Thread: 12L14 Steel purchasing online
-
11th Jun 2019, 10:21 AM #1
12L14 Steel purchasing online
Does anyone else living far away from a metal supplier like I do have a source for ordering 12L14 steel online?
Cheers
Jim
-
11th Jun 2019, 11:30 AM #2Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
If you cant find anywhere im happy to mail you some or courier it if you are in a rush.
-
11th Jun 2019, 11:59 AM #3future machinist
- Join Date
- Mar 2008
- Location
- nowra
- Posts
- 1,598
Where on the south coast are you?. I am happy to give you some.
BETTER TO HAVE TOOLS YOU DON'T NEED THAN TO NEED TOOLS YOU DON'T HAVE
Andre
-
11th Jun 2019, 01:45 PM #4Intermediate Member
- Join Date
- May 2019
- Location
- Tucson, Arizona, USA
- Posts
- 46
Hi Jim,
I have ordered from McMaster-Carr. I'm not sure what the postage would be to your neck of the woods.
David
https://www.mcmaster.com/grade-12l14-steel
12L14 McMaster-Carr.jpg
-
11th Jun 2019, 01:48 PM #5
Caskwarrior, that's extremely generous of you. Thank you very much for that kind offer mate.
Welder, that's also extremely generous of you as well!
I'm near Milton about an hours South of you.
I've just rung up some fabricators in Ulladulla and most weren't interested except one who said they'd order some in
for me the next time they do a steel order.
Does it machine as good as I have read about it?
All my steel has come from junk sources and its heritage is unknown, some has been shocking and gummy to machine and some a real pleasure, but I don't know what the good steel is.
Once again, thanks guys for being so generous and so willing to jump in and help.
-
11th Jun 2019, 01:51 PM #6
-
11th Jun 2019, 02:05 PM #7Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
If McMaster would ship to aus, all our industrial suppliers would go out of business, it would be great.
Sent from my Nokia 8 Sirocco using Tapatalk
-
11th Jun 2019, 02:59 PM #8
-
11th Jun 2019, 05:25 PM #9Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
I just hope that the OP doesn't need 6 feet of 4" stock! It will be an eyewatering US$ 890 +shipping +GST on all that.
-
11th Jun 2019, 06:49 PM #10
There is a guy in Queensland selling on eBay, as long as you don't need much as postage is the killer.
Using Tapatalk
-
11th Jun 2019, 07:06 PM #11Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
-
11th Jun 2019, 07:24 PM #12Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Jim,
I get my 12L14 from ABC Specialty Metals in Melbourne. Run by a couple easy going Brits. I have no idea whether they mail or not but I have found their prices to be pretty good.
Greg.
-
11th Jun 2019, 07:25 PM #13Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Even if McMaster shipped to Oz the postage on steel would probably make it more expensive than buying local.
R.C,
Stressproof is lovely stuff to machine. The people who make it shipped me 3 feet of ⅝" round free of charge when I asked them where I could get it in Oz (answer: nowhere).Chris
-
11th Jun 2019, 07:59 PM #14Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
David, the postage is something cruel as it is done via courier...
As an added complication, Mcmaster some years ago decided that they were not going to take on any new customers from outside the US. They have kept supplying to existing customers but will not deliver to anything other than a business address - so hobbyists are high and dry.
Even access to the catalogue is tricky, as every so often, a pop up will ask you to log into your account. Means going through a forwarder in the US is hard as you can't always find what you want or get a part number
MichaelLast edited by Michael G; 11th Jun 2019 at 08:03 PM. Reason: added a bit
-
12th Jun 2019, 07:50 AM #15Diamond Member
- Join Date
- Oct 2011
- Location
- Sydney, NSW
- Posts
- 1,249
HI,
There's a seller on E bay who posts. I can't remember his name but if I found it this afternoon I'll post it.
I have 1.8m of 63mm Diam 12L14 that for some reason I bought last year. Apart from moving it around when I moved I haven't used any of it yet (I got it for a good price!).
Ben
Similar Threads
-
Purchasing a cold cut saw
By warmtone in forum WELDINGReplies: 37Last Post: 3rd Dec 2015, 09:49 PM -
quick MMA welder purchasing questions
By new_guy90 in forum WELDINGReplies: 5Last Post: 20th Apr 2010, 05:26 PM -
Purchasing Tig Wire
By Metal Head in forum WELDINGReplies: 2Last Post: 3rd Nov 2008, 09:41 PM -
Purchasing a MIG welder
By quinno in forum WELDINGReplies: 11Last Post: 23rd Aug 2008, 12:34 AM -
Purchasing a MIG welder
By adam_g in forum WELDINGReplies: 1Last Post: 6th Jun 2007, 09:30 PM