Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 6 of 6

Thread: shrinking disc

  1. #1
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,725

    Default shrinking disc

    A tool panelbeaters use, a disc mounted on a angle grinder. Would it be possible to make a disc out of stainless, rather than buying one ? They are not cheap to buy . The friction heats up the area to be shrunk , usually a spray of water is used .

  2. #2
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,671

    Default

    I can't see why not.
    They are ~1.6mm stainless according to this:

    https://www.autobodytoolmart.com/shr...s-p-15602.aspx

    Steve

  3. #3
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,671

    Default

    The commercial ones look like they are pressed out of sheet, but I reckon it would be hard to get that outer flange formed nicely and keep the face flat fabricating one yourself. I don't think the thickness is critical, more that they form them out of 1.6mm for manufacturing reasons.

    I think it might be easier to turn one up out of plate. Probably 6 or 8mm would be thick enough to get a similar radius on the edge as what the commercial ones have, recess the center for the flange nut and just leave the rest original thickness.

    Steve

  4. #4
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

  5. #5
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,475

    Default

    Shudder ! No guard He's lucky he still has fingers.
    Best Regards:
    Baron J.

  6. #6
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Common sense should have told him that the 4" grinder was too small for the disc.

    The other way would have been to extend the A/G handle.

    Common sense is not always common.

    Grahame

Similar Threads

  1. Disc Sander RPM
    By Dusty Wheels in forum METALWORK GENERAL
    Replies: 10
    Last Post: 1st Aug 2019, 04:40 AM
  2. Disc sander build
    By Pete O in forum METALWORK PROJECTS
    Replies: 10
    Last Post: 11th Jan 2019, 03:31 PM
  3. witch cutting disc do you use?
    By wodstok in forum WELDING
    Replies: 12
    Last Post: 10th Feb 2011, 08:39 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments