Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 4 of 4
Thread: morse taper #2
-
23rd Jul 2019, 12:04 PM #1Intermediate Member
- Join Date
- Jul 2019
- Location
- Caboolture
- Age
- 47
- Posts
- 28
morse taper #2
Hi All,
Have the opportunity to buy a mill that has a morse taper #2
Would i have troubles with tooling for something like this?
What issues should i be thinking about with morse taper #2
Dont know too much about them
Thanks
Daniel
-
23rd Jul 2019, 12:19 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
I don't know about others but my MT2 stuff seems to slip a lot easier than MT3.
This is much less of a problem if it has a draw bar capability - if not I would not buy it.
-
23rd Jul 2019, 12:56 PM #3Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
I'm happy with the MT2 on my small mill/drill.
Some even used MT1.
There's lots of stuff you can buy with MT2 - collet and drill chucks are easy to find for example.
For milling, it really needs a drawbar, so get them with threaded ends. M10 is common but watch out there's also 3/8 inch so you might end up with two drawbars.
-
23rd Jul 2019, 01:11 PM #4
I don't see any problems with a MT2, and being a mill it will have either metric or imperial drawbar. MT tooling is cheap compared to say NT30
Using Tapatalk
Similar Threads
-
Morse Taper MT2 and 2MT
By presch in forum METALWORK GENERALReplies: 4Last Post: 19th Jun 2019, 11:36 AM -
Jarno or Morse taper
By woodfast in forum METALWORK GENERALReplies: 4Last Post: 29th Jun 2015, 12:14 AM -
Morse Taper 1-3?
By goodwoody in forum METALWORK GENERALReplies: 19Last Post: 25th Nov 2014, 06:52 AM -
morse taper collets
By rfurzer in forum METALWORK GENERALReplies: 1Last Post: 9th Jan 2011, 08:21 PM -
Morse Taper Turning
By jvdv in forum METALWORK GENERALReplies: 46Last Post: 13th Sep 2006, 03:26 PM