    Default Filling dings

    What is the preferred product for filling in 'dings ' in beds and tables ? I've seen JB weld mentioned and liquid steel . Also the knead together stuff ?

  2. #2
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,217

    Default

    A stone and fill the dings with oil works OK. Unless you are doing a full rebuild.
    Gold, the colour of choice for the discerning person.

  3. #3
    Join Date
    Jun 2011
    Location
    Australia east coast
    Age
    71
    Posts
    2,713

    Default

    Quote Originally Posted by .RC. View Post
    A stone and fill the dings with oil works OK. Unless you are doing a full rebuild.
    Agree. Make sure there are no raised edges and then ignore the dings.

    If you want a precision, brand new, unmarked machine table/surface, buy a new machine and never use it. The person who buys it at your estate sale will thank you, but meanwhile, you might as well not bother owning it (unless you're a collector and just like to boat about your toys).

    OTOH if the previous owner used the table as an anvil - you knew that when you bought it, so you should have already had a plan to address the problem. Devcon isn't a plan.

    PDW

  4. #4
    Join Date
    Oct 2007
    Location
    Sydney
    Posts
    3,112

    Default

    Agree with the above, carefully stone it down, and if you did it yourself you've probably had enough words to say about it at the time, none of which can be printed here. Put it down to experience and move on.

    For a bed I'd very carefully stone the burr down and generally leave it alone. Don't fill it with anything as, unless it's complete chop suey, it won't affect the function. There will still be plenty of material around it to bear on.

    For a table it will depend on the damage and the machine. You could have it surface ground if the damage is light and you just want it pristine. You could fill the holes with JB weld or similar and make it look like a table filled with bog. Bog that will likely fall out again given most people's use of it, and will be soft so attract grit. You could drill out the holes and press in plugs. That's probably the ideal repair and done with skill will result in a repair about as good as it can get. However is really only an option for the occasional hole. I've seen drill tables that were literally disgusting, they looked like nobody had ever used anything under the material when drilling. Literally. The tables looked like the surface of the moon with a giant impact crater in the centre. In cases like that you could bore out the centre and press/loctite in an insert and then grind or scrape it flat. Especially scraping cast iron, you won't be able to see the repair. But they are all relatively serious repairs.

  5. #5
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    Quote Originally Posted by morrisman View Post
    What is the preferred product for filling in 'dings ' in beds and tables ? I've seen JB weld mentioned and liquid steel . Also the knead together stuff ?
    No preferred product as such, it depends on how bad the damage is.

  6. #6
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    What are you calling a ding?

  7. #7
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    As in a lot of requests for help on something, pictures tell a thousand words. So, if we had a few pics, we would be able to give a lot better information. I've a few scrap blocks of cast, if it's that bad.
    Kryn
    To grow old is mandatory, growing up is optional.

  8. #8
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    Devcon

  9. #9
    Join Date
    Jan 2016
    Location
    Wodonga Vic
    Age
    38
    Posts
    633

    Default

    if it's purely for aesthetics maybe fill the dings with molten antimony lead and scrape flat?

  10. #10
    Join Date
    Nov 2004
    Location
    Bungama SA
    Age
    52
    Posts
    960

    Default

    Quote Originally Posted by NedsHead View Post
    if it's purely for aesthetics maybe fill the dings with molten antimony lead and scrap flat?
    Yes Sb and some As makes a nice hard lead, tad of copper and silver also helps to make a hard lead... just like the bullion we get from the blast furnace at work , this lead will bend a little then snap/break.
    We use this kind of blend to patch chipped concrete in our crane landing bays and out on the final products logistics bays, gets driven on by forklifts constantly(up to 25T) so its pretty tough but you could dent it with an impact from a heavy sharp object
    ....................................................................

  11. #11
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    As others have said, stone it flat so there are no parts that are proud of the precision surface. The small dent will likely reduce your contact area by an unnoticable amount. Filling it with any of those puttys (JB etc) will not contribute to the contact surface and so will be a phsycological repair at best.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  12. #12
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,723

    Default pic

    A ding or two in my old Holbrook T13 lathe bed ding.jpg, directly underneath the chuck . Probably the chuck was dropped more than once It look horrible .

  13. #13
    Join Date
    Oct 2007
    Location
    Sydney
    Posts
    3,112

    Default

    Don't worry about them, they are on the tailstock ways and won't affect function. If you want pristine ways, buy a new lathe and wait until you put some in yourself!

    If it really bothers you, make up a way cover so WHEN you crash the lathe or drop something on the ways, you won't damage the ways and don't have to look at those who have gone before you.

Similar Threads

  1. Filling and Retapping in alloy
    By mcchaddy in forum METALWORK GENERAL
    Replies: 13
    Last Post: 20th Oct 2010, 08:19 PM
  2. Filling holes in metal, what techniques are available?
    By chris330 in forum METALWORK GENERAL
    Replies: 11
    Last Post: 5th Nov 2008, 03:32 AM
  3. Filling my Primus gas bottle
    By jmk89 in forum METALWORK GENERAL
    Replies: 15
    Last Post: 9th Jul 2008, 10:51 AM
  4. filling a metal depression for powdercoating
    By bigpeeet in forum METALWORK GENERAL
    Replies: 4
    Last Post: 25th Nov 2007, 09:25 PM
  5. filling up Acetylene Oxy set
    By timbo123 in forum METALWORK GENERAL
    Replies: 8
    Last Post: 27th Jun 2007, 01:59 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •