Needs Pictures: 0
Results 16 to 25 of 25
-
9th Nov 2019, 08:18 AM #16Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
No worries - it can be a confusing topic.
-
12th Nov 2019, 08:30 AM #17Intermediate Member
- Join Date
- Jul 2019
- Location
- Caboolture
- Age
- 47
- Posts
- 28
i am going through this same issue i think.
Have a QCTP AXA 250-111
My mars lathe has a bolt to hold old tool post down.
This bolt is to large for the QCTP.
I only had 5 minutes to look at it yesterday so not sure on sizes or anything.
But would i be better off changing bolt or boring QCTP ?
Thanks
Daniel
-
12th Nov 2019, 08:39 AM #18Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
Change the bolt/stud.
-
17th Nov 2019, 04:58 PM #19Intermediate Member
- Join Date
- Sep 2016
- Location
- Adelaide
- Posts
- 27
question about the indexing plunger
hi, so I bought now an AXA 100 QCTP from M&G in Melbourne - so yes, I have to make a new stud with Imperial thread, which I cannot do myself on my Metric Hercus, so its either buying a gearset to do so, or find a lathe where I can machine one for me. Either choice is not gonna be easy, but anyhow, i gotta solve that.
More importantly, the indexing plunger cannot be used on my QCTP, it hasnt got any holes for it, neother is there any space to drill them in, but would be just pushed down by the QCTP, why did you take it out and how do you get the QCTP now square to the chuck? You align the tool somehow?
Thank you very much
-
18th Nov 2019, 07:52 AM #20Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
If I need to get the toolpost square to the chuck, like when I am parting off, I leave it loose and move the carriage to the left so that a face of the TP block is up against a flat surface of the chuck. Then tighten it.
-
18th Nov 2019, 12:31 PM #21Intermediate Member
- Join Date
- Sep 2016
- Location
- Adelaide
- Posts
- 27
QCTP for Hercus 260
Okay - thanks a lot for the tip. Sounds reasonable. I probably have to develop a process for this when I actually get to using all this.
But could you also please enlighten me why you took that index plunger out? It might pop up when you turn the QCTP, but then you could press it lightly down and turn the QCTP all the way? I see I guess when I get there.
And also - All I need is the correct imperial thread die and turn the stud to the correct diameter - and done. no threading required
cheers
Werner
-
18th Nov 2019, 01:18 PM #22Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
I didn't need to remove the index spring plunger. It will work OK with it still in place - just as a system I find it a bit annoying.
To cut your threads, using a die might work, as long as you guide it with a tailstock mounted holder to ensure accuracy.
Or maybe someone here could make a stud or stud+sleeve for you.
For example, Pipeclay does bits for Hercus lathes.
-
18th Nov 2019, 01:26 PM #23Intermediate Member
- Join Date
- Sep 2016
- Location
- Adelaide
- Posts
- 27
QCTP for Hercus 260
I try to get it done - but thanks for the offer and idea - I'll keep that in mind
I m bit confused tho - did you not state in reply #4, and I quote: " ... The Spring loaded indexing plunger was removed by tapping out from underneath...."
That made me think you have no indexing plunger anymore, sorry. I misunderstood.
-
18th Nov 2019, 05:42 PM #24Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
Sorry, I should have said, "I didn't need to remove the plunger, but I did anyway because it was annoying."
-
19th Nov 2019, 12:03 PM #25Intermediate Member
- Join Date
- Sep 2016
- Location
- Adelaide
- Posts
- 27
Similar Threads
-
Hercus 260 Quick Change Tool Post size
By localele in forum THE HERCUS AREAReplies: 8Last Post: 31st Oct 2015, 05:43 PM -
Advice on a quick change tool post for a Hercus 9" ( a gift so I cannot check the fit
By Ben Dono in forum METALWORK GENERALReplies: 3Last Post: 15th Dec 2014, 07:45 PM -
Quick change tool post
By TKO in forum METALWORK GENERALReplies: 5Last Post: 20th Oct 2013, 10:15 PM -
Quick Change Tool Post
By tinkera in forum METALWORK GENERALReplies: 3Last Post: 22nd Sep 2010, 11:17 AM -
Adapting quick change tool post holder to suit Hercus 9" lathe
By neksmerj in forum METALWORK GENERALReplies: 10Last Post: 10th Jun 2007, 10:37 AM