Tru-grip chuck??
Anyone seen one of these Tru-grip chucks before?
Taper is NT40, there's a small center piece inside the body and looks like there should be some type of collet to go with it.
Steve
-
19th Feb 2019, 04:46 PM #2China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
I gave one to a mate a couple ago years ago, did not fit any thing I have it is a collect chuck I think they come in various size collects
-
19th Feb 2019, 06:29 PM #3Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Tru-grip chuck??
I can't find anything about it online, and its a weird design. The taper on the body would tend to spread a collet, so I'm assuming its not relevant to the clamping.
When you screw the nut on fully there is still a gap between the body taper and the nut taper, so I'm guessing the collet might have looked something like this in section:
Steve
-
19th Feb 2019, 09:06 PM #4Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,079
I suspect the centre in the bottom is not for the collet, but rather as a stop for the tool so you can take it out for sharpening and put it back at the same depth to avoid having to reset your Z-axis mid job.
I found this pic of various collet styles including some old/obsolete ones, perhaps it's an E (as opposed to ER)
-
19th Feb 2019, 09:22 PM #5
Hi Guys,
It reminds me of the "Autolock" tool holder, particularly with the centre pin. It probably would work in a similar way ! With the right collets of course.Best Regards:
Baron J.
-
19th Feb 2019, 09:38 PM #6Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Clarkson chuck. I think was the first and should give plenty search hits.
Uses threaded shank milling cutters
-
19th Feb 2019, 09:44 PM #7Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
P.s. the collet is threaded. The cutter screws through the collet, hits the center, forcing the collet towards to nut and this locks everything up
-
19th Feb 2019, 11:24 PM #8Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Definitely not a Clarkson autolock as they have a lugged base on the collet that is larger diameter than the body. This Tru-Grip has a parallel internal diameter for most of the way, then relieved slightly larger at the base where the center part is located.
Also not an E collet as they have a tapered body.
I agree that the center is more likely to be a stop for the tool than the collet though.
Steve
-
20th Feb 2019, 06:51 AM #9
Clarkson Autolock Chuck
Hi Guys,
These are the the best pictures that I cold find of a Clarkson Autolock on an int 40 taper.
s-l225.jpg a-l225.jpg
The collet and a chuck, though I don't think that the collet fits that chuck.Best Regards:
Baron J.
-
21st Feb 2019, 06:45 PM #10Senior Member
- Join Date
- May 2015
- Location
- Richmond
- Posts
- 214
Osborn Titanic II collet chuck.
-
21st Feb 2019, 09:02 PM #11Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Awesome - thanks!!
Steve
-
22nd Feb 2019, 06:47 PM #12Senior Member
- Join Date
- Jul 2012
- Location
- Griffith NSW
- Posts
- 435
I had one of those mounted on an R8 shank for a chinese made mill drill toy. Granted, the mill drill was a complete POS, but I was not a fan of the collet chuck either. I could never get endmills to register on centre in the chuck, forever cutting a flute a lot heavier than the others. I ditched it for a chinese made ER32 collet and it was lightyears ahead of it. Then someone stole it and...well...I wasnt exactly upset to see it gone...
Similar Threads
-
Pattern for Biax leather grip strap
By jhovel in forum METALWORK GENERALReplies: 6Last Post: 18th Feb 2016, 10:49 PM -
collets : to chuck or not to chuck
By steamingbill in forum METALWORK GENERALReplies: 4Last Post: 26th Jul 2014, 10:17 PM -
belt grip
By danielhobby in forum METALWORK GENERALReplies: 2Last Post: 5th Jun 2010, 07:01 PM -
I need a 3 jaw chuck
By BenM78 in forum METALWORK GENERALReplies: 10Last Post: 9th Feb 2010, 09:28 AM -
Vice Grip vs LockJaw
By Screwdriver in forum METALWORK GENERALReplies: 21Last Post: 16th May 2007, 07:41 PM