I had my 3 jaw scroll chuck apart to day to clean it out which brought to mind something that I've read about a lot.
That is that "a scroll chuck should be tightened using all of the available chuck key holes" (pinions).
So tonight I did a bit of searching and there are several threads on various forums, going back several years.
Lots of different opinions expressed as to how to "correctly" tighten a scroll chuck.
Lots of people in favour of using all the pinions (because that's how they were taught) plus plenty of others saying use the same pinion every time or it doesn't matter.
Others believe that the chuck is marked to show the best pinion to use. ( which is useless if the chuck has ever been apart and re assembled with the pinions in different holes)
Reading some of the posts I cant help but wonder if some of the people who made them actually know how a scroll chuck works.
To me it shouldn't matter which pinion is used (but I'm always open to an opinion change) as the pinion only turns the scroll and its the scroll that actually tightens the jaws.
Anyway I thought Id put it out here for discussion.
peter
-
1st Jan 2020, 10:58 PM #2
Hi Peter, Guys,
I personally don't bother going round the pinions or using just a specific one to tighten the jaws on the lathe three jaw chuck. I understand the arguments that the scroll isn't a precision fit in the chuck body and can move slightly when force is applied from different pinions. But if you have to tighten a chuck to that extent to get a firm grip on your work then the jaws are probably bell mouthed and quite worn.
On the other hand, I do occasionally go round the holes on the drill chuck, particularly if the drill is large and is likely to slip under pressure. Large reduced shank blacksmiths drills spring to mind here along with hole saws.
Happy New Year All.Best Regards:
Baron J.
-
1st Jan 2020, 11:03 PM #3Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Some good food for thought, will be intersting to see what comments come back from the machinists and amatuers. Thanks for bringing this up.
KrynTo grow old is mandatory, growing up is optional.
-
2nd Jan 2020, 12:21 AM #4Senior Member
- Join Date
- Aug 2011
- Location
- Perth, Western Australia
- Age
- 67
- Posts
- 362
I have always run a four jaw (non scroll) on my lathe but every now and then I stick a 100mm scroll four jaw in the big one for little jobs. As I was taught for a scroll chuck I tighten all the pinions.
Drill chucks now are manly keyless but if using a key chuck, as I was taught, I do go round and tighten on all holes.
Tony
-
2nd Jan 2020, 12:42 AM #5Golden Member
- Join Date
- Dec 2011
- Location
- Sydney
- Posts
- 505
I have an Elliott Forte 3 jaw 5 inch steel body chuck with one pinion marked "0", which presumably is (or was when new) the one best pinion to use.
While I never actually measured the concentricity of grip with different pinions, the Elliott has always seemed a good accurate chuck regardless which pinion is used,
and from memory more consistent than my Pratt Burnerd iron body chucks were they were new.
Bill
-
2nd Jan 2020, 07:08 AM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
On a scroll chuck in reasonable condition, I can't see it would matter which pinion is used to tighten it.
I usually only use one (randomly selected) to tighten. However, I occasionally check all three and get a little bit out of 'the others'. I can only surmise that friction within the chuck allows the scroll to hang slightly on the pinion.
Michael
-
2nd Jan 2020, 07:30 AM #7Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
I normally only use one pinion, but if i need something super tight in the chuck i will use all the pinions. On cheaper chucks you can tighten the pinion before the high point to tweak the run out.
-
2nd Jan 2020, 09:19 PM #8Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
Interesting answers .
I'm not disputing any of them but I still don't get how using 1 or all three pinions can change how the chuck tightens. Unless there is a large amount of wear (or poor manufacturing quality control) in the chuck between the scroll plate and the chuck body. Maybe using different pinions might effect it then but I still cant see how. You could even assemble the chuck with out the pinions installed and still tighten it by sticking a screwdriver or similar into the hole and levering on the gear teeth.
Am I missing something? I'm just a dumb fitter at the end of the day.
peter
-
3rd Jan 2020, 02:21 AM #9Senior Member
- Join Date
- Aug 2011
- Location
- Perth, Western Australia
- Age
- 67
- Posts
- 362
I suppose some of the things we are taught just stay with us.
On the other hand I was taught to come over the spinning chuck if filing a job in the lathe. I cannot do it, I have visions of getting my arm caught.
Tony
-
3rd Jan 2020, 03:12 AM #10
Hi Peter, Guys,
If you can visualise the scroll wheel not being a perfect fit inside the chuck body or a perfect fit on the inside bore, there will always be some slight play, maybe only a few thou, but its there. The pinions will push the scroll wheel to take up this play. The next pinion will push the scroll to take up any further play, and so on.
Now imagine the scroll unwound and layed out. It would look like a straight sloping line. Any play in the scroll wheel will cause the line of the scroll to vary its position, either up or down. Further imagine the three jaws in fixed positions along that line. Each jaw will have its own amount of play which will vary depending upon the diameter of the work in the jaws and the scroll position at that diameter.
In short there will always be one pinion that will be tighter than any other, conversely there will always be one pinion that is more loose. The same applies to the jaws, each jaw will have a different force applied to it, simply due to machining tolerances. This is the basic reason that a three jaw scroll chuck will never hold a work piece with zero run out and the same reason that it is very hard to get the chuck to repeat at any setting once you remove the work piece.
Not an easy thing to explain, but tolerances and wear and tear play a big part. In my opinion people over tighten three jaw lathe chucks needlessly. I've seen a couple of chuck scroll plates that have had distorted scrolls !Best Regards:
Baron J.
-
3rd Jan 2020, 03:02 PM #11Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
BaronJ.
Thanks for that explanation. Its actually the best I've seen yet.
I don't use my 3 jaw all that much and when I do its not for jobs that need repeat-ability. I'm not on the clock at home so if it take an extra few minutes to set up in the 4 jaw then so what.
thanks
Peter
-
3rd Jan 2020, 03:06 PM #12Most Valued Member
- Join Date
- Aug 2008
- Location
- Charlestown NSW
- Age
- 65
- Posts
- 1,673
-
3rd Jan 2020, 04:43 PM #13Senior Member
- Join Date
- Jun 2007
- Location
- Victoria, Australia
- Posts
- 114
When it matters I use the indicator with the 3 jaw and achieve adjustments from 0.07 to 0.02mm by adjusting tension on the scrolls. Sometime when the moons are aligned I am able to get 0.00m But if it really matters and work piece has to removed and swapped around or worked elsewhere if the workshop, the 4 jaw is mandatory.
Similar Threads
-
Old Scroll Saw
By bwal74 in forum METALWORK - Machinery, Equipment, MARKETReplies: 10Last Post: 24th Apr 2019, 06:46 AM -
A Centring Post for the Turnado Ball Turner
By Anorak Bob in forum METALWORK GENERALReplies: 14Last Post: 6th Nov 2018, 09:59 PM -
Centring Attachment
By Anorak Bob in forum METALWORK GENERALReplies: 8Last Post: 20th May 2016, 01:38 PM -
Wanted - tightening collet on headstock
By oggy in forum THE HERCUS AREAReplies: 7Last Post: 29th Apr 2016, 06:33 PM -
Centring Microscopes
By Anorak Bob in forum METALWORK GENERALReplies: 33Last Post: 24th Oct 2013, 12:55 PM