Results 1 to 5 of 5
Thread: Hobbing baby bevel gears
-
8th Jul 2019, 11:13 PM #1Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,080
Hobbing baby bevel gears
Thought I'd share this as I'm guessing most people here wouldn't have been exposed to this sort of specialised work.
One of my recent jobs at work was cutting some small brass bevel gears (I think the pitch was Mod 0.4) on our Mikron 120.01 bevel gear cutter
IMAG3282.jpg
The process is essentially the same as hobbing in that the cutter and workpiece are synchronised in rotation as the work is fed across, but there are a few key differences in the cutter itself. The cutter just has 2 wings that form the teeth as opposed to a proper hob, there are also a range of cutters for each tooth pitch, much like the different numbered gear cutters for mills, which are chosen based on the size of the gear and the number of teeth to be cut. Another major difference is that each wing cuts only one flank of the gear teeth, so the cutter needs to be centralised with the aid of a microscope attachment (which I was firmly told to NOT drop at any cost , this machine is some 50 years old and spare parts don't exist)
IMAG3301.jpgIMAG3302.jpg
All the cutting parameters are set via a gear train, the cutter spindle is tilted over to the helix angle of the cutter and the work spindle is set to the required pitch angle of the gear (in this case, 45 degrees)
IMAG3290.jpgIMAG3288.jpg
There's a deburring attachment to clean up the back of the gear as it's being cut, a hard stop for the starting position and an automatic stop as well, so it's simply a case of loading each blank on the arbor (which is held in a collet and adjusted to a maximum of 0.0005" total runout) and flicking the start lever.
IMAG3284.jpgIMAG3283.jpgIMAG3289.jpgIMAG3287.jpg
Some time later there's a finished gear
IMAG3285.jpgIMAG3286.jpg
-
9th Jul 2019, 11:06 AM #2
Amazing little machine, thanks for sharing
Using Tapatalk
-
9th Jul 2019, 11:24 AM #3.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Wonderful photos of a beautiful little machine and the work it produces!
Than you Elan.
Bob.
-
9th Jul 2019, 07:47 PM #4Diamond Member
- Join Date
- Sep 2006
- Location
- Mallacoota,VIC,Australia
- Age
- 53
- Posts
- 1,010
Great job. Looks like an old machine, but she does beautiful work. Thanks for sharing.
All The Best steran50 Stewart
The shortest way to do many things is to do only one thing at once.
-
15th Jul 2019, 01:27 AM #5Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 575
Very impressive, that's great work and I'm a bit envious - that is the machine I needed a few weeks back, I'm working on a model 4 stroke engine and needed a pair of 45deg bevel gears for the distributor drive, armed with a set of 0.4Mod involute cutters it took me 3 goes before I had just 1 gear, the second one was just a rerun so only took about 10-15 min, both gears are made from 1020 MS, the socket head screw in the pic is one of the 3mm head bolts.
gears 2.jpg
Similar Threads
-
is this thing as simple as 2 x 45 degree bevel gears ?
By steamingbill in forum METALWORK GENERALReplies: 22Last Post: 10th Oct 2018, 09:23 AM -
Baby Shaper NSW
By rustyovali in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 1Last Post: 6th Aug 2018, 12:16 AM -
Qualos No 2 Gear Hobbing machine.
By T70MB in forum METALWORK GENERALReplies: 3Last Post: 14th Nov 2017, 07:50 AM -
Bevel Gears and Helicopters
By Anorak Bob in forum METALWORK GENERALReplies: 15Last Post: 7th Jan 2013, 12:14 AM -
Gear Hobbing on a Lathe
By 19brendan81 in forum METALWORK GENERALReplies: 9Last Post: 31st Aug 2011, 11:55 AM