) and a shaft running through the center. The shaft has an angled section that rests on the inner part of the bearings.
I'll get some more pics ...
EDIT: shed, our posts crossed in mid air. Interesting - if I can't actually find the real thing to fit, I can always make some bushing for alignment and actually use a thrust bearing. Could work.
-
20th May 2020, 07:25 PM #6Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
Actually you might have more luck at a bike shop https://hollandbikeshop.com/en-gb/bi...silver-578372/
-
20th May 2020, 07:26 PM #7Golden Member
- Join Date
- Apr 2018
- Location
- Drouin Vic
- Posts
- 634
It looks very much like a bicycle head-stem bearing, might be worth trying a bike repairer?
-
20th May 2020, 08:14 PM #8Senior Member
- Join Date
- Feb 2009
- Location
- jilliby nsw
- Age
- 71
- Posts
- 111
I was going to say bike shop too, the other possibility is that seeing the cage looks ok just replace the balls. I have in the past bought them at bearing places but bike shops might have them too. One more choice is get something at bike shop with the correct size balls and swap them to your cage. cage can be cleaned up with some rust dissolver. Good luck with it.
-
20th May 2020, 09:25 PM #9Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,552
Replace them with sealed roller bearings?
-
20th May 2020, 09:41 PM #10Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
5/32?
Failing being able to find a cage the same size or reuse the ones you have with new balls, just leave them out and add an extra ball or two.
May make reassembly a little trickier, but other than that you'll never know the difference.
-
20th May 2020, 10:16 PM #11
I have replaced plenty ball bearings without cages on bikes. They used to sell the balls at bike repair shops over here in the Netherlands, not sure if they stil do.
If you go that route, just put plenty of grease in the race and stick the balls in. They wil hang on to the grease during assembly.
Usually the number of balls is one ball less than chuckfull ;-)
Peter
-
20th May 2020, 10:23 PM #12Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
-
21st May 2020, 09:40 AM #13Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Most bearing shops sell loose balls
-
21st May 2020, 10:15 AM #14Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Wow guys, thanks. I think we're on the money here - either a bike shop or just lose the cage and pack with grease and extra balls as per a bicycle - as it happens, while I was at bearing shop I got a bunch of balls in case I needed to fashion a cage or two. Nice!
Just a note that may have been missed - there are two in the mower (one for each wheel) and I can reuse one - but the other side is toast.
As an aside: Here are pics showing where they live - so I thinking the lose-the-cage-and-pack-with-grease thing should work just fine:
IMG_20200520_183855.jpgIMG_20200520_183907.jpg
Thanks all - that's given me something to go on. The old mower might yet still live again. Here it is:
IMG_20200331_180149.jpg
Thanks again,
Greg.
-
21st May 2020, 05:29 PM #15
Hi Guys,
I've got one of those ! Its been hiding in the back of the garage for the past four decades, ever since we got a flymo. I had totally forgoten about it until the wife saw that picture and reminded me we have one of those.Best Regards:
Baron J.
Similar Threads
-
Coal or coke supply
By 12bolts in forum THE SMITHYReplies: 5Last Post: 18th Jul 2016, 11:17 PM -
On-line Industrial Supply
By RayG in forum METALWORK GENERALReplies: 5Last Post: 24th Apr 2012, 07:53 PM -
Transarc 200 supply options
By Bryan in forum WELDINGReplies: 2Last Post: 30th Nov 2010, 10:05 PM -
axle supply
By danielhobby in forum TRAILERS & OTHER FABRICATED STUFFReplies: 0Last Post: 29th Nov 2010, 12:29 PM -
Basic supply question
By Driver in forum METALWORK GENERALReplies: 5Last Post: 3rd Jan 2005, 09:54 AM