3rd Mar 2020, 08:54 AM #1
Fly cutter for pocket knife blade slot
Thank you steamloco1954 for the thread about the fly cutter.
For a long time I have been searching for a method to form a nail nick slot in re made pocket knife blades.
To explain, I collect old time pocket knives and on some of the types I have acquired the blade is either worn away from sharpening or just plain broken off from abuse.
A sample pic below.
Hence the need to make a new blades. Until now i thought the only way was with a milling machine and slitting saw which I dont have.
What I do have is the lathe, a means to make a fly cutter and some HSS and a good drill press which has very little run out.
Also I have recently acquired a pretty good cross slide vice from racingtadpole. I am confident that the Drill Press will do the job as the load is minimal.
I'll keep you all posted with pics now as I am now able to transfer pics from the Android phone to the iMac.
GrahameWhittingslowe knife.jpg
-
3rd Mar 2020, 11:19 AM #2Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
Fly cutter
The old goat again
I would be more inclined to turn the flycutter in the lathe and mount the work in the crosslide vice.
From personal experience the drill press is for drilling and other processes lead to a disaster.
A flared cup wheel of around 320 grit would grind the feature in and hold the profile if not pushed to hard. I bought a T & C grinder that had some in the mess delivered. Only 40mm dia so a high RPM is needed. They were used to nick clearance in step drills at the transition point.
Regards
BC
-
3rd Mar 2020, 06:20 PM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
How about using the tip of a dove tail cutter to do the nail slot?
Michael
-
4th Mar 2020, 12:57 PM #4
Hi Steamloco1954
At the moment i have the equipment to attempt the process in the drill press.
The cross slide vice is a fairly big one and would not fit unless I sat it on the longitudinal lathe ways. Until I am sure the drill press won't work I will stick with the DP for the moment.
I tried some mounted stones I shaped with wheel dressing stick and mounted diamond point but the stoned crumbled away too easy. They were cheap ones .
Michael
Same workholding deal for the diamond point. The blade will have to nail nicked before it is shaped if I am to hold it it a QCTP holder which is the only way I can picture (in my head) of grasping it.
I am not dismissing your ideas out of hand but I will have to find out the hard way that the drillpress does not work.
Grahame
-
4th Mar 2020, 04:43 PM #5Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
Fly cutter
Hello Graham.
If your using a mounted point in a drill press you will find the rpm is way too low. The work will then crush dress the abrasive and cutting will be minimal. If you can clamp a die grinder to the drill quill and use the drill press only for feed, the abrasive will perform much better. My 320 grit cup wheels were chipped when I checked them so went to the bin. There are a few p120 cup wheels surplus to my needs if you want one. Approx 40 X 20 X 10mm. They are 38A and orange?
Send me a PM and I can post a wheel if it will help.
Regards
BC
Similar Threads
-
Stanley Knife Blade as Finishing Tool ?
By steamingbill in forum METALWORK GENERALReplies: 4Last Post: 13th Aug 2016, 12:10 AM -
Looking for a 3/16" x 1" woodruff slot cutter
By bob ward in forum METALWORK GENERALReplies: 10Last Post: 16th Nov 2014, 03:11 PM -
Pocket size layout guide for holes.
By aametalmaster in forum METALWORK GENERALReplies: 0Last Post: 19th Aug 2012, 04:24 AM -
Waldown knife / blade grinder, Info Wanted
By lightwood in forum METALWORK GENERALReplies: 9Last Post: 27th Apr 2012, 12:50 AM -
Small tee slot cutter
By neksmerj in forum METALWORK GENERALReplies: 4Last Post: 2nd Jul 2007, 01:16 AM