Thanks Thanks:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Page 1 of 2 12 LastLast
Results 1 to 15 of 23
  1. #1
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,725

    Default Where to buy cast round

    I need to buy cast iron round stock

    found this mob

    Sydney Steel Merchant, Steel Fabrication, Stainless Steel Supplier

    anybody had dealings with them ?

    Bohler don't seem to have cast iron any more .

  2. #2
    Join Date
    Jul 2011
    Location
    Melbourne Australia
    Posts
    1,376

    Default

    Flocast in Reservoir. Most of the other merchants get it from them.

    Cast Bronze Bar,Copper Alloys Brass,Aluminium Bronze Bar,Bronze Bushing Manufacturers Australia

    They cut to length. There might be a mimimum charge. When you make an inquiry, a guy named Luke will get back to you, and I guarantee his email will BE IN ALL CAPITOL LETTERS.

    Thats only 5 minutes from here, if you want some one to pick it up and on-ship it.

    Regards Phil.

  3. #3
    Join Date
    Aug 2012
    Location
    Tamborine Mountan
    Posts
    102

    Default

    Bohler don't seem to have cast iron any more .[/QUOTE
    Bohler list cast iron under non ferrous in their products menu,
    or at least their Brisbane outlet does,
    Leroy.

  4. #4
    Join Date
    Jul 2011
    Location
    Melbourne Australia
    Posts
    1,376

    Default

    You could also try Global Metals. They have just moved from Thornbury to Dandy South. So at least that's on your side of town.

    Global Metals

    The joints probably still in disarray. I was at the Thornbury branch two weeks ago. They had to move 1,500 tonnes of metal out to the new place last week.

    Regards Phil.

  5. #5
    Join Date
    Mar 2009
    Location
    Melbourne
    Age
    54
    Posts
    825

    Default

    A really cheap source of roundish cast stock is old sash window weights.
    I find them pretty good for sizes up to 1.25" by the time you machine them round.
    Obviously they aren't super fine grain but I have found them to be generally pretty good especially when you can get two for a buck.
    It all depends on what you need the stock for.
    Cheers,
    Greg.

  6. #6
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    40
    Posts
    4,515

    Default

    I use Edcon regularly for BMS flat bar, ally bar and 12L14. I have had good service although they can take a while if they need to get something in. They ship to me via Barnetts. Would make sense for you to get something from Melbourne though Mike, not Sydney.
    1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.

  7. #7
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,725

    Default

    OK thanks .

    Interalloy is another possible option but they usually want you buy a minimum standard length which is a pain, they don't seem to sell off cuts .

    I am running out of old cast iron pullies to machine down ! I sometimes find the exercise weights at op shops but they are often made from a pretty crappy stuff, difficult to machine and the smaller ones are dog bone shaped so your limited with what you can do with them .

  8. #8
    Join Date
    Mar 2009
    Location
    Melbourne
    Age
    54
    Posts
    825

    Default

    Interlloy will sell whatever length you need they just have a $100 minimum order (last time I bought from them, it might be more now)
    I found them quite helpful on the phone and just cobbled together enough cast, 4140 and EN36 to get $100 worth.
    Order turnaround was overnight and it was an eye opener driving through their warehouse to collect the order.
    Cheers,
    Greg.

  9. #9
    Join Date
    Dec 2010
    Location
    Syd
    Posts
    492

    Default

    If the Edcon store you're dealing with doesn't have the stock, bringing it in from another one can get exxy buying small quantity. They'd be about the last ones I'd deal with for interstate sourcing going on that experience.

  10. #10
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,725

    Default Arrogant

    I rang Interalloy but it was a waste of time

    The salesman was arrogant..he said " our off cuts go into the scrap bin " and " whats your business name ?" and "we charge a 15 dollar cutting fee plus GST " and minimum charge is 150 bucks "

    Bohler is the same, they behave as if a bit of cast iron is the crown jewels .

    And people wonder why we don't make anything any more

  11. #11
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    It may cost you in freight but Surman metals here in Adelaide do sell by the kg.

    Michael

  12. #12
    Join Date
    Jul 2011
    Location
    Melbourne Australia
    Posts
    1,376

    Default

    Did you try Flocast? The place where just about every one else gets their cast from. The only thing they sell is cast bar or bronze alloys..

  13. #13
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,725

    Default

    I will try Flocast and Global metals tomorrow ... thanks for the help .

    One thing I can say . I will never go anywhere near Interalloy or Bohler again , I' ve had enough of their silly attitude ...

  14. #14
    Join Date
    Jul 2011
    Location
    Melbourne Australia
    Posts
    1,376

    Default

    Quote Originally Posted by morrisman View Post
    I' ve had enough of their silly attitude ...
    You'd have to go there. Both Interalloy & Bohler, would be in excess of 50 staff. They're not you're local scrappy or steel merchant.

    Nothing happens until its cleared accounts, then a cut order will be issued, two blokes involved there, the crane operator and the saw operator. Plus a store man, and some one running the dockets. $15 bucks a cut, they will be doing their nuts.

    What processed you to go near Interalloy. The second, third & forth words of their web site say "Engineering Steels & Alloys"

    Interlloy | Engineering Steels + Alloys

    Bohler, Like wise. "Engineering, Stainless & Tool Steel suppliers". Stainless Engineering Steel Supplies | Engineering Steel Tool Suppliers

    You go to them if you need K245, P20, EN36, Orvar, Dievar, Chrome plated, etc.

    When I tell you, other merchants get there cast from Flocast. Take a look at the two specs from Flocast & Interalloy for 4E cast.

    http://www.flocast.com.au/4E-Chemica...sis-Range.html

    Grey Iron 4E | Interlloy | Engineering Steels + Alloys

    I think you will find the Spec's are verbatim. Or am I wasting my breath here. I can tell you that because LUKE D with the CAP LOCKS, has told me, I might be able to pick up the size I want, because he's just sold a full bar length to Interalloy.

    Bohler and Interalloy will get you any amount you want, as long as its in mill quantities of 5,000 kg's. Despite what their web site says. Been through this 5 times since 2011, trying to find bricks for the scraping classes.

    Global hold rectangular in Perth for the mining industry, and Flocast are the font for anything round / hollow.

    Phil.

  15. #15
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    I am surprised you are having trouble getting cast iron. Here I just go to the local bolt/steel merchant and they are able to get me what I want, usually ex stock, although I buy very little of it. But certainly a small steel supplier might be more forthcoming then a large business that sells to the small steel supplier.

    I know Qne Steel here will not sell me half a length of special steel, they will direct me to the small supplier, they will sell me full lengths though.
    Gold, the colour of choice for the discerning person.

Page 1 of 2 12 LastLast

Similar Threads

  1. Scraping round stuff
    By Bryan in forum METALWORK GENERAL
    Replies: 3
    Last Post: 3rd May 2013, 12:20 AM
  2. Cast iron VS Cast steel lathe compound slide
    By Ueee in forum METALWORK GENERAL
    Replies: 10
    Last Post: 23rd Dec 2012, 11:40 PM
  3. Round Trailer Lights
    By zuffen in forum TRAILERS & OTHER FABRICATED STUFF
    Replies: 2
    Last Post: 3rd Sep 2011, 05:38 PM
  4. Cutting Alum Round Bar
    By Bidgee in forum METALWORK GENERAL
    Replies: 6
    Last Post: 5th May 2010, 06:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •