    Hello All, After reading one of Eskimo's posts re overcrank engine I was inspired to have a go at constructing one after viewing the plans. Materials are mostly relatively easily obtainable brass, aluminium and mild steel sections. The bit I cant find is a brass block measuring 50 x 50 x 70 mm which forms the main body of engine and a piece of flat bar that is 70 x 50 x 10 which is machined for the ports to feed & exhaust the 2 cylinders.
    Can any body point me in the right direction or provide a link to a supplier. A surf around google didn't find a seller for this size section.
    I'm a bit loathe to start construction until I am sure I can get all the materials. Thought about substituting materials but there are 2 cylinders that are silver soldered to this main body.
    Potty Overcrank.JPG
    I live just south of Newcastle NSW if there may be a supplier in that area or sydney. Thank you

  2. #2
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    I would be happy to pick what you need up from George white in Melbourne and post to you?

  3. #3
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Some of the larger materials sometimes have to be whittled from round bar stock...

    Michael

  4. #4
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by Michael G View Post
    Some of the larger materials sometimes have to be whittled from round bar stock...

    Michael
    Yes we are unlucky here compared to the US.
    Over the years I've looked at the US online prices for different materials and even with the value of our dollars compared to there's it's so cheap and also available to buy for the hobbiest.
    Using Tapatalk

  5. #5
    Join Date
    May 2019
    Location
    Picnic Point, Sydney
    Age
    77
    Posts
    314

    Default

    Edcon carry brass sections

  6. #6
    Join Date
    Feb 2009
    Location
    jilliby nsw
    Age
    71
    Posts
    111

    Default

    Quote Originally Posted by Dave J View Post
    Yes we are unlucky here compared to the US.
    Over the years I've looked at the US online prices for different materials and even with the value of our dollars compared to there's it's so cheap and also available to buy for the hobbiest.
    Yes some good stuff in the US, but unfortunately the high cost of postage is the killer.;

  7. #7
    Join Date
    Feb 2009
    Location
    jilliby nsw
    Age
    71
    Posts
    111

    Default

    Quote Originally Posted by Snapey View Post
    Edcon carry brass sections
    Thanks for the tip Snapey. Checked their web site and might be in luck. Will ring them tomorrow. cheers

  8. #8
    Join Date
    Feb 2009
    Location
    jilliby nsw
    Age
    71
    Posts
    111

    Default

    Quote Originally Posted by caskwarrior View Post
    I would be happy to pick what you need up from George white in Melbourne and post to you?
    thanks for your very kind offer. I may have found a Sydney supplier that I will contact tomorrow
    .

  9. #9
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by hpa1 View Post
    Yes some good stuff in the US, but unfortunately the high cost of postage is the killer.;
    That's exactly what I was getting at, the price of postage kills it.
    Why can't we have Australian suppliers like that with a range of sizes with prices.
    Using Tapatalk

  10. #10
    Join Date
    Mar 2014
    Location
    South of Adelaide
    Posts
    1,227

    Default

    Quote Originally Posted by Dave J View Post
    That's exactly what I was getting at, the price of postage kills it.
    Why can't we have Australian suppliers like that with a range of sizes with prices.
    The market is too small in Australia.

  11. #11
    Join Date
    Nov 2009
    Location
    australia
    Posts
    57

    Default

    Better open your eyes next time you do a google search, or maybe go to Specsavers --------

    George White | Australia's leading stockist & distributor of non-ferrous metals - Contact Details

  12. #12
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Quote Originally Posted by mardtrp View Post
    Better open your eyes next time you do a google search, or maybe go to Specsavers --------

    George White | Australia's leading stockist & distributor of non-ferrous metals - Contact Details
    Had a bit of a look through there online catalogue, is there 50x50x70 long that he needs available through them?
    Sadly they don't list prices, that usually means way overpriced.
    I bought glasses today on my own accord, so who knows the world might now open up to me.
    Using Tapatalk

  13. #13
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    George whites prices are okay, and they have a good selection of rounds, square stock I'm not so sure.

  14. #14
    Join Date
    Feb 2009
    Location
    jilliby nsw
    Age
    71
    Posts
    111

    Default

    Rang Edcon steel in Sydney today. They have the brass in stock and will cut me a 70mm length. As expected a bit pricey but at around $40 for 50mm square material, I reckon its both reasonable and affordable. Ill pick up a block next week.
    Thanks guys for all your ideas, assistance tips and suggestions, this forum is outstanding. Booked in to specsavers next week mardtrp, thanks for the reminder Cheers

  15. #15
    Join Date
    May 2019
    Location
    Picnic Point, Sydney
    Age
    77
    Posts
    314

    Default

    Edcon aren't cheap but it's the convenience of being able to buy just about any material & have it cut to your required sizes.

Page 1 of 2 12 LastLast

Similar Threads

  1. what rods for thin brass to brass ??
    By Mathuranatha in forum WELDING
    Replies: 7
    Last Post: 23rd Nov 2020, 08:17 PM
  2. Jo Blocks
    By YBAF in forum METALWORK GENERAL
    Replies: 6
    Last Post: 12th Feb 2016, 01:07 PM
  3. How can I touch up V blocks?
    By Michael G in forum METALWORK GENERAL
    Replies: 23
    Last Post: 8th Oct 2014, 10:04 PM
  4. VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
    By thumbsucker in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 7
    Last Post: 18th Mar 2013, 03:36 PM
  5. Gauge blocks
    By morrisman in forum METALWORK GENERAL
    Replies: 9
    Last Post: 23rd Dec 2012, 11:44 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •