SIlver Solder -Suppliers - High silver content
I'd like to have a go at making a steam boiler for some little engines that I made recently, went shopping for silver solder. After trying the local Reeces, BOC and Bunnings and Totaltools and only getting a maximum 5% silver content I did some googling and found this in Qld.
Seems a bit odd that am not getting many hits, am using Silver solder 56% .com.au as search keywords
Should I be trying different keywords or looking at jewellery suppliers ?
Where do you folk get your high silver content silver solder from.
Bill
-
23rd Feb 2019, 08:51 PM #2Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,513
SBA245 is 45% silver. I use that if I need a low temperature brazing rod. It's not cheap but great stuff.
https://www.colliermiller.com.au/pro...nish-45-silverNev.
-
23rd Feb 2019, 09:07 PM #3Senior Member
- Join Date
- Jul 2007
- Location
- Perth
- Posts
- 332
Deleted duplicate post.
-
23rd Feb 2019, 09:09 PM #4Senior Member
- Join Date
- Jul 2007
- Location
- Perth
- Posts
- 332
Bill,
Try EJ Winter in Bathurst. Alan
-
23rd Feb 2019, 09:10 PM #5Member
- Join Date
- Dec 2014
- Location
- melbourne
- Posts
- 72
In the past I have sourced high content silver solder from Johnson Matthey (Aus) Ltd.
Also called Noble Metals Aus.
Tel: 03 9344 7700
64 Lillee Cres. Tullamarine 3043
-
23rd Feb 2019, 10:20 PM #6Member
- Join Date
- Dec 2014
- Location
- melbourne
- Posts
- 72
I have sourced high content silver solder from Johnson Matthey (Aus) Ltd
Also known as Noble Metals Australia
Tel: 03 9344 7700
64 Lillee Cres. Tullamarine 3043
matthey.com
Robert
-
23rd Feb 2019, 11:40 PM #7Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
I just go to my local welding supply shop, from memory it was about $15 a stick, about 400mm long X 1.6mm.
KrynTo grow old is mandatory, growing up is optional.
-
24th Feb 2019, 06:18 AM #8
-
24th Feb 2019, 07:55 AM #9Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Commercial refrigeration uses a lot of different grade silver solders. Talk to one of the suppliers to the industry, IME most of them do counter sales.
-
24th Feb 2019, 09:23 AM #10Senior Member
- Join Date
- Jan 2012
- Location
- Melbourne
- Posts
- 149
SBA Amalgamated , Bayswater.
https://www.sbagroup.com.au/amal/sba...brazing-table/
-
24th Feb 2019, 09:38 AM #11Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
I am very supprised that BOC didnt have at least 45%..BOC should have even had some higher grades...sounds like counter staff dont know what you wanted.
Reece is a refrigeration supplier, as are Heatcraft, Actrol and Airfrige...all of whom would have 45% silver solder.
However Reece is also a plumbing store and plumbers dont use 45% so depending on amount of refrigeration trade at that particular store, they just may not stock it....the other three would definitely have it as would BOC
-
24th Feb 2019, 10:01 AM #12Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
copper to copper will be easier with SBA115...no flux needed if copper is clean
with steel to copper one should use SBA245..flux needed
-
24th Feb 2019, 01:15 PM #13China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
As said above BOC have it the person you dealt with must have been green
-
24th Feb 2019, 02:54 PM #14Golden Member
- Join Date
- Nov 2010
- Location
- Gippsland Victoria
- Posts
- 733
Thanks ....
Thanks for all of the tips. Will investigate the various suggestions and yes looks like the BOC chap may not have known that they do have high silver content rods on the website.
Am reading the Stan Bray "Making Simple Model Steam Engines" and Tubal Cain "Soldering and Brazing" and building the Jenny Wren boiler from Tubal Cain "Building Simple Model Steam Engines".
Making the end caps was far easier than I expected - heating red hot and annealing the copper was a doddle with my little gas torch so soldering it should be okay too, will see.boiler parts.jpg
Bill
-
25th Feb 2019, 05:56 PM #15Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 574
I recently made a Jenny Wren "look alike" and even though I have some of BOC 45% stuff I didn't have any trouble with the boiler using the 15% stuff from Bunnings.
Similar Threads
-
Silver Solder Purchase
By Briangoldcoast in forum JEWELLERYReplies: 1Last Post: 2nd Oct 2018, 12:11 PM -
WTB ADL Silver solder rod
By GWH74 in forum WANTED TO BUYReplies: 0Last Post: 28th Apr 2016, 08:19 AM -
245 Silver solder
By fxst in forum METALWORK GENERALReplies: 2Last Post: 16th Oct 2012, 12:22 AM -
source of silver solder other than BOC?
By desbromilow in forum METALWORK GENERALReplies: 6Last Post: 30th Aug 2012, 11:30 AM -
Silver Solder Pt 2 How to
By Grahame Collins in forum METALWORK GENERALReplies: 0Last Post: 11th Jan 2007, 10:51 AM