Hi Alan,
This square is 250mm long so it's maximum allowable deviation from squareness is 5um.
I'm not sure why it makes mention of 160mm at the top of the page.
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
30th Oct 2019, 06:32 PM #32Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
I may have access to one of these master squares that has a current calibration certificate tomorrow.
https://www.ebay.com/itm/Coorstek-Ce...-/332637672065
Hopefully i will have time to check my ebay square, it will be interesting to see exactly how square it is.
-
30th Oct 2019, 06:39 PM #33Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
-
30th Oct 2019, 07:13 PM #34Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Wow. That's no carpenter's square!
I will be very interested in how your square stacks up compared to its "certificate"
Geeezzz you get to play with some fun stuff!
Simon
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
1st Nov 2019, 06:54 PM #35Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
So i didn't get a chance to test my square against the master, but i did a rough check on the mill that just got re aligned and got about .01mm of error. i will try and do a better check next week.
Similar Threads
-
Ignyte Precision Granite Surface Plate 24" x 18" x 4"
By kwijibo99 in forum METALWORK - Machinery, Equipment, MARKETReplies: 10Last Post: 5th Jul 2016, 10:41 PM -
An "unearthed" CVA precision capstan lathe
By jhovel in forum METALWORK GENERALReplies: 14Last Post: 2nd Jul 2011, 12:16 PM -
hercus 9" precision lathe
By Metal Tinkera in forum THE HERCUS AREAReplies: 9Last Post: 19th Apr 2011, 07:55 PM -
Opposing toothed "Clutch-Plate" Nuts? (a bit like "Castle" Nuts...)
By Batpig in forum METALWORK GENERALReplies: 6Last Post: 5th May 2009, 08:18 PM -
Difference "Galvanised" and "Primed" Steel
By Fr_303 in forum METALWORK GENERALReplies: 4Last Post: 22nd Jan 2008, 05:59 PM