5th Mar 2015, 05:17 PM #1
Metal ID please brains trust
I have 3 or 4 old steering locks like this one. Stuck the handle and the forked part in the bandsaw to cut it today. Polished a nice patch it did. I guess some grade of tool steel?
Out comes the cut off saw or grinder I suppose.
-
5th Mar 2015, 05:54 PM #2New Member
- Join Date
- Nov 2010
- Location
- Perth W.A
- Posts
- 0
Probably case-hardened,
Hardened outer layer but mild or carbon steel underneath.
-
5th Mar 2015, 09:23 PM #3Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,216
Case hardened, or induction hardened or possibly nitrided.. Whatever was the cheapest in China to do... So probably a cyanide bath...
Gold, the colour of choice for the discerning person.
-
5th Mar 2015, 10:55 PM #4Cba
- Join Date
- Aug 2007
- Location
- Melbourne
- Age
- 68
- Posts
- 1,410
-
6th Mar 2015, 07:58 AM #5
Thanks all.
I had done a search but couldn't locate much at all regarding material type. I know when they were first introduced they showed hacksaws trying to cut them I had forgotten that till this morning
I had no idea though that the handle tube would be just as tough.