9th Dec 2019, 01:35 PM #31Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
There is no way you will get that welded and re machined for $65. Also my experiences with welding annoy castings has been unpleasant to say the least.
-
9th Dec 2019, 01:59 PM #32Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
OK next problem.
I tried removing the facing cutter that's in it.
It seems to be stuck pretty hard. Isn't it just a matter of loosening the drawbar nut and giving it a whack with a hammer ?
That didn't work. The guy that sold it to me said he only used it for one task which was milling a face on something so this cutter prob hasn't been removed for years.
I don't know what the drawbar should look like but it's only threaded rod in there now.
P1040085.jpgP1040086.jpg
-
9th Dec 2019, 03:12 PM #33
Looks like a round column mill drill, so it will be either MT3 or R8, if so you need to give it one good hit with the quill locked and I'd use a piece of aluminum between
to save the threads on the draw bar.
As you said it's probably stuck over the years.Using Tapatalk
-
9th Dec 2019, 03:21 PM #34Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
If it's stuck it's because its a Morse taper. You are probably going to need a significant shock to get it out.
-
9th Dec 2019, 03:23 PM #35Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
I would probably take the drawbar all the way out, then make a close fitting drift and wail on that. The drawbar is probably bending and dissipating all the energy from your hammer blow.
-
9th Dec 2019, 04:19 PM #36
Chuck has a ring
Photo
Using Tapatalk
-
9th Dec 2019, 04:40 PM #37Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
-
9th Dec 2019, 05:18 PM #38
-
9th Dec 2019, 05:20 PM #39
I also made boxes for the rotary table, chucks and faceplates. Everything has lifting points so easy accessed by the crane hook.
Using Tapatalk
-
9th Dec 2019, 05:33 PM #40Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
Had to duck into town.
When I came back I used a bigger hammer and out it popped.
Another thing I found...The motor was mounted around 20mm too low so the belt wasn't lined up very good. I don't know why the guy left it like it.
So I lifted it up to where it should be. While fiddling with that is when I discovered the broken pulley. So part of that was of course the belt adjustment.
I reckon it will take me 20 mins every time I want to change speeds on this thing. It's a pain in the royal butt.
-
9th Dec 2019, 06:25 PM #41
I have a vfd for my mill and motors to fit when I get around to it.
I just stay around the 4 speeds that doesn't need belt swapping.Using Tapatalk
-
9th Dec 2019, 06:45 PM #42Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
-
9th Dec 2019, 10:19 PM #43Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Any chance of a pic of your motor adjustment please. It may be possible to fit one of several items to make speed changing quicker.
If the motor is mounted on a hinge type arrangement, a push type toggle lever could be fitted. If it's mounted on twin sliding bars, some sort of cam arrangement might be suitable.
KrynTo grow old is mandatory, growing up is optional.
-
10th Dec 2019, 04:41 AM #44
-
10th Dec 2019, 09:08 AM #45Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
Yep, here it is.
I was thinking of a couple of ideas myself, that I could do to it once I get it cleaned up and mounted on the stand. A couple of the free items it came with are lots of thick dirt and a kilo of sharp swarf.
It will need a big clean and lube. X and Y are hard to move and winding the head is near impossible. Once I get the machine freed up I'll seriously consider mounting some sort of motor drive for the head, just need to find a cheap DC motor with a worm drive larger than a windscreen wiper.
P1040088.jpgP1040089.jpgP1040092.jpg
Similar Threads
-
Ring roller
By KBs PensNmore in forum WANTED TO BUYReplies: 4Last Post: 21st Jun 2018, 12:23 AM -
Another ring roller
By Michael G in forum METALWORK GENERALReplies: 3Last Post: 15th Apr 2017, 01:12 PM -
H&F Ring Roller
By Dingo Dog in forum METALWORK GENERALReplies: 7Last Post: 13th Apr 2017, 09:26 PM -
O-Ring Supplier
By Normanj in forum METALWORK GENERALReplies: 14Last Post: 30th Nov 2010, 09:36 AM -
Ring making
By Eindringling in forum METALWORK GENERALReplies: 4Last Post: 6th May 2007, 03:03 AM