Needs Pictures: 0
Results 1 to 15 of 18
-
26th Nov 2018, 06:43 AM #1New Member
- Join Date
- Nov 2018
- Location
- Canada
- Posts
- 2
How do I attach an aluminum panel to aluminum tubing
Hi there. I'm new to metal working and the forum. I'm trying to figure out how to attach an aluminum panel to some aluminum tubes. I have a rectangle made out of 3/4" aluminum tubing and the two long sides have a flange on the inside. The aluminum panel sits inside of the rectangle on the flange (See pictures). I'm not sure how to best attach the aluminum to the flange. I would also prefer to have the aluminum panel sit flush with the top of the tubing as I will be resting something on both the tubing and the panel on one side. The space is 2.8 mm. Appreciate the help!
-
26th Nov 2018, 06:50 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
G'day Mark
Welcome to the forum. That sort of panel is just meant to sit there I think. If you really wanted it locked into place, I would suggest some superglue.
Michael
-
26th Nov 2018, 08:32 AM #3
I'd use a 2mm strip of aluminum flat bar as a packer, then use black silicone both sides to glue it in place.
The 0.8mm will be enough room for the a thin layer of silicone either side of the flat bar.Using Tapatalk
-
26th Nov 2018, 02:39 PM #4New Member
- Join Date
- Nov 2018
- Location
- Canada
- Posts
- 2
Hello and thank you both for the reply. I will be attaching something to the aluminum panel so it will be a bit heavier and I want to make sure it stays in place. Will the black silicone/glue hold it together very securely? Thanks!
-
26th Nov 2018, 02:48 PM #5Diamond Member
- Join Date
- Sep 2006
- Location
- Australind , WA
- Age
- 58
- Posts
- 1,281
-
26th Nov 2018, 03:19 PM #6Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
If using silicon make sure it's a neutral cure. Aluminum isn't so fond of the acetic in the acid cure type.
Sikaflex 227 is what I use for bonding jobs on older Landrovers which have aluminum panels.
Steve.
-
26th Nov 2018, 03:30 PM #7Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
I would also use Sikaflex. I like the Sikaflex 11FC. It comes in black. Bunnings stock it.
Chris
-
26th Nov 2018, 05:02 PM #8Senior Member
- Join Date
- May 2013
- Location
- Rockhampton, QLD
- Age
- 68
- Posts
- 456
Welcome to the forum Mark.
-
26th Nov 2018, 06:03 PM #9Using Tapatalk
-
26th Nov 2018, 06:54 PM #10Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Silicone is a lot cheaper than Sikaflex too.
Chris
-
26th Nov 2018, 07:24 PM #11Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
He's in Canada guys - they don't have Bunnings there (and possibly may not have Sikaflex either)
Michael
-
26th Nov 2018, 07:48 PM #12Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
well spotted!
Chris
-
27th Nov 2018, 05:39 PM #13Senior Member
- Join Date
- Nov 2012
- Location
- Mid North Coast NSW
- Posts
- 423
-
27th Nov 2018, 07:32 PM #14Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,915
Definitely not silicone IMHO, as an adhesive it's rubbish Sikaflex (polyurethane) all the way for my money. Sikaflex actually isn't that great, Simson or Bostic are much better quality, although it really shouldn't matter in this application.
-
27th Nov 2018, 08:57 PM #15
Similar Threads
-
Joining Aluminum Tubing
By aagui in forum WELDINGReplies: 16Last Post: 18th Jan 2017, 09:15 PM -
Tapering or coupling aluminum tubing
By horseatingweeds in forum METALWORK GENERALReplies: 22Last Post: 13th Oct 2016, 09:12 AM -
aluminum arc welding
By johnyjamtin in forum WELDINGReplies: 6Last Post: 22nd May 2014, 12:59 AM -
Aluminum
By benupton in forum METALWORK GENERALReplies: 5Last Post: 1st Apr 2010, 01:11 AM -
Aluminum Solder
By Nurgle in forum METALWORK GENERALReplies: 7Last Post: 2nd Aug 2007, 12:46 PM