    Default Preventing flash rust - bunch o' bolts de-rusted using molasses

    I've had a bucket of lightly rusted bolts and other odd fixings sitting in molasses for the last couple of weeks and it has done a lovely job of removing the rust, but they flash rust quicker than they can dry in the sun at present. Manually wiping them off isn't an option as there's hundreds of them (it's my odds 'n sods fixings bucket).

    Any recommendations for post-molasses treatment of bulk items? For smaller runs I've dropped things into a large ziplock bag with some WD40 and squelched it around for a while which keeps the rust off until things are dry and can be oiled, but I'm operating at a different scale this time and could do with a better method.

    Cheers

  2. #2
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Moph,

    Bucket of boiling water to rinse off and then into a dry bucket. Spray with WD40.

    The boiling water will heat the items up causing them to dry off quickly, the WD40 will protect them until you can oil or otherwise treat them.
    Best Regards:
    Baron J.

  3. #3
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    If the bits already have a light rust, boil them in vigorously boiling distilled water. This will convert the red rust to a very thin layer of black oxide most of which will wipe off, the remainder will be a faint dull grey but somewhat protective but oil will add to that protection. If they eventually lightly rust again repeat the distilled water boil. Multiple light rusts and distilled water boils is effectively cold metal bluing and the more times it’s done the more protective the coating.

    Using vinegar, citric or oxalic acid (VCO) as a rust removal agent means less mess and no washing or immediate oiling needed when pulled from these solution. Blow completely dry with clean compressed air and don't let them get wet, and bag them and they won’t rust for some time. They can be painted directly over the dry VCO. They only need oil if you intended to store them for months.

  4. #4
    Join Date
    Sep 2006
    Location
    Mallacoota,VIC,Australia
    Age
    53
    Posts
    1,010

    Default

    Hot water is a good idea perhaps just tip hot water over them whilst their in say a garden sieve and then tip diesel over them.
    All The Best steran50 Stewart

    The shortest way to do many things is to do only one thing at once.

  5. #5
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    far out sounds like a pain. Send them all of to the electro plater.
    Um what happened did you have a bucket of molasses lying around then some how the bolt feel in there?
    what does molasses taste like?
    I heard i tee spoon a day. reverses the greying process in human hair.

  6. #6
    Join Date
    Dec 2015
    Location
    Perth
    Age
    42
    Posts
    31

    Default

    Quote Originally Posted by azzrock View Post
    far out sounds like a pain. Send them all of to the electro plater.
    Um what happened did you have a bucket of molasses lying around then some how the bolt feel in there?
    what does molasses taste like?
    I heard i tee spoon a day. reverses the greying process in human hair.
    No idea what it tastes like; I bought a 20L bucket from a feed store that I use for the lawn. I distribute it via fertigation (inject it into the irrigation system) every now and then. It apparently feeds beneficial microbes in the soil resulting in increased soil nutrient availability.

    Molasses contains chelating agents that bind with the rust and make it water soluble. The rust dissolves into the molasses/water solution leaving behind clean metal. Major advantage is it doesn't attack the base metal like stronger acids can; drawback is it's a slow method (2+ weeks typically).

    I'm not electroplating them. They're just a bunch of random fixings that come in handy every now and then, but certainly not worth spending money on.

  7. #7
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    hi moph. impressive.
    so im picturing. a very nice lawn/ garden. Interesting.
    So many solutions pop up on this site for annoying little problems.
    Hpw did you know about this??
    aaron

  8. #8
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by azzrock View Post
    what does molasses taste like?
    I heard i tee spoon a day. reverses the greying process in human hair.
    Taste depends on type, light molasses tastes like sugar cane, dark molasses in more bitter but apparently has more goodies in it.

    As kid I once ate more than I should have and got a severe case of the squirtz. It took me years to try it again.

  9. #9
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    haha. thats how you learn. do they desolve it in tea??

  10. #10
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    haha. thats how you learn. do they desolve it in tea??

  11. #11
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Yes is dissolves in tea. Horses really like it. SWMBO uses as a bribe/treat for her horse. It’s added to horse water troughs to get reluctant-dehydrating horses to drink more water.

  12. #12
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    lets not forget rum

  13. #13
    Join Date
    Nov 2011
    Location
    Port Sephens NSW Southside
    Posts
    123

    Default

    azzrock

    Is the rum for the horses, the rusty parts or you???

  14. #14
    Join Date
    Dec 2015
    Location
    Perth
    Age
    42
    Posts
    31

    Default

    The boiling water did the trick. Sieved them out of the molasses, cold water rinsed a couple of times, then the boiling water rinse followed by blowing them off with compressed air. Gave them a spray of RP7 then a quick shake in a bag with 3-in-1 oil. Let them sit out in the sun for a couple of hours before rummaging around in the tray with a clean cotton rag to get rid of the excess oil.

    They look good so far. No flash rust - some still have touches of surface rust and could likely have done with longer in the molasses, but they're good enough to go back in storage.

    First photo is after molasses, oiling and drying. The second image is just a stock image off the web (I didn't take a before photo) but is similar to how they looked before treatment. Quite an improvement.

    20200223_174143.jpg yCmPW8j.jpg

  15. #15
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    Lanox is an alternative product to WD40 etc, has lanolin in it and is claimed to have a better rust preventive action.
    A bit more expensive, get it at Bunnings, auto shops etc - spray or brush on versions.

Page 1 of 2 12 LastLast

Similar Threads

  1. Molasses rust removal
    By morrisman in forum AUTO RESTORATION
    Replies: 6
    Last Post: 1st Jan 2017, 07:45 PM
  2. Black rust & molasses
    By georgedgerton in forum METALWORK GENERAL
    Replies: 2
    Last Post: 26th Nov 2015, 11:30 AM
  3. HIGH TENSILE BOLTS Vs MILD BOLTS.
    By chambezio in forum METALWORK GENERAL
    Replies: 13
    Last Post: 3rd Jan 2014, 08:25 PM
  4. welding flash
    By mid life crisis in forum WELDING
    Replies: 4
    Last Post: 23rd Jun 2012, 09:29 PM
  5. Replies: 9
    Last Post: 2nd Jul 2009, 11:12 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •