Desiccant canisters
My local Bunnings (Mornington VIC) has these on special for $15. It's a decent sized unit. Might be good for sticking in tooling cupboards.
Last edited by jack620; 15th Jul 2019 at 11:36 PM. Reason: spelling
Chris
-
15th Jul 2019, 11:51 PM #2Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
After further research it turns out Damp Free desiccant is not meant to be used near metal. It contains a calcium salt, so it might actually make corrosion worse.