Page 1 of 3 123 LastLast
Results 1 to 15 of 38
  1. #1
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,475

    Cool Bump center tool.

    Hi Guys,

    Because I needed to true up an 8" inch length of 35 mm diameter aluminium bar in the lathe three jaw, prior to parting off some slices and having heard about "bump centring", I thought I would give it a go and make one.

    30-07-2017-013.JPG 30-07-2017-012.jpg

    It is a very simple tool to make ! Basically a ball race fastened to the end of a piece of bar.

    30-07-2017-015.jpg 30-07-2017-014.jpg

    Above is a couple of pictures of the one I've made. A piece of 1/2" square bar four inches long, to fit into my Myford tool holder. A 5 mm hole drilled 12 mm from one end and threaded M6. Since this ball race has a 15 mm bore and is 15 mm thick, I turned a plug from a bit of black bar, with a 20 mm diameter flange, and drilled a 6 mm through hole for the cap screw.

    In use you just need to put the tool into the tool holder, and approach the work piece with the ball race. As the race contacts the work it will push it, simply apply pressure until the work piece runs true. Then re-tighten the chuck jaws.

    In my case I centre drilled the work piece and since I was going to part off some slices, used a live centre to support the free end.
    Best Regards:
    Baron J.

  2. #2
    Join Date
    Apr 2012
    Location
    Healesville
    Posts
    2,129

    Default

    Hiya BaronJ, yes they are a handy tool, I have one and call it a push tool.
    Mine is just a piece of 1" dia black bar turned at the end and the brg press fitted on.

    cheers, shed

  3. #3
    Join Date
    Jun 2007
    Location
    Vic
    Age
    48
    Posts
    544

    Default

    Hi BaronJ. I love that too, very quick to chuck thin work piece.

    20170730_213417.jpg

  4. #4
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Neat BJ.

    Like Shed, I opted for the easy version, albeit a boys version with its little bar and bearing. Works nicely. Probably should have made it fifteen years ago!

    Bob.

    DSC_7597 (Large).jpg DSC_7590 (Large).jpg DSC_7589 (Large).jpg

  5. #5
    Join Date
    Apr 2009
    Location
    Ballina N.S.W.
    Posts
    644

    Default

    Hi All,
    These are a very handy tool. When I first saw the design quite a few years ago, from memory from the man of great innovations John Stevenson, I knocked up rough version. Often I need to open up the ID on flat washers so I added on a small bearing that came from a fishing reel overhaul. this works great as you can approach the washer from an angle and get down to using it on very small washers.
    Bob
    Attached Images Attached Images

  6. #6
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Innovative dovetailing Bob.

    I like the small bearing idea. I will be copying it.

    Bob.

  7. #7
    Join Date
    Apr 2009
    Location
    Ballina N.S.W.
    Posts
    644

    Default

    Hi Bob,
    When I built this tool I was not sure if it would work so I just took the easiest path, after using it for quite a while now it is one of my favorite tools for rough setting jobs in the three jaw chuck as well as the washer use. It is a light duty tool so no need for full dovetails. You will enjoy the adding the small bearing.
    Bob

  8. #8
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Hi Bob,

    Any chance of letting me know the size of the small bearing? I know your lathe is larger than mine so what I'm thinking might be small (10mm-ish) may not be so. There are numerous inexpensive fishing reel bearings available on eBay to choose from.

    3x10x4mm Fishing Reel Bearing Stainless Steel Balls/Retainer Corrosion Resistant | eBay
    8x12x3.5mm Fishing Reel Bearing Stainless Steel Balls / Cage Corrosion Resistant
    7x14x5mm Fishing Reel Bearing Stainless Steel Balls / Cage Corrosion Resistant | eBay

    Bob.

  9. #9
    Join Date
    Apr 2009
    Location
    Ballina N.S.W.
    Posts
    644

    Default

    Hi Bob,
    Just measured my bearing it is 10mm OD * 4mm wide. Looks like the first link you have shown would be the one. I used loctite to hold the bearings in place to keep the bulk of the fitting down.
    Bob

  10. #10
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Bob, if you want them I have some bearings that are 3/8" OD, 1/8" bore, 5/32" thick. I also have some that are 5/32" OD, 5/64" bore and 1/16" thick (arrived in a box of stuff - never used them)

    Michael

  11. #11
    Join Date
    Jun 2007
    Location
    Vic
    Age
    48
    Posts
    544

    Default

    I removed these from the hard drive of an old computer. Let me know if that is any good to you Bob?

    20170801_172129.jpg

  12. #12
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Quote Originally Posted by Michael G View Post
    Bob, if you want them I have some bearings that are 3/8" OD, 1/8" bore, 5/32" thick. I also have some that are 5/32" OD, 5/64" bore and 1/16" thick (arrived in a box of stuff - never used them)

    Michael
    Hello Michael,

    I will take you up on your offer. How about one of the 3/8" OD bearings to yet further increase my indebtedness?

    A grateful Bob.

  13. #13
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Hello Trong,

    Thank you very much for your kind offer but I have accepted Michael's. No point in me being too greedy.

    Bob.

  14. #14
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Hang on - I thought I owed you? Shall we call it a draw and start again?
    I'll get it in the post tonight

    Michael

  15. #15
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Holly crap. What a great little tool. Another tool I need to make!

    Thanks for posting!

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

Page 1 of 3 123 LastLast

Similar Threads

  1. Bump
    By Rod Gilbert in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 5
    Last Post: 13th Apr 2013, 10:11 AM
  2. Reversed live center.
    By aametalmaster in forum METALWORK GENERAL
    Replies: 1
    Last Post: 9th Jan 2012, 02:08 PM
  3. how do you center a 4 jaw chuck ?
    By welder in forum METALWORK GENERAL
    Replies: 6
    Last Post: 11th Jul 2011, 10:06 PM
  4. Center finders
    By Stustoys in forum METALWORK GENERAL
    Replies: 7
    Last Post: 5th Jan 2011, 12:58 PM
  5. Non Morse Taper Live Center ?
    By Plushy in forum METALWORK GENERAL
    Replies: 5
    Last Post: 8th Nov 2010, 10:48 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •