Needs Pictures: 0
Picture(s) thanks: 0
Results 16 to 30 of 34
Thread: Transporting oxy-acetylene
-
13th Oct 2019, 03:30 PM #16China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Not a problem for me I have a lPG tank firmly bolted down will stop pretty much any coming forward ( HA! HA!)
-
13th Oct 2019, 03:55 PM #17Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Pressure vessels such as LPG, acetylene etc. are very robust even in a fire. They can take quite alot of heat before failing. Certainly wrt to LPG, the closer to being full, the longer they will last in a fire before exploding. Reason being is that the liquid LPG acts as a coolant and will absorb much of the heat from the impinging flames in a fire. The equilibrium ratio of vapour to liquid is changed as the liquid absorbs the heat and changes phase to a vapour. The increased pressure from this is expelled via the pressure relief valve. Eventually the liquid is boiled off to the point where the walls of the bottle that are exposed to direct heat no longer have the liquid from the fuel to absorb the heat. One of two things will happen, the bottle will safely vent until it's empty, or the walls will be heated sufficiently enough to weaken and no longer have the strength to hold the pressure. Then you have what's called a BLEVE. Boiling liquid expanding vapour explosion.
Most pressure vessels that fail explosively as a result of fire do so with a BLEVE. Rarely does the valve fail from the heat. They are obviously suseptable to mechanical damage but not thermal. It's usually the strongest part.
On our trucks we carry compressed air to 200 Bar (soon to be 300 Bar or 4400 psi) in both the cabin (behind our seats) and in our lockers. They are not even made of steel but carbon fibre. We also carry two C size cylinders of medical oxygen. Ambulances (at least in Vic) carry larger cylinders of oxygen in a locker just behind the driver. I can't imagine they would explode, even in an accident. They are very robust although the valve group may get damaged in such a situation but they are well secured.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
13th Oct 2019, 05:00 PM #18China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
simonl, about two years ago my friends factory in Jamestown burnt to ground absolutely nothing left, except that is for a oxy/acetylene set standing up in the ashes minus the hoses the gauges were also destroyed
my mate commented to the fire captain and he said is was quite common for gas cylinders of different types to come through a fire without exploding however they always treat the situation as a potential explosion
-
13th Oct 2019, 06:52 PM #19Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
In 2009 i was standing on my back verandah watching and waiting for a 1 klm or so wide fire front to hit me, there was no noise like sirens helicopters ect they were all hiding, you could only hear the roar from the bushfire.
Then i won tattslotto... the wind changed, lucky for me but not for the poor buggers that lived in chum creek.
As the fire took off up that valley the relative silence was punctuated by exploding LP gas cylinders, i dont know how many went off
as i had other things on my mind at the time than counting gas cylinder blasts, but it was many, a lot, and it did not seem to take that long for them to go boom.
-
13th Oct 2019, 06:59 PM #20Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Yep. They should always be treated with caution during and after fire.
It's always a little unnerving when you enter a structure fire that is well going and you see pressure vessels. As a general rule, if you put a hose stream on them and they don't steam up then your ok. We also carry thermal imaging cameras now and so we can see at a glance how full they are and what temp.
I've had a car on lpg explode on me when I was standing maybe 10m away and about to move in for extinguishment. It tore the roof and boot lid off and it sent it 60m behind me. It blew windows out in houses down the street. Not very often that happens. I think the safety relief valve failed in that system.
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
13th Oct 2019, 07:14 PM #21
Hi Guys,
What about camper vans that have the LPG tank under the vehicle completely exposed to the road dirt and wet ?
There are no inspections or particular conditions for installation other than the outlet should be placed at the top ! To prevent liquid entering the regulator. These under floor tanks range from 20 Lt up to 55 Lt. They do have a mechanism to prevent you filling them above 80% full though.Best Regards:
Baron J.
-
13th Oct 2019, 07:18 PM #22Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Shed, you got kissed on the d...ck that day!
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
13th Oct 2019, 07:40 PM #23Most Valued Member
- Join Date
- Apr 2012
- Location
- Healesville
- Posts
- 2,129
-
13th Oct 2019, 08:26 PM #24Banned
- Join Date
- Aug 2015
- Location
- QLD
- Posts
- 735
Seems many ways to move a gas bottle..
My 10c... If yer want to keep them upright in car - First, all windows down. Move passenger seat forward. Place bottles behind passenger seat and strap them in an relatively upright position to seat back. Drive.....
.
-
13th Oct 2019, 08:36 PM #25Senior Member
- Join Date
- Aug 2011
- Location
- Perth, Western Australia
- Age
- 67
- Posts
- 362
Some 40 odd years ago there was about 20 of us working when someone dropped a G size oxy bottle. The head hit a steel beam taking the valve off. The bottle flew across about 300 mm off the floor for 40 m then went off the side 10 stories up.. Landing some 300 m away in the slag pit. How no one got hurt that day I will never know.
To this day I never leave a bottle in an unsecure situation.
I cannot remember when it started, CIG or BOC gas but the guys at the depot stopped loading the bottles for you. They just leave it on the dock for you to load. That way you cannot come back at them if you ignored all the signs they have around the place, did not read the fine print you signed and not load it properly. If anything went wrong its your problem.
