    Default How to fix broken retractable air hose reel

    Factory neighbour asked me to try to fix their retractable reel - you know the ones that I can never work out how to lock after you have pulled some hose out?


    After taking the fixed swivel hose centre off and removing the cover, it became obvious the clock spring end had broken – where the 90° bend is:

    IMG_0687.jpgIMG_0688.jpg

    Spring is 25mm x 1.6mm section. I was about to measure the length and look on eBay for a new spring, until I looked at the other end, where they have a pin through two holes to form a loop.

    Aha! I can bodge up a clamped solution. First, clamp the spring in place, then grind a hole:
    IMG_0689.jpg
    using a Dremel™-like tool (spring seemed too hard to drill), then find a saddle clamp:
    IMG_0690.jpg
    and bend it, so a bolt can hold the spring in that slot:
    IMG_0691.jpg


    Reassemble, and it works well enough.

    The saddle clamp is flimsy (mild steel, probably thinner than the spring steel), but it is only locating the spring in a slot. Should give the owner another decade?

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Nice fix. That's the trouble with springs like that, the ends break off and makes them useless, till NOW, THANKS.
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Nice job.

    Great to build up credit with your neighbours. Never know when you may need a favour!!

    Simon

    Sent from my SM-G970F using Tapatalk
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

Similar Threads

  1. Overhead retractable power cable
    By node105 in forum METALWORK PROJECTS
    Replies: 13
    Last Post: 10th May 2020, 08:34 PM
  2. A Simple Retractable Threading Tool
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 24
    Last Post: 3rd May 2018, 11:15 AM
  3. How to modify fishing reel
    By Arron in forum METALWORK GENERAL
    Replies: 23
    Last Post: 21st Aug 2015, 09:51 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •