Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 10 of 10
Thread: Gibb Strip
-
4th Oct 2019, 09:14 AM #1
Gibb Strip
Does gibb strips come in standard sizes, or are they all proprietary to each manufacturer/machine?
I have a machine that is missing one and I’m wondering if it can be bought off the shelf and cut to length? Machine is obsolete and not worth anything other than preservation of history & company long gone.
It’s been suggested to use a strip of brass. All gibb strips I have experienced have been ground steel with a trapezoid shape.
This one fits a dovetail so would be trapezoid also.…..Live a Quiet Life & Work with your Hands
-
4th Oct 2019, 09:39 AM #2Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
I have made a few, they are surprisingly complicated things to make more to do with holding the workpiece for machining.
I have never heard of them being a "standard" item. Usually made out of cast iron.Gold, the colour of choice for the discerning person.
-
4th Oct 2019, 09:54 AM #3Most Valued Member
- Join Date
- Jun 2012
- Location
- SA
- Posts
- 1,649
I've only ever seen them made from cast steel. They were not cast iron as you can bend them cold a limited amount for a permanent set. Cast iron can flex cold to a limited degree, but needs heat for a permanent set.
Making one would be easy if you had access to a shaper. I recollect seeing strips of gibb material being sold years ago in various cross section dimensions (all trapezoid). You then have to make it fit.
Cheers RobThe worst that can happen is you will fail.
But at least you tried.
-
4th Oct 2019, 10:02 AM #4
I don’t have the equipment to make one other than by hand. I’d love a shaper, I guess a mill would do it if you can setup for the correct angle.
Would mild steel work in a home shop scenario not production level usage?…..Live a Quiet Life & Work with your Hands
-
4th Oct 2019, 10:29 AM #5Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Is it a parallel or tapered gib?
-
4th Oct 2019, 11:42 AM #6Member
- Join Date
- Nov 2009
- Location
- australia
- Posts
- 57
Make one from brass, as it's far easier to file than steel.
If your not going to use it as a production lathe, then a brass gibb will outlast your lifetime.
-
4th Oct 2019, 04:43 PM #7
-
4th Oct 2019, 05:41 PM #8
Brass willll be fine, seen many machines with brass flat gibs.
Usually they are spot drilled to let the gib bolts hold it to save it sliding out.Using Tapatalk
-
4th Oct 2019, 06:59 PM #9Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
I have a jig for parallel gibs upto 13" long 1/4" thick and down to 5/16" wide , 60 degree dovetail.
-
4th Oct 2019, 07:16 PM #10
Sorry I'm thinking of flat rectangular gibs I've seen, not tapered ones.
Using Tapatalk
Similar Threads
-
Workshop Led Strip Lighting.
By RayG in forum METALWORK GENERALReplies: 44Last Post: 15th Nov 2013, 02:07 PM -
Good trick to strip paint
By nearnexus in forum METALWORK GENERALReplies: 15Last Post: 14th Sep 2013, 12:14 AM -
bending brass D strip
By Boatasaurus in forum METALWORK GENERALReplies: 6Last Post: 9th Nov 2009, 08:01 PM -
Uses for brass strip??
By Yonnee in forum METALWORK GENERALReplies: 10Last Post: 26th Mar 2008, 09:25 PM