Thanks Thanks:  0
Likes Likes:  0
Needs Pictures Needs Pictures:  0
Results 1 to 7 of 7

Thread: bandsaw speed

  1. #1
    Join Date
    Apr 2014
    Location
    Perth
    Posts
    134

    Default bandsaw speed

    hi
    is 1300 fpm to fast to cut aluminium on a bandsaw
    cheers steve

  2. #2
    Join Date
    Oct 2015
    Location
    melbourne
    Posts
    473

    Default

    Charts seem to say 600-1000fpm
    I've seen 50mm Al cut with a normal circular saw...which could be up to 10000fpm.
    Might depend on the thickness and teeth/inch of the blade.

  3. #3
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,080

    Default

    I've cut ally on a woodworking bandsaw, not sure how fast it was going, but definitely faster than any metal bandsaw.

  4. #4
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Guys,

    I've got a 10" inch chop saw that runs at 2800 rpm that is specifically intended for aluminium and has a cutting capacity of 100 mm square. I also cut 20 mm thick aluminium sheet on the vertical wood bandsaw without too much trouble.

    You do need to be aware that depending upon the size of material you are cutting, it can get very hot quite quickly.
    Best Regards:
    Baron J.

  5. #5
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Depends on the thickness.

    I regularly cut 6 mm Al on a 3000 fpm WW bandsaw.
    I use a wax lube - ie ores the was onto the cut line and sometimes onto the blade.

    Cutting thicker than this at this speed can start to gall in the cut.
    1000 fpm should be OK

    With the tables I cut up to 30 mm thick but I do use a composite blade - negative kerf teeth.
    With a WW blade it is possible for the saw to grab the work and tear out teeth.
    The teeth go flying off around the workshop like little bullets and the tables saw bucks around across the floor due to unbalanced blade.

    TsBladep.jpg

  6. #6
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Bob, Guys,

    My chop saw came supplied with all HSS blades ! Its only later that I fitted a TCT blade. The original wax lubrication doesn't work very well with the TCT one, the blade doesn't get hot enough to keep the wax liquid, so I use a WD40 spray can.
    Best Regards:
    Baron J.

  7. #7
    Join Date
    Aug 2019
    Location
    Revesby - Sydney Australia
    Age
    57
    Posts
    1,196

    Default

    Quote Originally Posted by BobL View Post
    tables saw bucks around across the floor due to unbalanced blade.

    I have been known to snap the teeth off the other side to balance a TCT !

Similar Threads

  1. High Speed No.O ???
    By Anorak Bob in forum THE HERCUS AREA
    Replies: 2
    Last Post: 8th Jun 2019, 10:19 PM
  2. Bandsaw blade speed.
    By BaronJ in forum METALWORK GENERAL
    Replies: 15
    Last Post: 2nd Feb 2018, 11:43 PM
  3. Wood Cutting bandsaw speed - budget workaround
    By steamingbill in forum METALWORK GENERAL
    Replies: 0
    Last Post: 25th Mar 2016, 02:54 PM
  4. Replies: 27
    Last Post: 15th Oct 2014, 08:34 AM
  5. The Need for Speed
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 4
    Last Post: 27th Jan 2011, 02:10 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •