    The last time I cut a keyway on the lathe, I just used a small piece of HSS blank. I ground it down to the size needed and put it straight in the tool holder. Apart from the cutter clearance angles, which was ground in the tool, the rake was adjusted by rotating the toolpost.

    The fiddliest bit was ensureing the tool was cutting at the correct height to ensure a symmetrical groove but that was done by eye anyway and it turned out fine.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  2. #32
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    Also sometimes it works better if you have two cutters, a narrow one and a finishing tool.

    Might repost the link to this book. https://www.dropbox.com/s/f48ewsbh13...20slotting.pdf
    Gold, the colour of choice for the discerning person.

  3. #33
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,475

    Default

    Hi Guys,

    When I did my keyways, I locked the spindle with the backgear and rotated the work piece until it was positioned where I wanted the keyway to be. Setting centre hight was quite easy.
    Best Regards:
    Baron J.

  4. #34
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    Quote Originally Posted by phaser View Post
    I've managed to cut some of the first keyway but it's very slow
    Yes it is a slow way to do a keyway because a lathe is not designed for this, so patience is needed
    to nibble your way through the job.

    Quote Originally Posted by phaser View Post
    and seems to be making a tapered slot because it pushes away from the job (springs) .
    You need to do more passes at the same DOC to clean up the taper, the lathe also would probably be flexing.

    Quote Originally Posted by phaser View Post
    Can't see why. I thought the grind I put on it would be good.
    You will quickly wear a flat at the cutting edge if you drag the tool back through the cut, effectively
    removing your tool relief, have look with a magnifying glass.

    As Simon said earlier you can rotate the tool around a bit and regain some clearance.

    To stop this happening you need to back the tool away from the work on the return stroke then reset your DOC
    for the next cut.

    cheers, shed

  5. #35
    jatt's Avatar
    jatt is offline Always within 10 paces from nearest stubby holder
    Join Date
    Aug 2008
    Location
    Bendigo
    Age
    51
    Posts
    760

    Default

    Thanx RC

    Don't remember seeing this book when I was in the green.
    Frisky wife, happy life. ​Then I woke up. Oh well it was fun while it lasted.
    From an early age my father taught me to wear welding gloves . "Its not to protect your hands son, its to put out the fire when u set yourself alight".

  6. #36
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default Um hope i can explain this well

    An idea that i have done befor is press a plug into the gear so that it is like the gear has no hole.
    Then center punch the gear where it joins the plug. Drill a hole the same diameter or slightly smaller than the size of the key. Press the plug back out of the gear hole. Now tou have a half round key way nearly the right size in the hole of your gear.
    Finish this to a square key way either by
    Using your lathe as a slotter. With a boring bar or carfully filing the half round slot into a square key way.
    Ive used this method successfully a few times.
    To fashion a boring tool thats suitable use round hss in a piece of bar secured buy a grub screw. As suggested buy others im sure.
    Also i have some home made boring tools that are simply hss arc welded to the end of a piece of bar. I didnt make them but they work fine.
    Aaron.

    Diy or die.

  7. #37
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    I did as suggested by moving the cutter away before withdrawing it each time, and had better success. I kept the cuts at .002 or less.
    The cutter was blunting way too fast originally so I'd say the heat from silver soldering it had ruined the hardness of the HSS. I've done a similar thing many times before by using a 60deg HSS cutter to make finger grips on the outside of knobs I made and never had the cutter blunt at all and I never moved the cutter away before withdrawing it during the process.

    The blanks turned out really good but I did find the key slot narrowed a smidgen as it got to the bottom. That's from wear in the width of the cutter, so I had to finish them with a 3 cornered file.

    P1040040.jpg

  8. #38
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Getting a lot closer to cutting these gears now.

    The shaft is 10mm spigot at the bottom, 12mm at the top, 18mm for the gear blank and 16mm threads (because I can cut 2mm pitch with the gears I've got).


    Shaft between centres and a drive dog.

    P1040042.jpg

    P1040043.jpg

    Actually, I got really lucky here. The last thing I did to the shaft was the top thread. I almost had it finished when I noticed the drive dog was loose.....Could have ended up with a really screwed up thread and ruined the whole thing.

  9. #39
    Join Date
    Oct 2015
    Location
    melbourne
    Posts
    473

    Default

    Quote Originally Posted by phaser View Post

    Actually, I got really lucky here. The last thing I did to the shaft was the top thread. I almost had it finished when I noticed the drive dog was loose.....Could have ended up with a really screwed up thread and ruined the whole thing.
    Been watching doubleboost? He did that exactly last week....

    Russ

  10. #40
    Join Date
    Dec 2013
    Age
    56
    Posts
    1,418

    Default

    Nice save, I hate when things go wrong after so much work.

    I was turning a m6 LH thread 30mm long in stainless steel on the lathe about a month ago, just for a trial peice while waiting for a L/H die from AliExpress.
    I knew it was a pushing it since I was not using a center to support it, then the 2nd last cut it climbed the HSS and wrecked it completely.
    Lesson leason learnt, don't be lazy, lol
    Using Tapatalk

  11. #41
    Join Date
    Aug 2009
    Location
    Sydney, NSW, Australia
    Posts
    1,844

    Default

    I tig welded a 6x6x100mm hss tool i had cut 10mm off one end and welded it onto the tip for boring on the lathe it worked really well but i ground the point the wrong way lol it has been the only tool not needing to be sharpen will see if i can find the pic when i get on the laptop its in one of my threads on here

  12. #42
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by russ57 View Post
    Been watching doubleboost? He did that exactly last week....

    Russ
    What? you mean his dog came loose ?
    Yeah I've seen a few of his videos. Do you have a link for that particular one ?

  13. #43
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    By the way .... This gear cutting jig design is by way of a South Australian guy on youtube and he calls his channel Zynudu .
    Many thanks to him.

  14. #44
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    Do you have a Mill and Rotary Table with either degree or dividing plates to suit the gears to be cut?

  15. #45
    Join Date
    Nov 2012
    Location
    Mid North Coast NSW
    Posts
    423

    Default

    Quote Originally Posted by pipeclay View Post
    Do you have a Mill and Rotary Table with either degree or dividing plates to suit the gears to be cut?
    No, on both scores there. Hence why I need to do it this way.

Page 3 of 4 FirstFirst 1234 LastLast

Similar Threads

  1. oxy welding help
    By bobsreturn2003 in forum WELDING
    Replies: 4
    Last Post: 9th Jun 2011, 04:46 PM
  2. co2 for mig welding
    By wodstok in forum METALWORK GENERAL
    Replies: 2
    Last Post: 13th Jul 2010, 10:07 PM
  3. Welding gal
    By Groggy in forum WELDING
    Replies: 6
    Last Post: 10th May 2009, 11:00 PM
  4. Where do you do your welding?
    By jmk89 in forum METALWORK GENERAL
    Replies: 16
    Last Post: 13th Mar 2008, 01:42 AM
  5. new to welding.
    By Bluegum in forum WELDING
    Replies: 8
    Last Post: 24th Oct 2006, 09:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •