Results 1 to 5 of 5
  1. #1
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,559

    Default Mill tool storage

    I was asked the other day how to store mill tooling in a drawer. I store mine vertically -
    P1040785.JPG
    but the question was put to me, so using a supermarket chopping board (yellow I think is uncooked poultry...), came up with this. The back is just some flat strips. The front was one piece where the holes were roughed with a hole saw and then cleaned up with a boring head. The base is some galv steel sheet. The back is screwed to the plastic strip, the front strip is sandwiched between an upturn and a strip, with a slight lead in on both edges to help guide the holder in (and keep it there when in position).
    P1040787.JPG
    The only issue (and why I think vertical is a better storage option) is that when the holders have a long overhang (long and/or heavy cutting tools), they can tip or not want to sit flat. Solvable with a loop at the back (or a peg in the threaded part), but extra mucking around.

    Michael

    (Bonus information - the paint pen rings (red or blue) on the second picture indicate metric or imperial draw bar threads. The draw bars are similarly marked so that if I'm going to screw things up, I do it properly)

  2. #2
    Join Date
    Mar 2011
    Location
    Southern Flinders Ranges
    Posts
    1,552

    Default

    Thanks for sharing. I’m on the quest for the same grail, but haven’t gotten as far as mill tooling yet.

    I like it, I see a variation to suit my MT3 tooling coming up., although probably colour coded to uncooked meat more than chicken

  3. #3
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Thanks for sharing Michael. I never get tired at looking at other people's tooling storage solutions. Mine is not as elaborate, just some holes bored into a timber book case that i acquired years ago.

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  4. #4
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default very nice

    that looks great Michael. a lot better than what i have done.
    Looks like a pretty good selection to mate.
    aaron

  5. #5
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Good stuff Michael,

    A place for everything and everything in its place. Its a good rule for our work spaces.

    I did a similar exercise when I obtained extra QCTP blocks from a Forum member and its has worked well.

    Your well thought out system minimizes the chance of misplacing tooling and damage.

    Unfortunately I have not taken my tool organization much past the lathe and drill press and the shed needs a total reorganization.

    So I am treating your post as a timely reminder.

    Thanks for posting

    Grahame

Similar Threads

  1. My Tool Storage Solution
    By Keith_W in forum METALWORK GENERAL
    Replies: 13
    Last Post: 5th Mar 2016, 01:21 PM
  2. Tool Storage Updates
    By Oldneweng in forum METALWORK GENERAL
    Replies: 22
    Last Post: 7th Dec 2015, 06:06 PM
  3. Tool bit storage tubes
    By marty989 in forum METALWORK GENERAL
    Replies: 34
    Last Post: 30th Nov 2012, 05:05 PM
  4. Tool storage tip of the day...
    By Greg Q in forum METALWORK GENERAL
    Replies: 3
    Last Post: 18th Jan 2012, 10:02 AM
  5. My Tool Storage cabinet
    By aametalmaster in forum METALWORK GENERAL
    Replies: 15
    Last Post: 5th Jun 2011, 02:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •