    Hi all,
    I need to make a tool for shaving out a gear keyway on the lathe.
    The keyway is 5mm in an 18mm bore.
    My plan is to stick weld a piece of HSS into the end of a round steel bar but I'm a little worried about affecting the HSS hardness.
    What should I do after welding it ?

  2. #2
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    Could you braze or silver solder it instead? Neither of those will change the temper. I have never seen hss weeded successfully.

  3. #3
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by caskwarrior View Post
    Could you braze or silver solder it instead? Neither of those will change the temper. I have never seen hss weeded successfully.
    I guess I could try silver solder, if my torch will get it hot enough. I've only got LPG.
    But then I'd have to get the HSS red hot for silver solder, wouldn't that change the temper ?

  4. #4
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,188

    Default

    The temp of the HSS won't be affected by welding - that is if you can weld it but like CW says I have not seen it welded, brazed certainly.
    HSS has to be held at red heat for a long time to substantially affect the hardness and even then it only changes by a few points on the hardness scale.
    Annealing requires hours of heat.

  5. #5
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    Quote Originally Posted by phaser View Post
    I guess I could try silver solder, if my torch will get it hot enough. I've only got LPG.
    I regularly use a primus lpg torch to silver solder carbide but I have to use the high silver content and fire bricks. How big is the cross section?

  6. #6
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,473

    Default

    Hi Guys,

    I agree with Ralph, I've never seen it welded either ! Usually it is silver soldered or brazed with sifbronze.

    As far as cutting a keyway is concerned just use a grub screw to secure the HSS. Its a lot easier.
    Best Regards:
    Baron J.

  7. #7
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Guys,

    I agree with Ralph, I've never seen it welded either ! Usually it is silver soldered or brazed with sifbronze.

    As far as cutting a keyway is concerned just use a grub screw to secure the HSS. Its a lot easier.
    A grub screw was the original idea but how do you make a 5mm square hole through a 14mm round bar and on an angle ?
    I could drill it but it's a hell of a lot of filing to make it square.

  8. #8
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    316L stainless rods are good for welding hss to steel.

    Sometimes I also use them for welding cast iron, steel to cast iron, cast steel.

    cheers, shed

    https://www.boc.com.au/shop/en/au/bo...rodes#product1
    Last edited by shedhappens; 3rd Aug 2019 at 04:48 PM. Reason: added link

  9. #9
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    It doesn't nessecarily need to be a square hole, as long as the grub screw is square to the face, that should be enough to hold it in position.
    Kryn
    To grow old is mandatory, growing up is optional.

  10. #10
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,473

    Default

    Hi Phaser,

    A grub screw was the original idea but how do you make a 5mm square hole through a 14mm round bar and on an angle ?
    You don't !

    Just drill a hole in the end of a suitable piece of bar, fit your HSS bit into the hole and secure with a grub screw.

    Put the gear in the lathe chuck and the cutter in the tool post, use the lathe saddle to move the tool in and out to cut the keyway. You will need to grind the cutting face correctly and you will only take off a few thou per cut.

    26062014-08.jpg
    Here is one I did earlier.
    26062014-01.jpg
    I found that cutting more than one key slot very tiring, so I made a tool to help.

    19062014-04.jpg 19062014-02.jpg
    This is the tool. There is just a grub screw to secure a length of suitable tool steel. In your case for a 5 mm wide key, use a 5 mm wide piece of tool steel.
    Best Regards:
    Baron J.

  11. #11
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    Quote Originally Posted by phaser View Post
    Hi all,
    I need to make a tool for shaving out a gear keyway on the lathe.
    The keyway is 5mm in an 18mm bore.
    My plan is to stick weld a piece of HSS into the end of a round steel bar but I'm a little worried about affecting the HSS hardness.
    What should I do after welding it ?
    Use it.

  12. #12
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    Quote Originally Posted by caskwarrior View Post
    Could you braze or silver solder it instead? Neither of those will change the temper. I have never seen hss weeded successfully.
    Me too, I can't seem to find HSS weeds, but I have welded it and used it after welding with Mig and stick.

  13. #13
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Phaser,



    You don't !

    Just drill a hole in the end of a suitable piece of bar, fit your HSS bit into the hole and secure with a grub screw.

    Put the gear in the lathe chuck and the cutter in the tool post, use the lathe saddle to move the tool in and out to cut the keyway. You will need to grind the cutting face correctly and you will only take off a few thou per cut.

    26062014-08.jpg
    Here is one I did earlier.
    26062014-01.jpg
    I found that cutting more than one key slot very tiring, so I made a tool to help.

    19062014-04.jpg 19062014-02.jpg
    This is the tool. There is just a grub screw to secure a length of suitable tool steel. In your case for a 5 mm wide key, use a 5 mm wide piece of tool steel.
    I have made several internal keyways using this same technique. I concur that it is a laborious task if you have to make several but as a one-off it still works very well. I really need to make one of those lever setups.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  14. #14
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by caskwarrior View Post
    I regularly use a primus lpg torch to silver solder carbide but I have to use the high silver content and fire bricks. How big is the cross section?
    My idea was to weld or solder it in like this.
    A round bar about 12mm slotted with a hacksaw and files to take the 5mm HSS bit.

    keyway cutter.jpg

  15. #15
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,217

    Default

    A stronger way is to mill an angled slot in the holder lengthwise and put the HSS in there and grind to suit. I will get a photo of one I prepared earlier.
    Gold, the colour of choice for the discerning person.

Page 1 of 4 1234 LastLast

Similar Threads

  1. oxy welding help
    By bobsreturn2003 in forum WELDING
    Replies: 4
    Last Post: 9th Jun 2011, 04:46 PM
  2. co2 for mig welding
    By wodstok in forum METALWORK GENERAL
    Replies: 2
    Last Post: 13th Jul 2010, 10:07 PM
  3. Welding gal
    By Groggy in forum WELDING
    Replies: 6
    Last Post: 10th May 2009, 11:00 PM
  4. Where do you do your welding?
    By jmk89 in forum METALWORK GENERAL
    Replies: 16
    Last Post: 13th Mar 2008, 01:42 AM
  5. new to welding.
    By Bluegum in forum WELDING
    Replies: 8
    Last Post: 24th Oct 2006, 09:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •