Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 8 of 8
Thread: Grinding wheel dressers
-
7th Aug 2019, 08:17 PM #1
Grinding wheel dressers
Apologies if I've posted this in the wrong spot, but I'm after some feedback etc on grinding wheel dressers, similar to the one in the link
https://www.banggood.com/Sintered-Di...r_warehouse=CNHafco AL320G Lathe
Toolex RF31 Mill/Drill
Saber Bandsaw
-
7th Aug 2019, 08:50 PM #2Member
- Join Date
- Nov 2009
- Location
- australia
- Posts
- 57
There quite OK for a few dressings, but the moment you wear thru that coating, then your going to need another real soon.
This type of dresser is a bit better and will last a lot longer, which will work out to be the cheapest in the long run.
Not saying to buy that one in the link, just go for that type of dresser.
https://kutritemfg.com/dressers.php
-
8th Aug 2019, 12:43 AM #3Senior Member
- Join Date
- Aug 2007
- Location
- Saskatoon, Saskatchewan, Canada
- Posts
- 292
I asked some guys using a concrete/road saw if they had any old blades. They gave me a few and I used a cutting disc in a grinder to cut wedges from the expansion slots in the edge to the hole. Wrap the heck out the point with duct tape or make a simple handle hammered over the point. One blade will give you a lifetime of dressing tools and a few for your pals.
I also have a small rock drilling bit end, the kind used to drill core samples, given to me. It works great too. Bigger diamonds!
Pete
-
8th Aug 2019, 06:57 AM #4China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
That type of dresser works very well I have had one years, however the one one pictured does not spell high quality to me
-
8th Aug 2019, 09:29 AM #5
-
8th Aug 2019, 11:16 AM #6Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 65
- Posts
- 3,103
Hi oldhack
I would absolutely recommend the one with the star wheels.
Also when they wear out you can buy new star wheels...which reminds me.
Phil
-
9th Aug 2019, 12:11 PM #7Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
anything wrong with diamond dressers?
-
9th Aug 2019, 06:36 PM #8Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
I use the type the op linked to at work. I have had it for about 5 years and on average would dress the 8" wheel we use for drill grinding twice a month. it shows no sign of wearing out any time soon, should be fine for use in a home shop.
Similar Threads
-
Grinding Wheel
By Oldneweng in forum METALWORK GENERALReplies: 18Last Post: 15th Jan 2017, 06:07 PM -
Ebay Diamond wheel dressers
By argeng in forum METALWORK GENERALReplies: 6Last Post: 17th Aug 2012, 11:08 PM -
Anyone qualified to compare wheel dressers?
By billrule in forum METALWORK GENERALReplies: 17Last Post: 20th Jan 2011, 09:34 PM -
Which Grinding Wheel For Grinding Tungsten Electrodes
By Metal Head in forum WELDINGReplies: 14Last Post: 8th Aug 2009, 02:23 PM -
Lap grinding wheel
By ROB NZ in forum METALWORK GENERALReplies: 6Last Post: 20th Jan 2008, 06:42 AM