Another bit of kit that I saw in an email. For those that like to make their own bits of Kit, some strap clamps, plus in the background, there's an adjustable stop arrangement for the milling machine vise.
https://www.homemadetools.net/forum/strap-clamps-t-nuts-79236?utm_source=newsletter&utm_medium=email&utm_campaign=05-
KrynTo grow old is mandatory, growing up is optional.
-
17th May 2020, 09:45 AM #2Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
I like the design (with the height-setting threaded bar on one side).
As a refinement;
- I would use a larger threaded bar, and grind/mill 6 flats on the end instead of a screwdriver slot.
- Maybe have a finer thread on that bar, for better adjustment.
P.S. Thinking about making T-slot nuts, a lot of the work time is milling the Ts.
Does anyone know a source for T profile steel? Like pre-rolled from a mill.
I'm assuming the factories that churn out stuff like this:
https://www.nei.com.au/wp-content/up...nhanced-en.pdf
have a source for precision cut profiles, and they just cut to nut length, thread, and blacken?
-
17th May 2020, 10:32 AM #3Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
also a larger head for the bolt that sits in top of the table.....I recon you'd leave dents on the table when tightening down.?
-
17th May 2020, 11:43 AM #4Golden Member
- Join Date
- Oct 2008
- Location
- Cairns, Q
- Posts
- 666
FWIW I keep a couple of handfulls of the old 1c and 2c copper coins in the top channel of the press. Not only are they useful for preventing the press ram from marking delicate work, but I also use them under the heads of the adjusting bolts on the strap clamps to protect the mill table. The 2c coins are just the right size for this.
Frank.
-
17th May 2020, 12:28 PM #5Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Nigel, I think you'll find that they are not a rolled section, probably just mill the steps on them, out of the bar size required. At least that's what mine look like. Would be easy to manufacture if you had a horizontal mill, 2 cutters side by side with a spacer of the right size.
I did some small ones for an X2 mini mill I had, that was a pain as you couldn't take a decent cut. I just milled them out of some MS 16X8 flat bar, in about 300mm long length after I drilled the ends and bolted down with a bolt at each end. then drilled, tapped, and then cut to length.
KrynTo grow old is mandatory, growing up is optional.
-
17th May 2020, 12:47 PM #6
Hi Kryn, Guys,
When I've made some, that is all I do, just mill the sides of some key steel of the right width and cut lengths off as required. Invert in the drill vise, move against a stop, clamp then and drill and thread.Best Regards:
Baron J.
-
17th May 2020, 11:47 PM #7Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
By coincidence I actually made some tee nuts tonight for my rotary table. Turned out that the 19x19ish hot rolled bar I had was good for width and height so I just ran a roughing endmill down each side. Drilled and tapped then cut the strip up on the bandsaw.
A tapping head would be nice though
Steve
-
18th May 2020, 06:23 PM #8
Hi Steve,
For tapping through holes like that I bought some spiral taps. I've found that you can go all the way through at about 100 rpm and the chip comes out like it does when drilling. When China comes back to life I'm going to get a set of metric ones. Although I do have sets of M6 and M8. Unlike hand taps there is only one tap, not three. Useless for blind holes though.Best Regards:
Baron J.
-
18th May 2020, 11:40 PM #9Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
Making Strap/Hold Down Clamps
Yes, some spiral taps are on my list to buy, but haven’t got there yet.
I actually managed to power tap the 8mm holes in the tee nuts, but just had the hand tap in the drill chuck on the mill. After about the third hole doing each hole in about 3 steps I hit the right combination of lube and quill pressure and the rest of the holes went through in one hit.
Steve
Similar Threads
-
Toolmakers Clamps, making and using,
By metaler in forum METALWORK PROJECTSReplies: 0Last Post: 31st Oct 2016, 07:47 AM -
Show us your weld table jigs,fixtures, clamps and hold downs
By Grahame Collins in forum WELDINGReplies: 51Last Post: 30th May 2016, 08:24 AM -
Pattern for Biax leather grip strap
By jhovel in forum METALWORK GENERALReplies: 6Last Post: 18th Feb 2016, 10:49 PM -
Bandsaw clamps: The making of...
By .RC. in forum METALWORK GENERALReplies: 2Last Post: 1st Apr 2013, 09:10 PM -
What are strap clamps ?
By morrisman in forum METALWORK GENERALReplies: 6Last Post: 18th Sep 2012, 08:15 PM