Tony
-
13th Oct 2019, 08:42 PM #26
Acetylene cylinders have a fusible plug in them which melts around 100 degrees. I think it's a lead/gallium alloy, and usually in the neck ring of the cylinder.
Once this blows, it basically becomes a air/acetylene torch, and empties itself.
-
13th Oct 2019, 09:04 PM #27Member
- Join Date
- Nov 2015
- Location
- Brisbane Australia
- Posts
- 85
I knew someone who worked at the Evans Deakins shipyards in Brisbane in the early 70's, he said he saw people laying over the oxy bottle, then get a sledge hammer and hit the regulator off. My mate said they could get them to go from one side of the Brisbane river to the other side.
The other story I know is that acetylene is a lot more explosive than LPG, my old plumbing boss said he had a teacher at college who put some acetylene in a matchbox, then lit it. It blew all the windows out of the classroom.
When I was at college I saw guys put acetylene into balloons and light the outside with a match and listen to the big bang.
Also you can't run acetylene gas through copper pipe, if you do the gas becomes poisonous, I only know that because were were taught that stuff at college and you tend to remember it.
Simon
-
13th Oct 2019, 09:54 PM #28
My mate who served his time at Dehaviland as an aircraft sheetmetalworker said they’d make a neutral flame, rap the torch on the bench to make it go out.
Fill a balloon and blow the telephone booths to bits.
Dont remember how they lit them.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
13th Oct 2019, 11:13 PM #29Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,915
On the subject of pressure vessels and fire. There was a fire brigade in the north of Tasmania named Bell Bay Brigade, just your average Volunteer Brigade with the exception of one small factor. I was one of only two fire stations in Tasmania to burn down, (caused by a thief trying to cover their tracks after knocking off the money out of the beer fridge). There were several relics from the fire on display in the newly rebuilt station. One was a .9Kg Dry Chemical extinguisher that had ruptured in the fire and blown a hole through both sides of a concrete block wall, the second item was a 160 BAR Breathing apparatus cylinder that had ruptured in the heat and looked like it had been packed with explosives. I developed an even greater respect for compressed gasses after seeing those two items.
I recall being paged to a structure fire one Friday night. As I drove over the hill toward the fire I can remember seeing explosions and what looked to be oversized sky rocket taking off. The structure was a shed belonging to a refridgeration mechanic and therefore had cylinders of refridgerant, acetylene and oxygen within as well as several fridges of varying size. Even a domestic fridge goes off quite well when the whole thing is heated enough. During the cleanup, a 9Kg cylinder of refridgerant gas was found that appeared to be pregnant. The side had blown out almost 50% and must have been so close to rupturing.
As far as the original question goes, I would exhaust every other option I had before putting Acetylene in your car upright or not. Let's just say that you are involved in a motor vehicle accident, not your fault of course. By carrying a gas cylinder inside your car, the level of risk for any emergency responder and yourself has just gone up dramatically. Usually if something goes pear shaped it goes downhill dramatically in my experience and I'm just not sure it's worth the risk.
Do you get your gas home delivered? Perhaps you could arrange for your gas supplier to move the cylinders for you or cart the cylinders with other workshop items in a trailer?
-
14th Oct 2019, 08:35 PM #30Senior Member
- Join Date
- Nov 2008
- Location
- Sydney
- Posts
- 112
Then i won tattslotto... the wind changed, lucky for me but not for the poor buggers that lived in chum creek.
As the fire took off up that valley the relative silence was punctuated by exploding LP gas cylinders, i dont know how many went off
as i had other things on my mind at the time than counting gas cylinder blasts, but it was many, a lot, and it did not seem to take that long for them to go boom.[/QUOTE]
I don't doubt your experience, but I am left wondeing why the cylinders exploded. All LPG cylinders I have encountered have a safety pressure rupture disk incorporated in the valve, as do other gas cylinders I have come across. Acetylene cylinders have one or more fusible plugs incorporated in the neck and or base to prevent over pressure and explosion. Perhaps they were old cylinders which had not had the required inspections carried out. I can still remember an exhibit at the local Technical College where I learned Oxy Welding which was of an oxy cylinder, without a modern valve with rupture disk, which had been in a shed fire. The cylinder was basically a flat piece of steel with the remnants of the base and neck still attached. It was reported that the explosion demolished the shed and house on the property, and severely damaged the houses on either side. The moral was to make sure your gas welding equipment is up to date. That was the mid 1950's.
Chas.
Similar Threads
-
Transporting granite
By shedhappens in forum METALWORK GENERALReplies: 23Last Post: 13th Sep 2016, 06:38 PM -
Transporting Churchill surface grinder
By bob ward in forum METALWORK GENERALReplies: 9Last Post: 22nd May 2014, 05:30 AM -
Transporting a Tool and Cutter Grinder
By Anorak Bob in forum METALWORK GENERALReplies: 6Last Post: 18th Jun 2011, 09:08 PM -
Transporting Lathes? (Colchester Mascot 1600)
By BrianLara400* in forum METALWORK GENERALReplies: 5Last Post: 8th Oct 2010, 01:00 PM -
New use for Oxy Acetylene set?