I broke my torque wrench
Today I broke the ratchet head on my torque wrench trying to remove the 46mm nut from my motorbike rear wheel. The pawl broke in half. It's an ETC brand ½" drive wrench. It's quite old but has had almost no use. There are hundreds of places online selling repair kits for ratchet heads, but none specifically for this brand. I'm confident there's one out there that would fit, but as they don't specify dimensions, I can't know which one would fit.
I don't really need the ratchet feature. I have a Norbar torque wrench with a ratchet that I use for most jobs. The ETC only gets dragged out when I have a job that exceeds the Norbar's limit. So I'm happy to permanently fix the cylinder into the head. I have oxy-acet and I have a mate with MIG and TIG. Does welding sound like a reasonable fix?
I can get a similar Kinchrome torque wrench for $78, so I don't want to invest too much time and money into repairing this one.
Appreciate any ideas.Chris
-
17th Feb 2018, 08:35 PM #2Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
I never use a torque wrench to undo anything. Wouldn't even consider having a ratchet type either.
Nev.
-
17th Feb 2018, 08:50 PM #3Senior Member
- Join Date
- Jul 2012
- Location
- Griffith NSW
- Posts
- 435
1050cc Triumph?
Ive got a breaker bar for taking it off and I sorta use the torque wrench to put it back on. I lube the threads with a smear of grease and then use the torque wrench to get it to spec, then use the breaker bar to adjust it until the locking ring and the holes line up again. Thats on my 2011 Speed Triple and Ive got that kingchrome torque wrench. She's up to its 7th set of tyres / 50 000km and Ive not broken the wrench yet!
-
17th Feb 2018, 08:56 PM #4
Hi jack620
ETC was Eastern Tool Company which made some pretty good stuff for the reasonable price that the tools were made for.
I have not seen the brand in maybe 20 years, perhaps they were absorbed into another company.
As a repair, I would favour brazing using a manganese bronze filler. A caution here is to be aware of the fume that the chrome plating will give off. Keep it away from your breathing zone,irrespective of what sort of brazing or welding you are performing.Its nasty stuff.
Failing the above just a couple of tacks each side with a 2.5mm Stainless steel ought to hold it.
Grahame
-
17th Feb 2018, 10:52 PM #5Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Neither do I normally, but why not? The ratchet is designed to operate anti-clockwise.
Ducati Monster 796. I use the same technique as you do when tightening the nut. I also use moly grease on thread and face of the nut. I only recently had the rear wheel off for a tyre replacement. Apparently the rear wheel nut on Ducatis is notorious for being difficult to remove.
Thanks Grahame. I've got plenty of blue coated bronze filler rods. Thanks for the heads-up on the chrome fumes.Chris
-
18th Feb 2018, 08:29 AM #6Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 65
- Posts
- 3,103
-
18th Feb 2018, 09:27 AM #7Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
You nay know this already, but the difference between torquing a nut that is 'dry' and lubricated is significant in terms of the tension that it puts on the thread. I'd be checking the manufacturer's instructions on what condition the threads should be in before tightening. In one situation we were having failures in our factory because a supplier's bolt threads were not clean - that was enough to take the bolts beyond yield...
Michael
-
18th Feb 2018, 09:49 AM #8Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
18th Feb 2018, 11:23 AM #9Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
Chris,
Someone in the way distant past told me that you should never use a torque wrench in the reverse direction, and to do so would render the torque wrench in need of recalibration. As I recall it was in relation to the W&B Double Click style of tool. The micrometer style which yours appears to be, presumably is ok with either LH or RH directions, otherwise there would be no reversible ratchet.
Just a heads up for anyone not familiar with that limitation.
Good luck with the repair of yours,
Rob
-
20th Feb 2018, 08:03 AM #10Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
I have the "double click" type torque wrench. I have never been told not to use them to undo bolts but I just assumed that was the case anyway.
I'll be interested to see how your fix goes with this wrench Jack!
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
Similar Threads
-
Collet Nut Wrench
By BaronJ in forum METALWORK GENERALReplies: 3Last Post: 28th Aug 2015, 11:17 PM -
Bugga. Broke a tap
By Michael G in forum METALWORK GENERALReplies: 72Last Post: 15th Nov 2014, 10:08 AM -
HIT Piipe wrench
By WesP in forum METALWORK GENERALReplies: 6Last Post: 24th Feb 2014, 09:09 PM -
Broke my new toy!
By snowyskiesau in forum METALWORK GENERALReplies: 12Last Post: 30th Mar 2012, 08:30 PM -
Oops it broke
By bitza500 in forum THE HERCUS AREAReplies: 3Last Post: 15th Oct 2009, 12:09 AM